Questions in electroplating Here is the first attempt. Seems quite good. Tried to scratch, nothing happens. Hard as it should.
... |
13-5-2024 at 13:13 by: WFChem |
searching for solution for immersion electroless nickel stripper Does anyone know why in sodium carbonate based strippers Sodium 3-nitrobenzenesulfonate is present a ... |
13-5-2024 at 12:14 by: WFChem |
Questions in electroplating Okay. I will try this also. Maybe there is another device on the market with housing and not the pla ... |
11-4-2024 at 05:14 by: WFChem |
searching for solution for immersion electroless nickel stripper [rquote=692360&tid=160284&author=Sulaiman]I've been reading a little about fluorine compound ... |
10-4-2024 at 07:48 by: WFChem |
Questions in electroplating [rquote=692363&tid=159939&author=Rainwater]Plate thick, machine later. Even with a perfect p ... |
10-4-2024 at 07:09 by: WFChem |
Questions in electroplating Hello,
thanks for your answer. I will test it again with a full basket and try to pump through th ... |
9-4-2024 at 13:39 by: WFChem |
searching for solution for immersion electroless nickel stripper Hi,
sandpaper, sand blasting is not possible. Its a hard nickel silicon carbide coating.
I am ... |
9-4-2024 at 04:13 by: WFChem |
searching for solution for immersion electroless nickel stripper Hi Sir,
the base material is aluminium.
Sulphuric acid with hydrogen peroxide does remove nick ... |
9-4-2024 at 03:36 by: WFChem |
searching for solution for immersion electroless nickel stripper Hi,
I have not access to the metalx nickel stripper from caswell. They dont ship to germany. Also ... |
9-4-2024 at 03:27 by: WFChem |
Questions in electroplating Hello,
a little update: In fact it seems the anode area was too small. The anode diameter with 8 ... |
9-4-2024 at 03:22 by: WFChem |
Questions in electroplating Sure the anode will corrode slowly. But the pitting was extreme. It looked like a rough diamant file ... |
10-2-2024 at 04:35 by: WFChem |
Questions in electroplating I will show a photo when its success. Hope it will not fail. |
8-2-2024 at 14:48 by: WFChem |
Questions in electroplating [rquote=688752&tid=159939&author=vanBassum]Are you trying to plate the inside of a cylinder ... |
8-2-2024 at 05:08 by: WFChem |
Questions in electroplating Hello,
thanks for fast response.
[quote]
Can you clarify that. Did your plated piece get pi ... |
2-11-2023 at 05:54 by: WFChem |
Questions in electroplating Hi,
I am Chris and recently started off in electroplating. I have some questions because my first ... |
1-11-2023 at 08:52 by: WFChem |