Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Search
Parchment Paper Diaphragm
To the list of materials suitable as a diaphragm, I would like to add:

Parchment paper

Its use ...
3-5-2025 at 07:08
by: bearbot22
Homemade diaphragms for electrolysis. New developments
Hi Hexabromobenzene!
I made further tests with non-woven PP.
The leakaing was greatly reduced by ...
9-1-2025 at 00:59
by: bearbot22
Cell for Testing diaphragm materials
Hello Hexabromobenzene,
thanks for your inspiring posts about finding the perfect DIY diaphragm.
I ...
15-12-2024 at 22:44
by: bearbot22
Divided Cell using "Blumat" - very simple
The construction of an electrolytic cell with membrane (diaphragm) is particularly simple with a “ ...
5-10-2024 at 10:46
by: bearbot22
DIY Divided electrochemical cell with stirring and cooling
@Catslovechemistytoo
Even if I want to, i can't run your experiment. My clay membranes are soaked i ...
20-8-2024 at 08:31
by: bearbot22
DIY Divided electrochemical cell with stirring and cooling
[rquote=694618&tid=158683&author=Catslovechemistytoo]

Interesting. But how are you using ...
13-8-2024 at 02:34
by: bearbot22
Ball Mill From A Cordless Drill
I don't think the cap will wear out as long as you keep everything aligned and the screw is centered ...
13-8-2024 at 02:14
by: bearbot22
Ball Mill From A Cordless Drill
Just converted my Cordless Drill into a Ball Mill / Tumbling Mill with no costs.

The Childproof c ...
12-8-2024 at 02:54
by: bearbot22
DIY Divided electrochemical cell with stirring and cooling
[rquote=692216&tid=158683&author=dicyanin]Beautiful work :cool: I am tempted to build one ac ...
22-6-2024 at 08:43
by: bearbot22
DIY Divided electrochemical cell with stirring and cooling
This looks very nice!
[rquote=688683&tid=158683&author=DXFlatline]I've got a unique method ...
4-1-2024 at 07:26
by: bearbot22
DIY Divided electrochemical cell with stirring and cooling
Hi Khlor! Thanks a lot for adding your design here.

[rquote=686817&tid=158683&author=khlo ...
25-8-2023 at 08:18
by: bearbot22
DIY Divided electrochemical cell with stirring and cooling
Hi mysteriusbhoice!

[rquote=674664&tid=158683&author=mysteriusbhoice]use ionomer cement i ...
16-8-2023 at 05:26
by: bearbot22
Improved DIY Electrolytic Cell
I improved the cell-design. Honeypot is now a lot easier to build and to handle.
Whith a current of ...
11-8-2023 at 06:46
by: bearbot22
DIY Destillation Device Howto
Anyone who wants to give the sodacan-alembik a try will find instructions in the attached file.

...
6-8-2023 at 02:32
by: bearbot22
Solvent recovery - DIY Alembik
Hi Sulaiman! I appreciate your reply, thanks!


[quote]
If sagging or chemical compatibility of ...
5-8-2023 at 07:39
by: bearbot22
Solvent recovery - DIY Alembik
today i got the improved sodacan-alembik to work and i'm quite satisfied with it.

as i found out, ...
3-8-2023 at 00:13
by: bearbot22
Solvent recovery - DIY Alembik
@Sulaiman
Thx for the reply.
I'm using a hot water bath now.

Drink Cans are coated on the ins ...
2-8-2023 at 07:49
by: bearbot22
Solvent recovery - DIY Alembik
I build a can-Alembik first try today and -as expected- it was far from perfect.

Could not manage ...
1-8-2023 at 01:20
by: bearbot22
Solvent recovery - DIY Alembik
I'm looking for a way to distill smaller amounts of solvent. In my case Isopropyl alcohol which i us ...
31-7-2023 at 06:29
by: bearbot22
DIY handheld peristaltic pump as separatory funnel replacement
This one-hand-operated and battery-powered pump transfers 200ml in less than 1 min.

In a chem-lab ...
17-6-2023 at 04:46
by: bearbot22
DIY Divided electrochemical cell with stirring and cooling
hi mysteriusbhoice,

the electrolyte used is 7-10% H2SO4 in water/alcohol - i'm not really sure pl ...
18-7-2022 at 05:16
by: bearbot22
DIY Divided electrochemical cell with stirring and cooling
I'm proud to present the design of an Electro-Chemical cell that has been developed and improved ove ...
20-6-2022 at 11:00
by: bearbot22

  Go To Top