Organometallic liquid gold luster
Can someone direct me to a patent or published process for formulating organometallic lusters? I am ...
24-12-2020 at 07:11
by: dieglegold
Organometallic liquid gold luster
What is the chemical process for making organometallic gold and silver liquid lusters, similar to th ...
23-12-2020 at 13:16
by: dieglegold
Short question / quick answer - Thread
I have made nitrogen triiodide ever since I was a kid. It is a wickedly dangerous compound, and a lo ...
3-11-2015 at 09:40
by: dieglegold
Touch powder
I have seen the term "touch powder" mentioned on this blog site. What is touch powder?
2-11-2015 at 10:52
by: dieglegold
Fulminating Gold
Until this last batch I had been using 99.99 % bullion gold. If you read above, I had plenty of pro ...
30-10-2015 at 12:31
by: dieglegold
Fulminating Gold
Well, I am back to generating disappointing results with fulminating gold. I received the bottle of ...
30-10-2015 at 08:51
by: dieglegold
Fulminating Gold
Cyanureeves, Tdep and others: I have now joined the ranks of those who can prepare fulminating gold ...
20-10-2015 at 15:06
by: dieglegold
Fulminating Gold
Hissingnoise: Sometimes a person receives an offer so generous that it simply leaves one breathless. ...
20-10-2015 at 14:50
by: dieglegold
Fulminating Gold
The video is most helpful! The devil is usually in the details, and I learned a couple of useful ti ...
20-10-2015 at 11:06
by: dieglegold
Fulminating Gold
Well, another failure-partially. I followed Tdep's advice by adding a large excess of ammonium hydr ...
20-10-2015 at 08:16
by: dieglegold
Fulminating Gold
I meant $13 for a 1000 ml bottle, not a pint.
19-10-2015 at 11:40
by: dieglegold
Fulminating Gold
I believe that Halogen has perhaps inhaled too much halogen.

Tdep: Excellent suggestion. I will ...
19-10-2015 at 10:33
by: dieglegold
Fulminating Gold
Cyanureeves: Understood, and thank you very much for providing additional details. Rather than prod ...
18-10-2015 at 19:38
by: dieglegold
Fulminating Gold
To answer aga's question above, the reason is because I am brand new to this forum and don't yet und ...
18-10-2015 at 16:28
by: dieglegold
Fulminating Gold
I have been trying to prepare fulminating gold for 2 months with rare success. Most of my batches d ...
17-10-2015 at 12:40
by: dieglegold