Thoughts On Anodes Here is a thought for an anode that I don't think anybody has tried at least from what I have read. ... |
27-7-2012 at 12:52 by: gregkdc1 |
Thoughts On Anodes My thoughts are this.
> It is known that MnO2 will make perchlorate but wear rates are high so i ... |
23-12-2011 at 19:13 by: gregkdc1 |
Thoughts On Anodes Just a few more "thoughts" on anodes. I have read this thread in its entirety as well as the PbO2 t ... |
23-12-2011 at 14:32 by: gregkdc1 |
Thoughts On Anodes All right Dann is that the Bi/Sn oxide anode or is it LD? If it is the Bi/Sn please tell us more. ... |
8-11-2011 at 08:12 by: gregkdc1 |
Polymer bonded anodes? I was wondering if an anode made out of lead dioxide and silicates would work? I know that calcium ... |