Search |
3D Printed Lab Parts in PVDF for Sale Max build size is 8.7" x 5.7"x5.7". I will preface that it's still experimental, it's a challenging ... |
6-12-2018 at 06:26 by: runninfarmer |
3D Printed Lab Parts in PVDF for Sale Here's a video of me printing a cylinder. After it's done I'll post another video of its toughness.
... |
5-12-2018 at 20:08 by: runninfarmer |
3D Printed Lab Parts in PVDF for Sale Hi David, no this is the more common FDM process. Unlike PTFE, PVDF is melt processable so it can b ... |
28-11-2018 at 19:33 by: runninfarmer |
3D Printed Lab Parts in PVDF for Sale Hi All,
I'm offering custom 3D printed parts of PVDF (polyvinylidene fluoride) for sale. PVDF is ... |
28-11-2018 at 18:21 by: runninfarmer |
K metal from KOH, Mg, and Diacetone Alcohol I've been studying this Nurdrage video here: https://www.youtube.com/watch?v=JAo2F9ymKXA
Nurdrage ... |
11-10-2015 at 14:45 by: runninfarmer |
6 g/hr Ozone Generator Build Yes, I have already stated air will form NOx with ozone, which is why I intend to use pure O2. Also, ... |
28-4-2015 at 05:47 by: runninfarmer |
6 g/hr Ozone Generator Build That is a good questions. The ebay page says 10W, while I found an identical one with 40W rating at ... |
27-4-2015 at 09:27 by: runninfarmer |
6 g/hr Ozone Generator Build How is that an exaggeration, particularly if passing pure O2? Unless you know the design equations f ... |
27-4-2015 at 08:33 by: runninfarmer |
6 g/hr Ozone Generator Build Pretty sure they're quartz tubes, you need a cooling fan to blow on the tubes, otherwise they overhe ... |
27-4-2015 at 06:13 by: runninfarmer |
6 g/hr Ozone Generator Build Thanks Dr.Bob! I'm excited to test it fully. Need to get my hands on a decent sized oxygen tank an ... |
26-4-2015 at 20:25 by: runninfarmer |
6 g/hr Ozone Generator Build I've built a 6 g/hr ozone generator using these ozone generators off ebay: http://www.ebay.com/itm/2 ... |
26-4-2015 at 18:14 by: runninfarmer |
Spinning Band Distillation Unit for Sale I've lowered my price to $400 or best offer. Thanks for looking |
11-3-2015 at 12:17 by: runninfarmer |
Spinning Band Distillation Unit for Sale That's true, I was thinking about that. Since ebay takes 9% I could go $600 on it. If anyone's inte ... |
5-3-2015 at 19:44 by: runninfarmer |
Spinning Band Distillation Unit for Sale Hi everyone, I have a nice spinning band distillation unit for sale. It's a nice piece of equipment ... |
5-3-2015 at 17:27 by: runninfarmer |
Magnesium Oxide Crucibles It appears you're right and you don't use a binder. I found this article from Los Alamos that descr ... |
9-11-2012 at 20:18 by: runninfarmer |
Magnesium Oxide Crucibles I would like to be in 1500-2200C range in air. Mainly to melt iron. I would like to try to make si ... |
9-11-2012 at 18:02 by: runninfarmer |
Magnesium Oxide Crucibles I've seen you can buy magnesium oxide crucibles on this website:
http://news.thomasnet.com/fulls ... |
9-11-2012 at 17:34 by: runninfarmer |
Corning Mega Pure MP-3A Water Purifier Distillation Unit My auction ended so here's an updated link to my ad with a buy-it-now or best offer option for those ... |
26-10-2012 at 16:30 by: runninfarmer |
Corning Mega Pure MP-3A Water Purifier Distillation Unit I have uploaded a video of me testing the unit on youtube and demonstrating that it powers on. The ... |
17-10-2012 at 16:45 by: runninfarmer |
Corning Mega Pure MP-3A Water Purifier Distillation Unit I have a Corning Mega Pure MP-3A Water purifier distillation unit for sale on ebay if anyone's inter ... |
17-10-2012 at 07:30 by: runninfarmer |
Ideas for High Temperature Experiments in Kiln/Furnace? Hi everybody, I recently constructed a high temp electric kiln/furance and was wondering if anybody ... |
13-3-2012 at 19:12 by: runninfarmer |
unconventional sodium I've seen a lot of people make sodium metal from NaOH using Mg as a reducer. I've also read the two ... |
5-12-2011 at 19:17 by: runninfarmer |
NaCl reduction with Mg? Sorry this is another "sodium question", but I've seen a lot of people make sodium metal from NaOH u ... |
5-12-2011 at 17:26 by: runninfarmer |