Next, imbue the surface of Mg or Al with the hydrogen atom radical (from the traditional nascent hydrogen generation methods based on say Al/NaOH).
One may assume that the •H radical functional behaves (per its seemingly reversible formation reaction: e- + H+ = •H ) as apparently a (e-,H+)
pair acting on ions. For an example from 'Hydrometallurgy 2008: Proceedings of the Sixth International Symposium', p. 818, a commercial reductive
leaching equation, to quote:
" PbS + 2 •H = Pb + H2S (5) " (see https://books.google.com/books?id=1etfSdk55SYC&pg=PA818&... )
which I view functionally as follows:
Pb(+2)S(2-) + 2 (e-, H+) = Pb + H2S (g)
......
[Edited on 4-10-2018 by AJKOER] |