[*] posted on 9-2-2009 at 13:16
What happens when latex rubber reacts with oil?


It's commonly mentioned that latex rubber is attacked by oil, including skin oils. I was wondering, what is the specific chemistry that is going on when this happens?
View user's profile View All Posts By User This user has MSN Messenger
PHILOU Zrealone
International Hazard
*****




Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 10-2-2009 at 03:55


It simply dissoves!;)
No chemical reaction




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
DrP
National Hazard
****




Posts: 625
Registered: 28-9-2005
Member Is Offline

Mood: exothermic

[*] posted on 10-2-2009 at 06:37


I guess it depends on the level of cross linking in the rubber though. If highly cross-linked then rather than disolving it will soften as the oil molecules work their way into the rubber structure. Old hard cracked rubber can be re-vitalised a bit by rubbing in some oil.