beerwiz
Hazard to Others
 
Posts: 130
Registered: 6-2-2014
Member Is Offline
Mood: No Mood
|
|
What type of vessel to use for MELTING NaOH or KOH at 1200C?
I want to run some experiments with molten NaOH and KOH at around 1200'C but I understanding that these molten hydroxides are very corrosive and eat
through glass and many other materials.
Which type of material/vessel can I use to melt KOH and NaOH that will withstand temperatures up to 1200'C?
|
|
|
mackolol
Hazard to Others
 
Posts: 459
Registered: 26-10-2017
Member Is Offline
Mood: Funky
|
|
I believe that crucibles are good for such purposes.
|
|
|
beerwiz
Hazard to Others
 
Posts: 130
Registered: 6-2-2014
Member Is Offline
Mood: No Mood
|
|
A crucible made of what material?
|
|
|
mackolol
Hazard to Others
 
Posts: 459
Registered: 26-10-2017
Member Is Offline
Mood: Funky
|
|
Just a plain crucible made of ceramic.
|
|
|
Tellurium
Hazard to Self

Posts: 84
Registered: 12-7-2017
Location: Group 16, Chalcogen City
Member Is Offline
Mood: smelly
|
|
You could use a nickel crucible, it withstands the 1200°C and it forms a protective layer against the hydroxides.
But as mackolol said plain ceramic should be ok, I also did a lot with molten NaOH and KOH in them
|
|
|
RogueRose
International Hazard
   
Posts: 1601
Registered: 16-6-2014
Member Is Offline
|
|
I would try making a pottery vessel (with Kaolin clay/Kaolite) and some MgO, possibly some zirconium oxide - all these have very high refractory
indexes, are resistant to alkaline and can handle the temp easily.
I'm working on something similar and am using nichrome wire as the heating element built into the crucible, and possibly using a electrode arc for
heating from above (I need higher heat than the 2500F available from nichrome
|
|
|
Mateo_swe
National Hazard
  
Posts: 587
Registered: 24-8-2019
Location: Within EU
Member Is Offline
|
|
I just ordered som alumina tubes from china on ebay.
Same company make crucibles in different forms and sizes and very cheap.
They have very high temp ones, just search ebay and you will find what you look for.
|
|
|
metalresearcher
National Hazard
  
Posts: 822
Registered: 7-9-2010
Member Is Offline
Mood: Reactive
|
|
Probably these bases will decompose in Na2O resp. K2O and water vapor at these temperatures. Or would you like to let it react with carbon to make the
alkali metals ?
|
|
|
morganbw
National Hazard
  
Posts: 561
Registered: 23-11-2014
Member Is Offline
Mood: No Mood
|
|
I am only curious on why you wish to use such a high temperature with any of these two salts.
|
|
|
beerwiz
Hazard to Others
 
Posts: 130
Registered: 6-2-2014
Member Is Offline
Mood: No Mood
|
|
I gave the white ceramic crucible a try and it was fine, it endured 2 hours of KOH at 1200'C.
@morganbw I'm making the philosopher's stone. The economy is in shambles and I need the gold to pay my rent. I also need the health benefits from the
stone to fight the corona virus, it's been widely known that it gives immortality and cures all ailments.
|
|
|
draculic acid69
International Hazard
   
Posts: 1371
Registered: 2-8-2018
Member Is Offline
|
|
What's the need for the high temps?
|
|
|