Panache
International Hazard
*****




Posts: 1290
Registered: 18-10-2007
Member Is Offline

Mood: Instead of being my deliverance, she had a resemblance to a Kat named Frankenstein

[*] posted on 18-4-2021 at 18:46
Distinguishing between coatings and surface treatments




This part came out of a Haake Rheometer. As far I can see it’s a single Machined aluminium part but with three really distinctly different surfaces, I’ve photographed the two surfaces that are unique (the third being being what is just common al machined surface.
The shiny one almost appears like an applied foil and the darker grey one is very thick.
Does anyone have an insight into these surfaces?


2C1904C8-24C1-4D71-85F2-D3D64DD88AA9.jpeg - 2.7MB B1373B2F-8FB8-4607-9D67-5D8E022FDCB9.jpeg - 3.1MB
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1800
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 18-4-2021 at 23:06


The shiny surface looks like regular machined aluminum to me, possibly anodized. The dark one could be anything but I'm guessing some sort of paint.



We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
wg48temp9
National Hazard
****




Posts: 789
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline


[*] posted on 19-4-2021 at 03:28


It looks like a casting. The grey coloured surface looks like an as cast surface meaning no treatment or coating.



I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
View user's profile View All Posts By User
Mateo_swe
National Hazard
****




Posts: 591
Registered: 24-8-2019
Location: Within EU
Member Is Offline


[*] posted on 20-4-2021 at 10:47


I would also guess a casted part that were machined on a lathe.
If one zooms in on the rim of the shiny top surface (not the bottom widest flange), one can see the tool markings left from each turn on the lathe.
Aluminium parts sometimes are anodized but i would guess its just bare aluminium surfaces where its shiny.
If the shiny parts were anodized i dont think you would see the faint tool markings, also anodized surfaces looks great but every scratch made after anodization is highly visible.