clearly_not_atara
International Hazard
*****




Posts: 2927
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 9-4-2025 at 12:37
Let's invent a new floor!


Recently I discovered this paper which attempts to build a better linoleum, as cross-linked epoxidized linseed oil:
https://www.sciencedirect.com/science/article/abs/pii/S09266... (carter2008.pdf)

Instead of the "natural" aerobic crosslinking of linolenic acid (by radical formation), Carter et al "forcibly" cross-link unsaturated fats by epoxidation followed by reaction with a diacid. This produced a stronger material with durability approaching that of polyvinyl chloride.

PVC had displaced linoleum due to its better properties and (eventually) lower cost, but it is probably the most toxic of the common polymers, because it is basically a bunch of alkyl chlorides. So it was interesting to see a mostly bio-based alternative.

However, the diacid cross-linker is bis-maleoyl dipropylene glycol:
dpgdimal.png - 83kB

This was preferable because it has a branched structure which lowers the melting point, and because the monoester of maleic acid has a reactive terminal COOH, due to the electron-withdrawing groups attached.

So the crosslinked ELO system was criticized in a master's thesis by some random Swede which actually makes a serious error in the results interpretation (someone will ask and I will explain), but does anyway raise a valid point about the crosslinker being derived from petrochemicals. The original paper actually acknowledged this problem, but the authors published no follow-ups.

Linseed oil is actually not the cheapest of the highly unsaturated oils (that is probably tung or walnut oil), but one of the nice things about linseed oil is that you can just buy epoxidized linseed oil, it's already an item of commerce, used for varnishes or something. In practice, various oils with high iodine value could be used.

Malonic anhydride is basically renewable. It is easily produced by the oxidation of furfural, which is one of the cheapest bio-derived chemicals coming from the distillation of sugars or polysaccharides. Of course, the home chemist is not going to oxidize furfural in a gas-phase process over a V2O5 catalyst -- they're going to distill malic acid, obviously.

It's the dipropylene glycol which is a sticking point. This is produced from propylene, which is not too easily had from biological sources -- usually, you can get C1 and C2 products from fermentation, a few C4, or you can use long-chain products that come directly from sugars.

But also, there's turpentine. Surprisingly, it can be farmed, by harvesting it from trees without killing the trees. Yields appear comparable to those for farming wood or vegetable oils. So I had the idea for a different diol coming from the ozonolysis of alpha-pinene:
pinodiol.png - 33kB
and the corresponding crosslinker:
pinodioldimal.png - 83kB
This is a little heavier than the dipropylene glycol version, but it is highly branched, so hopefully it is also a liquid.

The ozonolysis of alpha-pinene was investigated in the 1950s with a goal of producing a diacid (requiring dehomologation of the pendant methyl on the alkene), and investigators claimed up to 80% yield of the pinene ozonide, but worse conversion of this to the acid (termed "pinonic acid", from which I derive the name "pinodiol" for the diol):
https://pubs.acs.org/doi/pdf/10.1021/ie50548a034 (fisher1955.pdf)

However, we are interested in alcohols, and so we don't have to worry about side-reactions during oxidation. (The pinonic acid researchers also wanted to achieve oxidation without using additional hydrogen peroxide, which makes everything harder.) Instead we want to reduce the ozonide in situ, which is usually efficient. You or I would probably use borohydride (sousa1960.pdf) but industry would use hydrogen over Raney Ni:
https://www.sciencedirect.com/science/article/abs/pii/S00404...

Attachment: carter2008.pdf (811kB)
This file has been downloaded 179 times (original paper)

Attachment: fisher1955.pdf (560kB)
This file has been downloaded 164 times (pinonic acid by ozonolysis)

Attachment: sousa1960.pdf (484kB)
This file has been downloaded 192 times (borohydride reduction of ozonides)





Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
bnull
National Hazard
****




Posts: 994
Registered: 15-1-2024
Location: East Woods
Member Is Offline

Mood: Fecking annoyed

[*] posted on 9-4-2025 at 13:44


Have you considered butanediol (choose an isomer)? It can be made by microbial fermentation of biomass.

Edit: Oops, forgot the review: Abhishek R. Varma, Bhushan S. Shrirame, Sunil K. Maity, Deepti Agrawal, Naglis Malys, Leonardo Rios-Solis, Gopalakrishnan Kumar, Vinod Kumar. Recent advances in fermentative production of C4 diols and their chemo-catalytic upgrading to high-value chemicals[J]. Chinese Journal of Catalysis, 2023, 52: 99-126.

[Edited on 9-4-2025 by bnull]




Quod scripsi, scripsi.

B. N. Ull

We have a lot of fun stuff in the Library.

Read The ScienceMadness Guidelines. They exist for a reason.
View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2927
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 9-4-2025 at 14:45


You need a little more than that. Butanediol is probably long enough, but it's not branched, which means the corresponding bismaleate is likely a solid. Usually you see lower melting points in open-chain branched hydrocarbons.

But turpentine is still the most expensive component of the process as I wrote it. So I definitely encourage more suggestions of possible diols.




Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
imidazole
Harmless
*




Posts: 46
Registered: 18-10-2014
Location: Massachusetts, USA
Member Is Offline

Mood: Radical

[*] posted on 10-4-2025 at 06:25


how about reducing lactic acid derivatives? that could be a way to make it. I can't think of many commercially available (renewable) branched compounds, maybe partial carboxylation/oxidation of mixxed unsaturated fatty acids, esterfying/acetal/acetylating them, and then then splitting them with ozone or something similar?

[Edited on 10-4-2025 by imidazole]
View user's profile Visit user's homepage View All Posts By User
chempyre235
Hazard to Others
***




Posts: 216
Registered: 21-10-2024
Location: Between Nb and Tc
Member Is Offline

Mood: Quite distracted

[*] posted on 10-4-2025 at 11:35


You could always try some urushiol! :P

More seriously, a bit of searching awarded me a few possible diols/polyols that could be useful. The issue I found was that most of the low MW natural/naturally derived compounds have a melting point well above room temp. However, the secret to a workable polymer and cost-cutting may be to use more than one kind of diol. Here are some that I found:

  • Ethylene glycol
  • Propylene glycol
  • Glycerin
  • Isosorbide (from sugar or cellulose)
  • 2,5-Bis(hydroxymethyl)furan (from sugar or cellulose)
  • Pantoic acid
  • Eucalyptol (after hydrolysis of ether)

I think this is a good idea to work on some cheap, naturally derived, nontoxic polymers. Be sure to keep us posted!

[Edit]: It may help to do some reading on natural stable biopolymers, like sporopollenin.

I also just found that the product of eucalyptol hydrolysis is called terpin, and can also be derived from geraniol or linalool by action with dilute H2SO4, according to Wikipedia.

I had another thought as well. 2-Methyl maleic acid (citraconic acid) could possibly be cheaper than normal maleate, as citraconic anhydride is obtained by dry distillation of citric acid. It is also a liquid at room temperature and dehydrates spontaneously, possibly facilitating easier esterification.

[Edited on 4/11/2025 by chempyre235]

[Edited on 4/11/2025 by chempyre235]

[Edited on 4/11/2025 by chempyre235]
View user's profile View All Posts By User
imidazole
Harmless
*




Posts: 46
Registered: 18-10-2014
Location: Massachusetts, USA
Member Is Offline

Mood: Radical

[*] posted on 11-4-2025 at 10:37


urushiol isn't as bad of a suggestion as you might initially think, given how lacquer is made, maybe other pinacols/phenols could be a source of inspiration for the process
View user's profile Visit user's homepage View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2927
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 11-4-2025 at 16:14


Yeah I think urushiol is pretty interesting since the ortho-bonded aromatics are often low-melting. It also appears to be surprisingly abundant, in that there is enough to be used to make things through traditional processes. The main obstacle might be its instability. If it can be obtained directly in good quantities, it's perfect. Most of the urushi lacquer I see is pretty expensive, though.

Pantoic acid seems pretty nice but I don't know how abundant it is. I considered isosorbide and furan-2,5-dimethylol but they seem too rigid (cyclic). The glycols are probably too light.
Quote: Originally posted by bnull  

Edit: Oops, forgot the review: Abhishek R. Varma, Bhushan S. Shrirame, Sunil K. Maity, Deepti Agrawal, Naglis Malys, Leonardo Rios-Solis, Gopalakrishnan Kumar, Vinod Kumar. Recent advances in fermentative production of C4 diols and their chemo-catalytic upgrading to high-value chemicals[J]. Chinese Journal of Catalysis, 2023, 52: 99-126.

[Edited on 9-4-2025 by bnull]
The suggestion of C4-fermentation gave me another idea. See, the aldol dimerization of aldehydes gives branched compounds. As imidazole mentioned, branched compounds are not that widespread in nature. But the aldol dimer of acetaldehyde is not really branched. The obvious next choice is butyraldehyde (as usual, C3 products are rare, except those derived from glyceraldehyde). Apparently, biobutanol production is already approaching industry:
https://marinefuels.totalenergies.com/news/press-release/tot...

And the dimer of butyraldehyde leads to the highly branched alcohol 2-ethyl-1,3-hexanediol, or "etohexadiol", already an item of commerce (but at an unfavorable price of about $10/kg) and a former insect repellent.
http://en.wikipedia.org/wiki/Etohexadiol
It is apparently not too prone to dehydration, since the original authors distilled it over an iodine catalyst to achieve this. The aldol addition happens easily in the condensed phase:
https://www.sciencemadness.org/whisper/files.php?pid=700256&...

Dehydration is probably averted by reducing before distillation.

Quote:
2-Methyl maleic acid (citraconic acid) could possibly be cheaper than normal maleate, as citraconic anhydride is obtained by dry distillation of citric acid.

Furfural is actually super cheap at the industrial scale (<~$1.5k/metric tonne) and it's easily produced from organic waste.
https://www.imarcgroup.com/furfural-pricing-report
https://en.wikipedia.org/wiki/Furfural
Quote:
Furfural is derived only from dried biomass. In addition to ethanol, acetic acid, and sugar, furfural is one of the oldest known organic chemicals available readily purified from natural precursors.




Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
imidazole
Harmless
*




Posts: 46
Registered: 18-10-2014
Location: Massachusetts, USA
Member Is Offline

Mood: Radical

[*] posted on 11-4-2025 at 16:36


I think Urushiol itself is a low supply / high demand product, but I was thinking in the ortho-bonded aromatics direction. I actually thought about Acetaldehyde, but dropped it for the reason mentioned. I can actually say there has been a lot of reading about Cellulostic Butanol recently, and it could become much more available.

Unrelated, but back in highschool I had this pie-in-the-sky idea to basically farm algae for biobutanol production, after a base treatment to pre-treat the algae, and then use synthetic humic acids as a amine scavenger to bring ph back up and split the cellulose from the fatty acids, and getting fertilizer, Butanol, and fatty acids, so I'm a huge fan of C-4 chemistry

I still think Lactic acid > Lactide > dipropylene glycol could be an interesting way to get the C-3 chemistry rolling, but I'm a fan of the way things are going with aldols.
View user's profile Visit user's homepage View All Posts By User
chempyre235
Hazard to Others
***




Posts: 216
Registered: 21-10-2024
Location: Between Nb and Tc
Member Is Offline

Mood: Quite distracted

[*] posted on 12-4-2025 at 08:35


What about o-coumaric acid? It could be added to the copolymer as a UV-absorbing agent. It also has the ability to crosslink, and can be made from hydrolysis of coumarin, which has several synthetic routes, and is found in a wide variety of plants.

Sporopollenins found in nature use p-coumarin and some other coumarin-based antioxidants for this purpose.

[Edited on 4/12/2025 by chempyre235]
View user's profile View All Posts By User
chempyre235
Hazard to Others
***




Posts: 216
Registered: 21-10-2024
Location: Between Nb and Tc
Member Is Offline

Mood: Quite distracted

[*] posted on 14-4-2025 at 07:56


Quote: Originally posted by clearly_not_atara  

Pantoic acid seems pretty nice but I don't know how abundant it is.

Apparently, pantoic acid is a biosynthetic intermediate in the process that produces vitamin B5 (pantothenic acid). This process is already exploited by bioengineers to yield isobutanol.

I don't have access, but I did find an article from Springer that covers this.
https://link.springer.com/article/10.1007/BF00182178

PubChem entry for pantolactone:
https://pubchem.ncbi.nlm.nih.gov/compound/989

Also, here is the Wikipedia page on a-ketoisovaleric acid, the precursor to pantoic acid.
https://en.wikipedia.org/wiki/Ketoisovaleric_acid

Perhaps another synthetic route to the lactone could be had by using a furan derivative as the starting ingredient.

Pantolactone.png - 2kB

@clearly_not_atara, what do you think of the possibility of terpin?


Terpin.png - 5kB

[Edited on 4/14/2025 by chempyre235]
View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2927
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 16-4-2025 at 19:09


chempyre: miller1993, attached. But this appears to be a conventional chemical synthesis, not a fermentation.

I really wanted some better guide to what I should hope for out of a diol. So I searched through the citations of Carter et al's original paper. However, they mostly simply copied the chemistry that Carter had used! With one exception, where linear straight-chain dicarboxylic acids were used, with a cure temperature of 160 C:
https://pubs.rsc.org/en/content/getauthorversionpdf/c5gc0091... (open access)

So I found the PhD thesis that the paper was based on:
https://openresearch.surrey.ac.uk/esploro/outputs/doctoral/T...

But here the only alternatives listed are all cyclic anhydrides. They don't work well, obviously, since the maleic chemistry was the signature advancement. And there is no explanation for why the anhydride was used in one case and the diacid in the other, though the original report using the anhydrides may tell us something:
https://www.sciencedirect.com/science/article/abs/pii/S00323... (boquillon2000, attached)

The essential requirement is: the bis-maleoyl ester diacid -- what I am tempted to call a "bimaleate" by analogy to a bicarbonate -- must be a liquid. It is also good for it to be "flexible", though we are not sure what that means; maybe a glycol or catechol is already flexible enough because of the bimaleate pattern.

In general, branched motifs and cis-oriented double bonds lower the mp of a compound, while cyclic structures and trans-oriented double bonds raise it. This is a very rough guide. Based on this, I like etohexadiol, and neopentyl glycol (neé pantoic acid).

So: is the bimaleate of etohexadiol a liquid at room temperature? What about that of the other alcohols?

Quote:
I still think Lactic acid > Lactide > dipropylene glycol

I have a hard time imagining how lactide is reduced to dipropylene glycol? In fact, reducing esters to ethers is very tricky. I did find one example which used NaBH4 + BF3 in mixed solvents:
https://pubs.acs.org/doi/pdf/10.1021/jo01053a054
This is a little too advanced...

Attachment: miller1993.pdf (668kB)
This file has been downloaded 155 times

[Edited on 17-4-2025 by clearly_not_atara]

[Edited on 17-4-2025 by clearly_not_atara]

Attachment: boquillon2000.pdf (199kB)
This file has been downloaded 159 times

[Edited on 17-4-2025 by clearly_not_atara]




Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
imidazole
Harmless
*




Posts: 46
Registered: 18-10-2014
Location: Massachusetts, USA
Member Is Offline

Mood: Radical

[*] posted on 16-4-2025 at 19:47


I was thinking catalytic hydrogenation and dehydration in one go, but from further research, it turns out you can go from lactic acid to propylene glycol directly, without needing to first reduce it to an ester in decent yields, which might be easier than trying to dehydrate it in the first place. (https://pmc.ncbi.nlm.nih.gov/articles/PMC5838540/)



Quote: Originally posted by clearly_not_atara  
chempyre: miller1993, attached. But this appears to be a conventional chemical synthesis, not a fermentation.

I really wanted some better guide to what I should hope for out of a diol. So I searched through the citations of Carter et al's original paper. However, they all simply copied the chemistry that Carter had used! This is an interesting example of the dysfunction of modern scientific research: it is just easier to get funding and support if you are doing something repetitive. I can't find anyone testing other crosslinkers, even just substituting the diol.

So I found the PhD thesis that the paper was based on:
https://openresearch.surrey.ac.uk/esploro/outputs/doctoral/T...

But here the only alternatives listed are all cyclic anhydrides. They don't work well, obviously, since the maleic chemistry was the signature advancement. And there is no explanation for why the anhydride was used in one case and the diacid in the other, though the original report using the anhydrides may tell us something:
https://www.sciencedirect.com/science/article/abs/pii/S00323... (boquillon2000, attached)

The essential requirement is: the bis-maleoyl ester diacid -- what I am tempted to call a "bimaleate" by analogy to a bicarbonate -- must be a liquid. It is also good for it to be "flexible", though we are not sure what that means; maybe a glycol or catechol is already flexible enough because of the bimaleate pattern.

In general, branched motifs and cis-oriented double bonds lower the mp of a compound, while cyclic structures and trans-oriented double bonds raise it. This is a very rough guide. Based on this, I like etohexadiol, and neopentyl glycol (neé pantoic acid).

So: is the bimaleate of etohexadiol a liquid at room temperature? What about that of the other alcohols?

Quote:
I still think Lactic acid > Lactide > dipropylene glycol

I have a hard time imagining how lactide is reduced to dipropylene glycol? In fact, reducing esters to ethers is very tricky. I did find one example which used NaBH4 + BF3 in mixed solvents:
https://pubs.acs.org/doi/pdf/10.1021/jo01053a054
This is a little too advanced...



[Edited on 17-4-2025 by clearly_not_atara]

[Edited on 17-4-2025 by clearly_not_atara]
View user's profile Visit user's homepage View All Posts By User