mercury and hydrogen sulfide
i've been making mercury for a while by ozcanium's method
https://www.youtube.com/watch?v=ZCFNJw86JaQ&t=183s
but the h2s corrodes my fume hood fan duct and i constantly have to replace it.
nilered does a similar reaction but makes no mention of h2s https://youtu.be/0e78I9_oH1E?si=AIzDZII36zMsdu8g&t=373
is there a way to slow/stop h2s production? will more hydroxide work?
thank you
|
|
|
j_sum1
Administrator
      
Posts: 6475
Registered: 4-10-2014
Location: Limbo
Member Is Offline
Mood: Just got through yet another "take this job and shove it" moment.
|
|
Can you scrub the H2S?
Pass it through a solution of NaOH
Given the nature of H2S, I would be inclined to use two scrubbers in series, probably using an aquarium bubbler to get a fine dispersion of bubbles.
The first would be in a flask. The second a large beaker. I would put a wet cloth over the beaker to catch anything remaining, and have that in a
fume hood.
Always with H2S, have your work area littered with test strips made of filter paper soaked on CuSO4. Smell is a good indicator that something is
escaping. But if your test strips darken then you know where it is escaping.
The good thing about H2S is that it smells bad and the danger threshold is higher than the smell threshold.
|
|
|
Texium
Administrator
      
Posts: 4748
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline
Mood: Seeking gainful employment
|
|
Bleach is even better than NaOH as a scrubber. It will oxidize the H2S,
rendering it odorless.
|
|
|
Texium
|
Thread Moved 17-9-2025 at 18:26 |
Radiums Lab
Hazard to Others
 
Posts: 299
Registered: 18-3-2025
Location: India
Member Is Offline
Mood: Experiencing the elegance of science.
|
|
You can use moist lead acetate strips for more effective test
Water is dangerous if you don't know how to handle it, elemental fluorine (F₂) on the other hand is pretty tame if you know what you are doing.
|
|
|
j_sum1
Administrator
      
Posts: 6475
Registered: 4-10-2014
Location: Limbo
Member Is Offline
Mood: Just got through yet another "take this job and shove it" moment.
|
|
True. But I prefer to avoid lead salts when there are alternatives.
|
|
|