Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Comparison of (relatively) inert atmospheres for preventing oxidation?
math
Hazard to Others
***




Posts: 114
Registered: 21-7-2006
Member Is Offline

Mood: No Mood

[*] posted on 26-10-2025 at 16:13
Comparison of (relatively) inert atmospheres for preventing oxidation?


Hi, I did think about ordering (from best to worst), atmospheres that would react the least with metals and paper/inks over time.

Argon (dry)
Argon (humid)
Nitrogen (dry)
Nitrogen (humid)
CO2 (dry)
CO2 (humid)
Air (dry)
Air (humid)

This is assuming same temperature, no UV.
I assume most molds won't grow without oxygen and water?

Advice welcome, thank you.
View user's profile View All Posts By User
BromicAcid
International Hazard
*****




Posts: 3324
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline

Mood: Rock n' Roll

[*] posted on 26-10-2025 at 19:03


In terms of ink, a CO2 atmosphere could wreak havoc with some dye based inks. It also would affect the acidity of the paper leading to breakdown.

Helium is another option though the crap from the big box stores has enough oxygen mixed in to make it useless for an inert atmosphere. If you want to throw caution to the wind don't forget hydrogen, methane, ethane, propane, and butane.




Shamelessly plugging my attempts at writing fiction: http://www.robvincent.org
View user's profile Visit user's homepage View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3947
Registered: 8-2-2015
Member Is Offline


[*] posted on 26-10-2025 at 19:58
I do not know the answer but .....


I'm sure that atmospheres for archival have been well tested and documented.
personally I know very little other than that there is no one-size-fits-all solution;
some things want to be as dry as possible to prevent molds, fungi, bacteria or oxidation
others need a certain humidity level to not dry up and crumble, etc.

I guess that ideally you need to specify your requirements more tightly.
(age, paper, ink and binding type, with illustrations ?
Is it to preserve/seal/store or for frequent access ?
would imaging and digital storage be better ?

the ultimate solution will depend upon available funds vs value to you of the items to be preserved.




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
Radiums Lab
Hazard to Others
***




Posts: 299
Registered: 18-3-2025
Location: India
Member Is Offline

Mood: Experiencing the elegance of science.

[*] posted on 26-10-2025 at 23:58


I personally would go with Argon(dry) because of following reasons:
- It's pretty cheap compared to other noble gasses
- You can store literally anything from alkali metals to halogens without a doubt
- It's heavier than air, so you don't risk it leaving the container pretty easily
_ N2 cannot be used with metals such as Li
_ CO2 atmosphere does not support alkali metals and sometimes alkaline earth metals too.
_ O2 and H2O no need to mention( the reason why glove boxes exist!)




Water is dangerous if you don't know how to handle it, elemental fluorine (F₂) on the other hand is pretty tame if you know what you are doing.
View user's profile View All Posts By User
Keras
International Hazard
*****




Posts: 1148
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 27-10-2025 at 00:36


I agree that argon is a good choice. Nitrogen works most of the time, but argon covers about everything and is not much more expensive, so go for it directly.
View user's profile View All Posts By User
macckone
Dispenser of practical lab wisdom
*****




Posts: 2214
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 2-11-2025 at 10:50


Argon is best but nitrogen is cheaper.
Neon may be cheaper than argon in some places and is just as inert as argon.
View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2927
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 2-11-2025 at 19:01


Nitrogen (dry) definitely beats argon (humid), except under very weird circumstances. Argon is more useful in general because it is heavier than air whereas nitrogen is lighter, so argon will tend to sit in the flask nitrogen... won't! :P

Also I would be pretty surprised to find neon cheaper than argon anywhere, it has a very very low bp and atmospheric concentration... it's very common in the Universe overall but only in places where helium is even more common.

Krypton might also be useful in some circumstances since it has a stronger "blanket" effect than argon. But it is quite expensive.

[Edited on 3-11-2025 by clearly_not_atara]




Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
Keras
International Hazard
*****




Posts: 1148
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 2-11-2025 at 22:58


The noble gases are very scarce on Earth.
Helium has escaped long ago, and the only source of it are alpha rays of radioactive isotopes.
Argon is *the* exception because it is heavier than air and results from the decay of radioactive potassium 40.
The other ones are only found as traces.
View user's profile View All Posts By User
Mateo_swe
National Hazard
****




Posts: 590
Registered: 24-8-2019
Location: Within EU
Member Is Offline


[*] posted on 7-11-2025 at 07:21


Any of the noble gases would be good as they are so unreactive with everything.
The fact that argon is heavier than air, commonly avaliable and cheap thanks to being used in welding make it highly useful for anyone wanting a smaller oxygen free environment.

The helium sold at party stores for baloons is often inhaled to get that funny voice so im not suprised they mix in some air to make it slightly less dangerous.
View user's profile View All Posts By User
FableP
Harmless
*




Posts: 16
Registered: 26-7-2023
Member Is Offline

Mood: No Mood

[*] posted on 9-11-2025 at 16:49


There are fountain pen inks that are specifically designed to be archival.
Presumably the greater potential for degradation would be the paper. I don't think its just oxidation & biological processes that attack paper over time, but UV light as well.
Its common to view ancient artefacts in low light environments to protect against degradation.
Argon seems to be the noble gas of choice for manuscript preservation.
View user's profile View All Posts By User