Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: making lithium from its hydroxide
symboom
International Hazard
*****




Posts: 1145
Registered: 11-11-2010
Location: Wrongplanet
Member Is Offline

Mood: Doing science while it is still legal since 2010

mad.gif posted on 4-5-2011 at 14:01
making lithium from its hydroxide


does anyone know how or if lithium can be made from its hydroxide like sodium and potassium can. it seems like it decomposes to lithium oxide some sources say but its melting point is a little above sodium hydroxide now its done with lithium chloride in propylene carbonate

462 °C melting point
924 °C decomp.

[Edited on 5-5-2011 by symboom]
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 5-5-2011 at 05:14


The only way Li is produced industrially is by the electrolysis of LiCl in a eutectic mixture with other salts.

In the past some ‘chemical’ routes have been used by heating the hydroxide, carbonate or chloride with strong reducing agents (Na, K, Mg, Ca, Al) in forcing conditions (high temperature, vacuum etc). None of these methods are now realistic.

Lithium metal is harder to obtain generally speaking than Na or K. Or Mg and Ca. Small amounts can be prised out of Li batteries (fresh, unused) and there are numerous web pages and UToobs dedicated to that subject.
Avoid shorting! :o
View user's profile View All Posts By User
Saerynide
National Hazard
****




Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline

Mood: Ionic

[*] posted on 5-5-2011 at 06:00


Ha! That was a fun project in my youngin' days - did that when the batteries first hit the market before youtube and tutorials for that was out :D

Definately avoid shorting. Be prepared for some very red fingers if youre not careful. Even a short of a split second or two causes the battery to get hot enough to give a rather painful burn :(




"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to... satisfy any applicable law, regulation or legal process"
View user's profile View All Posts By User
Waffles SS
Fighter
*****




Posts: 1019
Registered: 7-12-2009
Member Is Offline


[*] posted on 5-5-2011 at 10:12


Melting point of Lithium Nitrate:255c
Seems it is better to make Lithium metal by electrolysis but i think Nitrogen Dioxide(mother fuc*er) will produce
View user's profile View All Posts By User

  Go To Top