making tablets
Can anybody suggest a suitable hardening agent to help my fertilizer tablets remain intact. I am using a tablet press which forms 20g fertilizer
tablets (using a mix of ibdu, potassium sulphate, monoammonium phosphate and magnesium sterate and calicum lignosulphonate). The calcium
lignosulphonate was meant to be a binder keeping the tablets hardr, but is not working. Any ideas would be appreciated.
[Edited on 26-3-2004 by plantdoctor]
|
|
|
Mr. Wizard
International Hazard
   
Posts: 1042
Registered: 30-3-2003
Member Is Offline
Mood: No Mood
|
|
What is "ibdu"? Lignium sulphonate (sp?) is a liquid used to spray on loose soil to consolodate it for use as a temporary road. Calcium
lignosulphonate would be a dry material, right? Are all the materials to be consolodated in the dry state and at room temperatures? Magnesium
Stearate is a 'soap' often used in pills. I noticed you didn't have any Magnesium Oxide in the mix. It would react with the ammonium
phosphate and a trace of moisture to form a very solid plaster, used in dental casting. Maybe if you added more Magnesium Stearate, Magnesium Oxide, a
trace of moisture and increased the pressure on the press, it would form a hard pill. You might try using a hydraulic jack and make yourself a reall
strong press.
|
|
|
axehandle
Free Radical
   
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
Well, I've done it, and this is my hydraulic press. I used aluminum (Fortal alloy (MG-Al)) for the bars, and 8/8 steel for the ´tensile carrying
bars.

[Edited on 2004-3-27 by axehandle]
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
|
Mr. Wizard
International Hazard
   
Posts: 1042
Registered: 30-3-2003
Member Is Offline
Mood: No Mood
|
|
It's a nice looking press. Is the curvature of the threaded rods due to the camera lens or did the get a little bent in use? I need to make one
like that. I don't have any nice chunks for the cross bars yet.
|
|
|
axehandle
Free Radical
   
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
The curvature is due to the camera. I calculated the maximum tensile stress on the steel to be 36 tons, the jack only gives 12... but it's enough
to make BP cakes with a density of 1.8 g/cc.
Edit: Oh, btw, the steel threaded rods are M16 in diameter. I had to pay through the nose to get 8/8 quality (about 40 EUR for all 4).
[Edited on 2004-3-27 by axehandle]
[Edited on 2004-3-27 by axehandle]
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
|
plantdoctor
Harmless
Posts: 3
Registered: 25-3-2004
Location: australia
Member Is Offline
Mood: I'm excited
|
|
making tablets
Thanks for your comments. ibdu is isobutylidene diurea. It is produced through the condensation of urea and isobutyaldeyde. It is used in agriculture
as a slow release form of nitrogen. Calcium Lignosulphonate is a powder (byproduct from paper making mills i believe). All products are combined at
room temperature. I will try the Mag Oxide. Would Magnesium carbonate work also?
| Quote: | Originally posted by Mr. Wizard
What is "ibdu"? Lignium sulphonate (sp?) is a liquid used to spray on loose soil to consolodate it for use as a temporary road. Calcium
lignosulphonate would be a dry material, right? Are all the materials to be consolodated in the dry state and at room temperatures? Magnesium
Stearate is a 'soap' often used in pills. I noticed you didn't have any Magnesium Oxide in the mix. It would react with the ammonium
phosphate and a trace of moisture to form a very solid plaster, used in dental casting. Maybe if you added more Magnesium Stearate, Magnesium Oxide, a
trace of moisture and increased the pressure on the press, it would form a hard pill. You might try using a hydraulic jack and make yourself a reall
strong press. |
|
|
|
Mr. Wizard
International Hazard
   
Posts: 1042
Registered: 30-3-2003
Member Is Offline
Mood: No Mood
|
|
Is this recipe one that has worked before? The magnesium oxide is mentioned because it, when mixed with ammonium phosphate, form a dental casting
plaster. I'm not sure what effect if any it would have on dry powders. How much pressure does your tablet press exert? The fertilizer spikes
I've seen can be hammered into the ground, which indicates an extreme pressure in their formation. They have a glazed look on their exterior,
almost like a rock.
I suspect it will take a big hydraulic jack (20 to 30 tons) , compressing a cylinder of powder 25mm in diameter or less, contained in a strong mould.
This is pure guessing on my part.
You might try hammering some of the components in a narrow pipe to see if they will consolodate.
|
|
|
axehandle
Free Radical
   
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
About the cake diameter and the jack: No a 12 ton one is enough to press BP cakes with a diameter of 75mm to a density of 1.8g/cc.
Since I basically had to hang my full body weight on the lever to squeeze the last millimeter, I've since upgraded to a 20 ton jack.
<b>Very</b> powerful.... 
And very heavy to carry home.... oooh, I remember how my back ached...
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
|
ordenblitz
Hazard to Others
 
Posts: 259
Registered: 18-7-2004
Location: Northwest
Member Is Offline
Mood: Bohr'd
|
|
Magnesium stearate is used as a lubricant in tabletting. It makes the tablet easier to eject from the die and tends to keep the material from sticking
to the punch faces, which causes capping. A lubricant will also aid the compression by reducing bridging in the die and promote better density with an