Cleaning silver electrodes


I notice that silver electrodes eventually turn black. The black stuff must be silver oxide (AgO2). Silver oxide is a mild oxidising agent so I tried soaking the electrodes in a solution of sodium metabisulfite (a reducing agent) but no reaction occurs. Would I have better luck by soaking them in an acid?
View user's profile View All Posts By User
hissingnoise
International Hazard
*****




Posts: 3940
Registered: 26-12-2002
Member Is Offline

Mood: Pulverulescent!

[*] posted on 6-5-2012 at 07:47


Most probably! Dilute HNO<sub>3</sub>, most likely . . .
View user's profile View All Posts By User
barley81
Hazard to Others
***




Posts: 481
Registered: 9-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 6-5-2012 at 10:34


Clean them like you clean tarnished silver in the kitchen: dissolve some baking soda in water, put an aluminum foil sheet in the solution, and then drop in the silver. The aluminum reduces the silver compounds that are adhering to the silver.

@hissingnoise when did you stop being Pulverulescent?

[Edited on 6-5-2012 by barley81]
View user's profile View All Posts By User
phlogiston
International Hazard
*****




Posts: 1383
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline

Mood: pyrophoric

[*] posted on 6-5-2012 at 13:45


The black layer is usually silver sulfide actually. Silver does not tarnish in oxygen.



-----