Carbon from Batteries
How do you get the carbon rods out of a battery? Do you just cut them up and take it out?
|
|
|
Saerynide
National Hazard
  
Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline
Mood: Ionic
|
|
Use diagonal cutters and peel up the rim of the can, then make vertical cuts on the pulled up rim and peel the rim away from from the can. Push the
contents out from the bottom and pull off that plastic cap thing you see inside. Most of the time, the carbon rod comes out with it. If youre not
lucky and its stuck, then you gotta dig all the stuff out to get the rod.
"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to...
satisfy any applicable law, regulation or legal process"
|
|
|
Geomancer
Hazard to Others
 
Posts: 228
Registered: 21-12-2003
Member Is Offline
Mood: No Mood
|
|
Yup, cut 'em up and take 'em out. Use "standard" or "heavy duty" (zinc chloride) cells, not the alkaline ones, which
don't have a rod. The cylindrical cells have a plastic wrapper over the zinc anode, which goes on top of a cardboad separator. The anode is
largly consumed once the cell is exhausted, and you may be able to take it apart with just a pair of pliers, or even strong fingers (not recomended).
Be warned, the rod seems to not like high current densities (at least as an anode), and erodes quickly.
|
|
|
kryss
Hazard to Self

Posts: 77
Registered: 11-7-2003
Location: N Ireland
Member Is Offline
Mood: No Mood
|
|
cheap ones - Tescos - are using a carbon powder paste.
|
|
|
Cyrus
Hazard to Others
 
Posts: 397
Registered: 24-4-2004
Location: Ancient Persia
Member Is Offline
Mood: No Mood
|
|
The rods are mixed with clay or a similar binder IIRC, have you ever tried to grind them up?- they certainly are not pure graphite! more like
gravelite. 
Don't throw out the black "junk" - it's manganese dioxide, which needs cleaning as it is impure. There is more in unused
batteries of course. And save the dull metal inner liner while you're at it, don't waste zinc!
|
|
|
TheBear
Hazard to Self

Posts: 78
Registered: 17-10-2002
Location: Sweden
Member Is Offline
Mood: distilled
|
|
I've recently opened about 20 old carbon zinc batteries which have supplied me with X hundreds of grams of MnO2 (contaminated with MnO(OH),
NH4Cl, ZnCl2). And 20 decent carbon electrodes aswell.
Any ideas for how to purify this? I read that MnO2 is suitable anode material for use in ClO3- cell. But they used Mn(NO3)x.
Can one cast an anode using molten MnO2?
[Edited on 27-9-2004 by TheBear]
|
|
|
neutrino
International Hazard
   
Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline
Mood: oscillating
|
|
Zinc and ammonium chloride are highly soluble in water while MnO<sub>2</sub> is insoluble, as MnO(OH) should be, so you can simply filter
this solution. The remaining (hydr)oxide(s) can easily be dizzolved in acids (except MnO<sub>2</sub> and HNO<sub>3</sub> to form the respective salts (although this will release a lot of corrosive fumes, so
be careful).
|
|
|
S.C. Wack
bibliomaster
   
Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline
Mood: Enhanced
|
|
On the off-topic question of the black powder, repeated washing might get rid of nearly all of the NH4Cl, if any is present, but some seems to be
adsorbed. I say this because I've heated some with KOH after careful washing and still got a detectable NH3 odor. Its not much though. What is it
adsorbed on? -
There is also acetylene black in there. I measured it once but forget exactly how much - lets say 10% of the total weight of the powder. Easy to
figure - make some MnCl2 or MnSO4. Given that the MnO2 has something like 2.5X the density of the C, a surprising amount by volume isn't MnO2.
"Fractional decantation" might get rid of much of the C if this is desired.
I have horrible memories of the messes made in my pre- pottery supply days.
|
|
|
JohnWW
International Hazard
   
Posts: 2849
Registered: 27-7-2004
Location: New Zealand
Member Is Offline
Mood: No Mood
|
|
MnO2 decomposes without melting at less than 230ÂșC to Mn2O3, unfortunately.
John W.
|
|
|
sarcosuchus
Harmless
Posts: 25
Registered: 16-9-2004
Location: in server hell
Member Is Offline
Mood: sleepy
|
|
if you need carbon rods there is all ways a welding shop were you can get what you need for cheap i found out that the one near me can order 2"
thick 3 foot long rodsfor $80 ish or so that was for some weird super high temp applications.. just fyi
famous last words\"hold my beer and watch this\"
|
|
|
MadHatter
International Hazard
   
Posts: 1371
Registered: 9-7-2004
Location: Maine
Member Is Offline
Mood: Enjoying retirement
|
|
Carbon rod
WOW ! That's a monster carbon rod ! My gouging rods are 3/8" x 12".
What's the name of the place where you found these babies ?
From opening of NCIS New Orleans - It goes a BOOM ! BOOM ! BOOM ! MUHAHAHAHAHAHAHA !
|
|
|
BromicAcid
International Hazard
   
Posts: 3324
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline
Mood: Rock n' Roll
|
|
You can also get nice graphite rods from jewlery suppliers, they use them to stir molten gold and the like. They are cheap, somewhat highly pure, and
can be somewhat large.
I also got carbon rods out of batteries, I bought a few of those lantern style batteries from a dollar store. Inside each was four long batteries in
a series. Each battery had a somewhat large graphite rod, too bad they don't hold up good in electrolysis.
[Edited on 10/4/2004 by BromicAcid]
|
|
|
MadHatter
International Hazard
   
Posts: 1371
Registered: 9-7-2004
Location: Maine
Member Is Offline
Mood: Enjoying retirement
|
|
Lantern batteries
BromicAcid, I also pulled those rods out of lantern batteries. Don't hold
up worth a damn during electrolyis. I'll stick with the gouging rods.
From opening of NCIS New Orleans - It goes a BOOM ! BOOM ! BOOM ! MUHAHAHAHAHAHAHA !
|
|
|
Kamisama
Harmless
Posts: 9
Registered: 27-4-2005
Member Is Offline
Mood: SilentButDeadly
|
|
Obtaining electrodes.
I read somewhere that you can obtain electrodes from things such as a 12 volt lantern battery.
Anyone know more detail on this? I have somewhat forgotten details on it.
It's quite an interesting thing to me because I have a bunch of old batteries laying around.
Reddi whip is funny. ^_^
|
|
|
darkflame89
Hazard to Others
 
Posts: 255
Registered: 1-3-2004
Location: With probability 1, "somewhere" in this
Member Is Offline
Mood: No Mood
|
|
Batteries have zinc cover, right? Would this work all the same if one had threw the entire battery into acid, wait for the zinc metal to dissolve. Then you will be left be a whole lot of mess, of which you can filter to get the
carbon rod and other insoluble products..
Ignis ubique latet, naturam amplectitur omnem.
|
|
|
Esplosivo
Hazard to Others
 
Posts: 491
Registered: 7-2-2004
Location: Mediterranean
Member Is Offline
Mood: Quantized
|
|
If you try dissolving the whole thing in hydrochloric acid it will dissolved resulting in the remaing funk being starch (used as a binder) and some
graphite powder IIRC. The Mn compounds will react with the hydrochloric acid (MnO2 will liberate chlorine), therefore do this reaction outside if you
do intend to do it. I find it quite a loss of acid, although if acid is cheap and you have a well ventilated area it might yield some very good, clean
graphite rods. Hope this helps.
Theory guides, experiment decides.
|
|
|
12AX7
Post Harlot
   
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Right tool, totally wrong application... just get some pliers, they slide out of the MnO2 gunk easily.
Tim
|
|
|
tumadre
Hazard to Others
 
Posts: 172
Registered: 10-5-2005
Member Is Offline
Mood: No Mood
|
|
You must burn off the substance that permiates the carbon rod, I heat the rod to red heat before I use them. after this you can soak the rod in the
desired material-such as oil for some electrocem. cells
mn3o4 melts at 940C decomposes to mno at 1020c all decomposition of mnx make mno which melts at 1700c
try a thermite reaction with Mg-Al or NA
|
|
|
MadHatter
International Hazard
   
Posts: 1371
Registered: 9-7-2004
Location: Maine
Member Is Offline
Mood: Enjoying retirement
|
|
Battery carbon rods
If you intend to use the rods in an electrolysis cell, it might be a good idea to soak them in linseed
oil for a few days prior to use. This process certainly slows down the erosion rate on my gouging
rods.
From opening of NCIS New Orleans - It goes a BOOM ! BOOM ! BOOM ! MUHAHAHAHAHAHAHA !
|
|
|
Madandcrazy
Hazard to Others
 
Posts: 117
Registered: 11-5-2005
Member Is Offline
Mood: annoyed
|
|
Use carbon rods (from Batteries with MnO2/ZnCl2) in an electrolysis, it might be a good idea because the carbon can be easy removed from the liquid
and end products.
Certainly a slow erosion of the rods, only a catalyst function for the electrolysis ?
|
|
|