Hello all,
I was just wondering if anyone knew off the top of their head what the oxidation like water spots on galvanized sheet metal are. They are a white
color and are spread all over the sheet metal in the emission accelerators I’m build at work for a pharmaceutical company. Anyway, I was wondering
if there was a good solvent or even a solution I could mix to remove this oxidation. I would like to avoid having to buff it out with a cotton wheel
and some jeweler's rouge. I have access to methyl ethyl ketone, and hydrochloric acid. But I can always go buy other chemicals if necessary.
Sincerely,
Tom Hagen
[Edited on 1-8-2004 by chemoleo]
N/A
|
|
|
Hang-Man
Hazard to Self

Posts: 70
Registered: 16-1-2004
Location: Canada
Member Is Offline
Mood: Wasted
|
|
Sounds like Zinc Oxide, a fine white powder. If you could scrape some off and heat it, it should turn yellow. Confirming zinc oxide.
I would clean it with dilute HCl, as it attacks zinc and its oxides. Make sure its quite dilute though, the zinc coating could be quite thin.
|
|
|
chemoleo
Biochemicus Energeticus
   
Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline
Mood: crystalline
|
|
The only problem being, those spots will return... unless you dissolve away the whole Zn layer. But then, what guarantee do you have that the
underlying metal won't get dissolved?
Besides, normally metal IS galvanised with Zn precisely in order to prevent oxidation of the metal underneath. So you wouldnt want to
dissolve it away!
Never Stop to Begin, and Never Begin to Stop...
Tolerance is good. But not with the intolerant! (Wilhelm Busch)
|
|
|
hpc
Harmless
Posts: 3
Registered: 15-7-2004
Location: Valdosta,GA. USA
Member Is Offline
Mood: awestruck
|
|
Tom, I know this might seem very "unscientific", but have you tried good ole WD40 ? I use it to remove water spots from stainless steel. it
might work on your galvanized.
|
|
|
Esplosivo
Hazard to Others
 
Posts: 491
Registered: 7-2-2004
Location: Mediterranean
Member Is Offline
Mood: Quantized
|
|
I think using dilute NaOH solution would work better since it would react with the zinc/zinc oxide layer without reacting with the metal layer beneath
(which I am supposing is iron).
As chemoleo said though, removing the zinc will remove the protection of the metal from oxidation.
Theory guides, experiment decides.
|
|
|
tom haggen
Hazard to Others
 
Posts: 488
Registered: 29-11-2003
Location: PNW
Member Is Offline
Mood: a better mood
|
|
Yes I thought about using some sort of acid to remove the oxides. However, I just want to be cautious because I don't want to remove the whole
galvanized coating. I suppose I could try sodium hydroxide. What if I use a dilute sodium hydroxide solution to remove the oxides and then quickly
rinse with water to prevent decomposition of the whole galvanized layer. Luckily the water spots are not that serious; I don't think they have
penetrated the whole galvanized layer.
[Edited on 30-7-2004 by tom haggen]
N/A
|
|
|
unionised
International Hazard
   
Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
IIRC zinc oxide should dissolve in NH3 soln but the free metal shouln't be attacked.
|
|
|
axehandle
Free Radical
   
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
NH3 sol., let's try it... I love empirism....
Ok, just rubbed my galvanized trash bin with 25% industrial ammonia solution. Result: Zinc layer more shiny, no visible damage to it. Seems it works,
but your mileage may vary...
[Edited on 2004-7-31 by axehandle]
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
|
tom haggen
Hazard to Others
 
Posts: 488
Registered: 29-11-2003
Location: PNW
Member Is Offline
Mood: a better mood
|
|
Ya I tried sodium hydroxide, and it made the surface finish more dull. It did work a little but did not remove all of the water spots. I don't
really know where to get industrial ammonia.