costa
Harmless
Posts: 1
Registered: 18-10-2004
Member Is Offline
Mood: No Mood
|
|
Hexavalent Chromium in Aluminum 6061-T651
Is the chromium found in aluminum 6061-T651 or 5052-H34 hexavalent form? Europe is placing a ban on hexavalent Cr and we need to determine if the
aluminum we use is impacted.
Thanks
Costa
(see http://www.aerospacemetals.com/aluminum.html for technical data)
|
|
|
chemoleo
Biochemicus Energeticus
   
Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline
Mood: crystalline
|
|
You are talking about an ALLOY!!
Which means, it is a mixture of elements, here chromium and aluminium, and NOT a mixture of Al and a chromium SALT (which hexavalent chromium would
be).
Both Al/Cr are in their free elemental state, so the Chromium has no formal charge.
Hence Al-Cr alloys do NOT contain Cr VI+.
So no need to worry here. If anything, the photographics industry will be impacted... and of course poor fools like us
Never Stop to Begin, and Never Begin to Stop...
Tolerance is good. But not with the intolerant! (Wilhelm Busch)
|
|
|
Nerro
National Hazard
  
Posts: 596
Registered: 29-9-2004
Location: Netherlands
Member Is Offline
Mood: Whatever...
|
|
Kiss your dichromate goodbey.
Does this also impair the superconductor industry? I think they use Cr in some of the experimental ceramics.
#261501 +(11351)- [X]
the \"bishop\" came to our church today
he was a fucken impostor
never once moved diagonally
courtesy of bash
|
|
|
Jen
Harmless
Posts: 7
Registered: 26-2-2004
Member Is Offline
Mood: No Mood
|
|
I doubt the semiconductor industry would worry because a) if they're going to be introducing it as a dopant, it will be in pitifully small
quantities b) as far as I know it's only the use/disposal of aqueous hexavalent ions that they're worried about. People try to steer away
from making dissolvable semiconductors or ceramics as it kind of defeats the point.
I'd be more worried about the fact that they don't actually know how hexavalent Cr works, and they haven't got anything to replace it
as far as corrosion protection goes. Every plane you have ever flown on, has (probably) been treated with hexavalent chromium to prevent problems
such as pitting corrosion in aluminium.
|
|
|