[*] posted on 15-9-2014 at 14:55
Liquid metal surface tension change w/ 1 volt


by charging the metal with only 1 volt, the surface oxide level is removed, and the tension drops from 500, to 2.

Can be used for extendable antennas, and maybe liquid circuit connections in rotating bearings

in PNAS soon

http://www.eurekalert.org/pub_releases/2014-09/ncsu-rcs09151...

video at link above
View user's profile Visit user's homepage View All Posts By User
violet sin
International Hazard
*****




Posts: 1497
Registered: 2-9-2012
Location: Daydreaming of uraninite...
Member Is Offline

Mood: Good

[*] posted on 15-9-2014 at 15:07


NICE. I have some galinstan. years back I applied voltage to it, and watched the surface of the metal swirl about one of the electrodes. might have to try that one again when I get a chance. thanks for sharing