burnt element
Harmless
*




Posts: 3
Registered: 3-3-2005
Member Is Offline

Mood: No Mood

[*] posted on 7-3-2005 at 18:59
platinum catalyst


I am interested in doing a thing that calls for this element. I've been browsing a little and my budget is not prepared for the price of platinum.
Is there a replacement with similar properties that doesn't break the bank.
As a side note:
I had a different user name before, I had asked about the separation of KOH in drain opener.
I got a book and have been studying long and hard. I have now gotten into the bio section and am getting anxious for some action.
I must of been crazy not to get involved in chemistry until now. What fun we're having!
View user's profile View All Posts By User
Thermal
Harmless
*




Posts: 41
Registered: 31-1-2004
Member Is Offline

Mood: No Mood

[*] posted on 7-3-2005 at 19:05


Well, it depends on what "thing" exactly you're planning on doing as to weather one catalyst can be satisfactorily substituted for another.
View user's profile View All Posts By User
burnt element
Harmless
*




Posts: 3
Registered: 3-3-2005
Member Is Offline

Mood: No Mood

[*] posted on 7-3-2005 at 19:11


direct reduction of the hydroxyl on the L-ephedrine sulfate sidechain in glacial acetic acid using 70% perchloric acid as a promoter and 5% palladium-on-carbon as the catalyst.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 10-3-2005 at 13:45


Pd or Pt?
View user's profile View All Posts By User
burnt element
Harmless
*




Posts: 3
Registered: 3-3-2005
Member Is Offline

Mood: No Mood

[*] posted on 10-3-2005 at 21:39


Pd is what I would like to use because I have a possible source. I'm just feeling out my options, I noticed that the replies stopped when I announced my intentions.
Somebody told me that I needed a prescription to purchase I2, the otherday at the try and save.
If I was trying to understand chemistry and I understood that I liked to experience the effects of chemicals and I also understood that understanding something is the only way to effectively make an educated decision....

What the fuck was I talking about?
View user's profile View All Posts By User

  Go To Top