tumadre
Hazard to Others
 
Posts: 172
Registered: 10-5-2005
Member Is Offline
Mood: No Mood
|
|
I use lithium-ion polymers in electrochemical cells
Did you ever wonder why lithium-ion batterys are called lithium-ion polymer batterys? The answer is because they have a polymer that allows ions to
go through this thin plastic. It is relativly easy to cut the outside of a lithium battery off and unroll the four layers (two polymer layers, anode,
cathode.
The only problem is cleaning the plastic, any remaining material can be removed with a temporary electrocem. cell using salt water etc.
Now where to get the lithium-ion polymer battery, by definition these batterys are rechargable, you can ask your friends for their dead laptop
batterys; each laptop battery (normaly 8 or 12 cells) has about 4 feet by 2.25 inches of this stuff per cell.
Has anyone tried this?
|
|
|
vulture
Forum Gatekeeper
   
Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline
Mood: No Mood
|
|
If I understand you correctly, you're salvaging the polymer from lithium-polymer batteries to use it as an ion-selective membrane, right? Clever.
You might want to salvage the electrolyte too, as there might be some interesting solvents/ions in there.
One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
|
|
|
Pyridinium
Hazard to Others
 
Posts: 258
Registered: 18-5-2005
Location: USA
Member Is Offline
Mood: cupric
|
|
Any idea what ions besides Li+ the membrane will or won't pass?
I wonder if somebody could design a few experiments around this, to see what does and doesn't go thru it.
|
|
|
neutrino
International Hazard
   
Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline
Mood: oscillating
|
|
It would probably be best to ask the manufacturer of the membrane.
|
|
|
Pyridinium
Hazard to Others
 
Posts: 258
Registered: 18-5-2005
Location: USA
Member Is Offline
Mood: cupric
|
|
| Quote: | Originally posted by neutrino
It would probably be best to ask the manufacturer of the membrane. |
Bah! Experiments are more fun.
|
|
|