technologist
Harmless
Posts: 21
Registered: 1-6-2006
Member Is Offline
Mood: No Mood
|
|
Ammonium Sulphate
I have a process to recover H2SO4 from spent acid dillute stream in any
industry, which is finally converted to Ammonium Sulphate efficiently
without much operating cost.
This Ammonium sulphate is anhydrous.
Now I am looking for either converting it back to conc. H2SO4 & recycle ammonia.
OR use it for further value addition.
Any suggestion is welcome
____________________________________
Visit my Blog - http://profmaster.blogspot.com
|
|
|
chromium
Hazard to Others
 
Posts: 284
Registered: 27-6-2005
Member Is Offline
Mood: reactive
|
|
Sell it as fertilizer.
|
|
|
neutrino
International Hazard
   
Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline
Mood: oscillating
|
|
You could always heat it:
(NH<sub>4</sub> <sub>2</sub>SO<sub>4</sub>
--heat---> NH<sub>3</sub> + NH<sub>4</sub>HSO<sub>4</sub>
That's halfway there. You could decompose it further, but temperatures that high would probably be uneconomical.
|
|
|
chemoleo
Biochemicus Energeticus
   
Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline
Mood: crystalline
|
|
Tsts, neutrino, but how would you seperate the acid from the ammonia? It's something I wondered many a time... and the only thing I can think of is
some separation of mass at high heat, i.e. while the AS is still in the form of NH3, H2O and SO3. Probably would work through ionisation, similar to a
mass spectrometer.
I can't see an easy method though.
[Edited on 7-6-2006 by chemoleo]
Never Stop to Begin, and Never Begin to Stop...
Tolerance is good. But not with the intolerant! (Wilhelm Busch)
|
|
|
MadHatter
International Hazard
   
Posts: 1370
Registered: 9-7-2004
Location: Maine
Member Is Offline
Mood: Enjoying retirement
|
|
Electrolysis
Electrolysis with the separation of the anode and cathode products may be useful. There
is a similar method in industry using a membrane, or bridge for the home chemist, used to
separate sodium chloride. Collecting the ammonia at the cathode could be a problem.
There may not be an easy or feasible solution depending on what you want to achieve.
I offer it only as a possibility.
From opening of NCIS New Orleans - It goes a BOOM ! BOOM ! BOOM ! MUHAHAHAHAHAHAHA !
|
|
|
technologist
Harmless
Posts: 21
Registered: 1-6-2006
Member Is Offline
Mood: No Mood
|
|
Hey Guys,
I am looking for a commercial process not Academic info from Literature or a process which is not feasible beyond lab.
___________________________________
Visit my Blog - http://profmaster.blogspot.com
|
|
|
stoichiometric_steve
National Hazard
  
Posts: 827
Registered: 14-12-2005
Member Is Offline
Mood: satyric
|
|
| Quote: | Originally posted by technologist
Hey Guys,
I am looking for a commercial process not Academic info from Literature or a process which is not feasible beyond lab.
|
very grateful we are, huh?
spoonfeeders unite!
|
|
|