Wood ashes
So i am trying to determine what is in wood ash. I understand there is calcium, potassium, magnesium, and sodium carbonates/oxides. What i have done
so far is burn a large amount of wood and collected the ashes, removed the majority of charcoal bits (there is a few flecks left but not enough to
matter that much) i also soaked the ashes in distilled water, with occasional stirring, filtered and repeated. after doing that 3 times i washed the
ashes with dilute acetic acid, definitely so CO2 released. Did this twice then dried the ashes. I evaporated the wash water (both from distilled water
and dilute acetic acid) i was left with a mix of compounds.
Now my problem is i am left with this gray, powdered sugar like stuff. it isn't water soluble, it doesn't burn, doesn't react with dilute acids, so i
am quite frankly confused at what it could be. I am pretty sure what ever it was was at one point water soluble, other wise it wouldn't have gotten
into the tree.
I live in the north east USA. The ground here is high in clay, acidic, and contains higher levels of uranium than most parts of the country. (uranium
is from the natural deposits under the state) The trees were at least 90-150 years old. (they had started to rot at the top, had to be cut down)
I am known as Napalm to my friends, because once i stick you you, you cant get me to stop until i have talked your ear off (or burned it off, which is
actually more likely)
|
|
|
Detonationology
Hazard to Others
 
Posts: 362
Registered: 5-5-2015
Location: Deep South
Member Is Offline
Mood: Electrophillic
|
|
What size filter did you use? Did the filtrate appear to be relatively clear upon filtering?
“There are no differences but differences of degree between different degrees of difference and no difference.” ― William James
|
|
|
Praxichys
International Hazard
   
Posts: 1063
Registered: 31-7-2013
Location: Detroit, Michigan, USA
Member Is Offline
Mood: Coprecipitated
|
|
In the first few distilled water washes you are likely to find hydroxides and carbonates of sodium and potassium, along with some phosphates.
The acid wash will have removed calcium and magnesium carbonates/hydroxides as the acetate salts.
I'm going to take a wild guess that the bulk of what's left is probably aluminosilicates/K, Na, Ca-silicate/carbonate glass with traces of transition
metal oxides.
[Edited on 10-2-2016 by Praxichys]
|
|
|
nscheffield
Harmless
Posts: 16
Registered: 25-4-2015
Member Is Offline
Mood: No Mood
|
|
the paper had a pore size of 2 µm, how ever i used a cheap coffee filter first to get the majority of the larger stuff out.
the filtrate that came out was clear, granted it had a slight color to it but no noticeable particles or cloudy-ness.
it just seems odd that the majority of the ash is aluminosilicates/K, Na, Ca-silicate/carbonate glass. The mass of what i leached out was not even 10%
by weight of the starting ashes. I am no expert in this particular field so if this is in fact what it is ill take your word for it.
thanks for your guys input
I am known as Napalm to my friends, because once i stick you you, you cant get me to stop until i have talked your ear off (or burned it off, which is
actually more likely)
|
|
|
arkoma
Redneck Overlord
     
Posts: 1763
Registered: 3-2-2014
Location: On a Big Blue Marble hurtling through space
Member Is Offline
Mood: украї́нська
|
|
I've been burning Pecan and Red Oak here in rural SW Arkansas and leaching the ashes. Been getting fairly high quality K2CO3
with rudimentary filtration and two recrystallizations.
"We believe the knowledge and cultural heritage of mankind should be accessible to all people around the world, regardless of their wealth, social
status, nationality, citizenship, etc" z-lib
|
|
|
nscheffield
Harmless
Posts: 16
Registered: 25-4-2015
Member Is Offline
Mood: No Mood
|
|
I just have a habit of wanting to not waste any possible chemical reagent. I keep everything that could possibly be used. Urine for the urea and salt,
pieces of metal (nails from junk fires, soda bottle caps, broken electronic) for iron/copper/zinc/ etc, even the gasses produced from my compost bin
(for ammonia, methane, and hydrogen sulfide)
so not knowing what was left over after leaching bugged the heck out of me. now i need to find a use for aluminosilicates/K, Na, Ca-silicate/carbonate
glass
I am known as Napalm to my friends, because once i stick you you, you cant get me to stop until i have talked your ear off (or burned it off, which is
actually more likely)
|
|
|
MeshPL
Hazard to Others
 
Posts: 329
Registered: 20-4-2015
Location: Universe
Member Is Offline
Mood: No Mood
|
|
Plant ashes contain phosphorus in form of oxide, but are not very rich in sodium.
|
|
|
Random
International Hazard
   
Posts: 1120
Registered: 7-5-2010
Location: In ur closet
Member Is Offline
Mood: Energetic
|
|
I don't think so
|
|
|
Detonationology
Hazard to Others
 
Posts: 362
Registered: 5-5-2015
Location: Deep South
Member Is Offline
Mood: Electrophillic
|
|
Phosphorus oxides? Not likely. Perhaps you meant to say phosphates (PO4)?
[Edited on 2-12-2016 by Detonationology]
“There are no differences but differences of degree between different degrees of difference and no difference.” ― William James
|
|
|
Texium
Administrator
      
Posts: 4738
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline
Mood: Seeking gainful employment
|
|
Somehow I find it doubtful that there would be any phosphorus pentoxide present in wood ashes. If any was formed in the heat of the fire at all, it
would absorb water from the atmosphere on cooling forming phosphoric acid which would react with with the alkaline components of the ash to form
phosphates.
|
|
|
DraconicAcid
International Hazard
   
Posts: 4502
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
Quote: Originally posted by zts16  | | Somehow I find it doubtful that there would be any phosphorus pentoxide present in wood ashes. If any was formed in the heat of the fire at all, it
would absorb water from the atmosphere on cooling forming phosphoric acid which would react with with the alkaline components of the ash to form
phosphates. |
I'm sure it would be in the form of phosphates. However, fertilizers often claim that they contain such-and-such a mass of phosphorus as P2O5, even
though it's as a phosphate. It comes from a very old way of looking at such compounds, like writing sodium carbonate as
Na2O*CO2.
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
|
MeshPL
Hazard to Others
 
Posts: 329
Registered: 20-4-2015
Location: Universe
Member Is Offline
Mood: No Mood
|
|
Yes I meant "phosphorus oxide", but the same way as it is present in phosphate fertilisers, I should have written phosphates, as that would be a more
correct and unambiguous way of saying that. Ashes also contain magnesium in form of oxide and salts.
|
|
|
feacetech
Hazard to Others
 
Posts: 163
Registered: 12-2-2007
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by DraconicAcid  |
I'm sure it would be in the form of phosphates. However, fertilizers often claim that they contain such-and-such a mass of phosphorus as P2O5, even
though it's as a phosphate. It comes from a very old way of looking at such compounds, like writing sodium carbonate as
Na2O*CO2. |
Its just a way of expressing the elemental composition in a fertiliser.
Total P as P2O5 or BPL or Just plain P
just a little bit of math trickery i.e. if I had X% P if I assume its in its oxide I can assume I have Y% of P2O5 (%P x 2.29136 (molar mass P2O5 / 2x
molar mass P))
Its a very common mathematical manipulation in chemistry as well as a way to trick you into thinking you are getting more!
|
|
|
Amos
International Hazard
   
Posts: 1408
Registered: 25-3-2014
Location: Yes
Member Is Offline
Mood: No
|
|
My guess would be calcium and magnesium phosphate, some sulfate, and quite likely oxides or hydroxides that were too calcined and unreactive from the
high temperature of the fire to react quickly with dilute acetic acid.
|
|
|
nscheffield
Harmless
Posts: 16
Registered: 25-4-2015
Member Is Offline
Mood: No Mood
|
|
Would a stronger acid help to remove some of the above mentioned compounds?
I am known as Napalm to my friends, because once i stick you you, you cant get me to stop until i have talked your ear off (or burned it off, which is
actually more likely)
|
|
|