ninhydric1
Hazard to Others
 
Posts: 345
Registered: 21-4-2017
Location: Western US
Member Is Offline
Mood: Bleached
|
|
Preparation of titanium nanoparticles
I have recently taken an interest in nanoparticles and their versatile applications and developments. Preparing silver nanoparticles is well
documented but I wanted to prepare a more obscure metal nanoparticle. During my research, I happened to stumble on an article describing the synthesis
of titanium dioxide nanoparticles and another article describing its uses and possible improvements (both articles attached below).
The article about TiO2 nanoparticles states that by adding TiCl4 to chilled distilled water and then adding urea will create a colloid of TiO2 in
water. From what I understand, TiCl4 is hydrolyzed to TiO2 and the urea somehow complexes with the TiO2 to form a suspension. Is this the correct
mechanism and will it work?
Upon researching the synthesis of TiCl4, I came upon a synthesis developed by plante1999, as quoted below:
Quote: Originally posted by plante1999  | Simply melt pyrosulphate with the ore in presence of NaCl, it will make HCl + TiCl4
Sources: my own work
In fact I already made most inorganic titanium compounds and many organic ones, I think that I have some(a lot) knowledge in this field.
[Edited on 17-5-2012 by plante1999]
[Edited on 17-5-2012 by plante1999] |
Has anyone tried this (besides plante1999 himself) and can confirm the reaction occurs? If it does, is a paint can an acceptable reaction vessel?
(Anders Hoveland was an interesting member too)
Attachment: tinanoparticles.pdf (531kB) This file has been downloaded 417 times
Attachment: Nanoparticles.pdf.pdf (2.3MB) This file has been downloaded 364 times
[Edited on 11-23-2017 by ninhydric1]
The philosophy of one century is the common sense of the next.
|
|
|
VSEPR_VOID
National Hazard
  
Posts: 719
Registered: 1-9-2017
Member Is Offline
Mood: Fullerenes
|
|
I wonder if you could use them for solar cells. I remember NerdRage had a video about producing simple solar cells using TiO2, carbon, and
raspberries. You should try it if you can produce enough nano particles.
https://www.youtube.com/watch?v=WHTbw5jy6qU
Within cells interlinked
Within cells interlinked
Within cells interlinked
|
|
|
ninhydric1
Hazard to Others
 
Posts: 345
Registered: 21-4-2017
Location: Western US
Member Is Offline
Mood: Bleached
|
|
TiO2 is often used in photocatalyzing specific reactions so it would make sense that it is an experimental component for solar cells.
The philosophy of one century is the common sense of the next.
|
|
|
clearly_not_atara
International Hazard
   
Posts: 2918
Registered: 3-11-2013
Member Is Offline
Mood: Big
|
|
TiO2 mp is 1840 C
Na2S2O7 decomposes starting at 400 C
Pardon my incredulity but I think we're going to need to see some extraordinary evidence to believe these compounds are in the same melt
|
|
|
ninhydric1
Hazard to Others
 
Posts: 345
Registered: 21-4-2017
Location: Western US
Member Is Offline
Mood: Bleached
|
|
I assume plante1999 meant that the reaction takes place when Na2S2O7 starts melting. I'm pretty sure I won't be able to reach temperatures up to 1840
degrees Celsius. It would be best for him to clarify, but he hasn't been online for a while.
The philosophy of one century is the common sense of the next.
|
|
|