DoctorOfPhilosophy
Hazard to Others
 
Posts: 130
Registered: 12-6-2012
Location: Ontario, Canada
Member Is Offline
Mood: enthralled
|
|
Two suggestions to the lithiumheads here:
1. If you want a clean sample but don't have fancy equipment (argon / vacuum pumps), sparge the oil you are using for storage with helium from a
balloon tank. Also you can "getter" the oil with sacrificial lithium from one battery, remove the corroded lithium, and add fresh lithium (presumably
for display, since for storage you would just keep it in the battery.)
2. Don't try to fuse (melt) the lithium into a blob using a ceramic crucible. It will explode and hurl molten alkali metal at your face. Theo Gray has
confirmed my result. The lithium reacts with the silicon and aluminum oxide and you get a nasty thermite-like bang.
Regarding this:
You can use lithium to make thorium from lantern mantles.
[Edited on 11-12-2018 by DoctorOfPhilosophy]
|
|
|
ElementsGuy
Harmless
Posts: 3
Registered: 13-9-2019
Member Is Offline
|
|
In regard to casting lithium metal, could I simply melt the lithium directly in a zinc mold and then let it cool? Any potential issues in doing this?
Also, the post mentioned using lithium to extract thorium from thorium mantles. How would one do that?
Thanks.
|
|
|
fusso
International Hazard
   
Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline
|
|
I think the Li will simply burn at such temperatures. Also I don't know if Li will alloy with Zn.
|
|
|