Another metal of Palladium


Hi,

Exist there for a catalysis of hydrogenation another metal with the characteristics of palladium even if other metals do not generate as much hydrogen
The Tungsten can it replace it! Or gold, silver,or other ?

Regards.
View user's profile View All Posts By User
vulture
Forum Gatekeeper
*****




Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline

Mood: No Mood

[*] posted on 18-11-2003 at 12:12


Raney nickel?



One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 18-11-2003 at 15:23


It depends what you want to do.
Ni is a fairly good hydrogenation catalyst.
View user's profile View All Posts By User
Organikum
resurrected
*****




Posts: 2344
Registered: 12-10-2002
Location: Europe
Member Is Offline

Mood: frustrated

[*] posted on 22-11-2003 at 04:30


Nickel can be made a hell of a hydrogenation catalyst - all sugar reductions for example are done with those. Just heating precipated Ni at 800°C under a stream of hydrogen is fairly out of reach I fear.
There had been rumors on tungstencarbide having similar properties to Pd/Pt, but I never heard something on this again.

Catalytic hydrogenation is art. This is by no way easy to do - with or without pressure.




Irgendwas is ja immer
View user's profile View All Posts By User
madbee
Harmless
*




Posts: 2
Registered: 17-11-2003
Location: europa
Member Is Offline

Mood: No Mood

cool.gif posted on 26-11-2003 at 09:00
Hum... . .


Thank you for all information I will look at the track of the tungstencarbide !
View user's profile View All Posts By User
If_6_was_9
Unregistered




Posts: N/A
Registered: N/A
Member Is Offline


[*] posted on 1-2-2004 at 17:03


See

http://www.geocities.com/dritte123/Nipat.html


http://www.geocities.com/dritte123/PSPF.html

  Go To Top