Mood: ?
|
|
Safely clean burned food residue on copper pan?
Mostly it's burned on grease and such from frying that got on the outside of the pan and burned on, and I don't want to damage the copper surface. I
tried oven cleaner but it turns the copper some nasty gray blue color, so I can't use that. Scraping the stuff off with steel wool will also ruin the
soft metal. What's safe to use on copper?
\"Good is a product of the ethical and spiritual artistry of individuals; it cannot be mass-produced.\" --Aldous Huxley
|
|
not_important
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
First thing to try is a long soaking in water + detergent, followed by scrubbing with a rough cloth, plastic brush or pad, or course salt (followed by
a real good rinse)
Is the outside lacquered? If so the food may have melded itself with the lacquer. You may have to resign yourself to stripping the lacquer (and the
grease) and put more effort into polishing the pans after that.
Acids - vinegar, lemon juice, and the like, plus salt are favorite home cleaning tip methods. But these really are targeted at tarnish on the copper,
reacting with and dissolving it; they're not that good at getting baked on food off.
|
|
Nixie
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 490
Registered: 12-12-2006
Member Is Offline
Mood: ?
|
|
No lacquer; I clean the copper with copper cleaner regularly to remove the oxides after a few cookings, but they don't touch the residues.
[Edited on 27-2-2008 by Nixie]
\"Good is a product of the ethical and spiritual artistry of individuals; it cannot be mass-produced.\" --Aldous Huxley
|
|
microcosmicus
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 287
Registered: 31-12-2007
Member Is Offline
Mood: spin up
|
|
Since its burnt on grease, try an organic solvent --- use alcohol to dissolve it or at least soften
up the mess. To keep the solvent from evaporating, keep the pan enclosed in some container
or bag with the alcohol is you want to soak it for a while.
Another thought is to use a warm basic solution to try to saponify some of the grease.
|
|
12AX7
Post Harlot
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Intense heat will burn off any carbon, anneal the copper and oxidize a substantial amount to CuO and Cu2O. Something to avoid.
Lesson learned, always cook with a sufficient layer of oil on the pan at all times!
Tim
|
|
Nixie
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 490
Registered: 12-12-2006
Member Is Offline
Mood: ?
|
|
It's about stuff that dripped onto the OUTSIDE of the pan and burned from the flame of the gas stove. I don't have a problem with the inside, it's
lined with a thin layer of steel on the inside.
\"Good is a product of the ethical and spiritual artistry of individuals; it cannot be mass-produced.\" --Aldous Huxley
|
|
bfesser
Resident Wikipedian
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2114
Registered: 29-1-2008
Member Is Offline
Mood: No Mood
|
|
Why remove it? It shouldn't reduce the functionality of the pan.
I would also recommend trying either an organic solvent or a saponification method.
|
|
bio2
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 447
Registered: 15-1-2005
Member Is Offline
Mood: No Mood
|
|
I have used gasoline and diesel which after soaking a day or two softens the burnt carbonized oil enough that it can be easily scraped off.
Another way to clean even hopelessly blackened stainless steel pots is to make them the anode for a while in a NaOH electrolyte. Gets it shiny new
looking.
|
|
chemrox
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline
Mood: LaGrangian
|
|
Copper reacts with moist air to form mixed Cu(OH)2 and CuCO3. This is the common patena you see on unpolished copper. Base is usually effective in
removing organic residues that are cooked onto metal surfaces. Hence oven cleaners are mostly lye. So what I'm getting at is this. You could go
ahead and use the oven cleaner and then polish off the blue haze (Cu(OH)2) when the cooked material is gone. You lose a little Cu but you do thatg
whenever you polish anyway.
"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
|
|