Mortar And Pestle Composition


I'm curious as to what your favorite mortar and pestle compositions are ?
I have 5 of them: porcelain, stainless steel, onyx, glass, cast iron. The cast iron
model is the most recent. With its very heavy pestle, grinding down materials
is almost effortless. Of course, my ballmill is preferred for any large amounts.
When it comes to very fine powdering, my glass model is probably the best.
I keep the onyx(Smithsonian Institute - Museum Of Natural History gift shop) for
display purposes only.

Any thoughts or flames ?




From opening of NCIS New Orleans - It goes a BOOM ! BOOM ! BOOM ! MUHAHAHAHAHAHAHA !
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 17-10-2007 at 16:33


I use my big Coors (4-5") porcelain mortar & pestle quite often. I would use a small onyx or agate set (if I had one) for preparing samples for melting points. I also have an iron set that I bought for pulverizing gold bearing quartz. But I still had to ball mill the powder before doing the fire assay.

I just like the looks of them also. I suspect you do too. ;)




The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
Ozone
International Hazard
*****




Posts: 1269
Registered: 28-7-2005
Location: Good Olde USA
Member Is Offline

Mood: Integrated

[*] posted on 17-10-2007 at 17:06


Ditto with the Coors. I use a small, highly polished agate model for mixing KBr and sample prior to pellet pressing for IR. The smooth surface does not take up particles like the rougher porcelain.

I must agree and add that nothing (except maybe a Jacob's Ladder) evokes "science" more strongly than a retort sitting next to a mortar and pestle;).

Cheers,

O3




-Anyone who never made a mistake never tried anything new.
--Albert Einstein
View user's profile View All Posts By User
chemrox
International Hazard
*****




Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline

Mood: LaGrangian

[*] posted on 17-10-2007 at 21:38


Ditto ditto a big Coors pestle and bigger mortar (to fit my hand) for grinding reagents and a small agate one for KBr mixing. No glass ... no metals ... I wish I had a retort ..Just for looks .. I do have a sidearm flask ...
View user's profile View All Posts By User
Sauron
International Hazard
*****




Posts: 5351
Registered: 22-12-2006
Location: Barad-Dur, Mordor
Member Is Offline

Mood: metastable

[*] posted on 18-10-2007 at 04:19


Apart from the typical lab types as listed above, I have made use of large (like 8-10" stone mortars and pesters and wooden ones for pulverizing herbs. These are common kitchen implements in Thailand. In fact the kitchen pestle is the Thai housewife's domestic weapon, equivalent to an American wife's rolling pin. For braining the errant husband as an object lesson.



Sic gorgeamus a los subjectatus nunc.
View user's profile View All Posts By User
not_important
International Hazard
*****




Posts: 3873
Registered: 21-7-2006
Member Is Offline

Mood: No Mood

[*] posted on 18-10-2007 at 04:55


I echo much of what has already been described. I have a copy of stainless steel M&P made in India, one reserved for spices, and a stone M&P like Sauron's that is great for grinding chilies as well as preliminary crushing of cassia bark and turmeric root. I've also a small set made from synthetic sapphire that is intended for sample prep, it resembles the agate morters favored for IR sample prep.
View user's profile View All Posts By User
Phosphor-ing
Hazard to Others
***




Posts: 245
Registered: 31-5-2006
Location: Deep South, USA
Member Is Offline

Mood: Inquisitive

[*] posted on 18-10-2007 at 05:41


Quote:
Originally posted by Sauron
In fact the kitchen pestle is the Thai housewife's domestic weapon, equivalent to an American wife's rolling pin. For braining the errant husband as an object lesson.



LOL *ducks, as flying plates crash against the wall and shatter, just in time to catch the flying pestle on the back of the head! Pop knots ensue.*

I have 2 small porcelain M&P, about 2" & 3", and a large porcelain one, 6"+ with the wooden pestle Sauron mentions above. Pop knots included! :)
View user's profile View All Posts By User
Sauron
International Hazard
*****




Posts: 5351
Registered: 22-12-2006
Location: Barad-Dur, Mordor
Member Is Offline

Mood: metastable

[*] posted on 18-10-2007 at 06:10


Indeed it is mainly for chilis that Thai cooks use the M&P and when they do the Thai kitchen assumes a most interesting atmosphere indeed.

The familiar pok pok pok of a Thai girl sitting on the floor with M&P between her thighs...




Sic gorgeamus a los subjectatus nunc.
View user's profile View All Posts By User
Phosphor-ing
Hazard to Others
***




Posts: 245
Registered: 31-5-2006
Location: Deep South, USA
Member Is Offline

Mood: Inquisitive

[*] posted on 18-10-2007 at 06:38


I use the large mortar w/ wooden pestle to grind up Glucosamine and Chondroitin tables to be spread over the dogs food in the evening. She wont take the pills whole, but ground up and mixed in a can of dog food and she devours it.
View user's profile View All Posts By User
Mr. Wizard
International Hazard
*****




Posts: 1042
Registered: 30-3-2003
Member Is Offline

Mood: No Mood

[*] posted on 18-10-2007 at 07:42


I have a large and small cast iron mortar and pestle; lucky acquisitions from a second hand store. They are more suitable for grinding mining samples than chemistry, as any product will have a healthy dose of iron added. I also have a small Coors porcelain one for when purity is an issue. It can also be cleaned more thoroughly.

The mortar and pestle is also the recognized sign for pharmacies here in the US. The Alembic, even though most don't know what it's called, is a more recognized chemistry symbol. The test tube and Erlenmeyer flask are also very recognized.
View user's profile View All Posts By User
Fleaker
International Hazard
*****




Posts: 1252
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 18-10-2007 at 10:24


I have a 320mm diameter Coors one, and then a small 85mm one from agate.

Anyone ever got to use one of those tiny little alumina mortar and pestles? They're pinkish in colour and fairly expensive, but they grind very well!




Neither flask nor beaker.


"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
View user's profile View All Posts By User
Panache
International Hazard
*****




Posts: 1290
Registered: 18-10-2007
Member Is Offline

Mood: Instead of being my deliverance, she had a resemblance to a Kat named Frankenstein

[*] posted on 26-2-2008 at 21:41


i have one made out of dry ice glass but i find it really impractical to use. Firstly it burns the crap out of your hands then it sublimes to nothing after first condensing water all over your sample, so annoying.
:P




View user's profile View All Posts By User
MagicJigPipe
International Hazard
*****




Posts: 1554
Registered: 19-9-2007
Location: USA
Member Is Offline

Mood: Suspicious

[*] posted on 26-2-2008 at 21:51


What? You can't be serious. I have never heard of that. I mean, I suppose I can see what it would be useful for but... like you said, the sublimation, condensation and subsequent freezing of water vapor, the extreme cold. Not to mention you would have to replace it every time it was used.

Am I missing something? Is the joke on me or does that actually exist?




"There must be no barriers to freedom of inquiry ... There is no place for dogma in science. The scientist is free, and must be free to ask any question, to doubt any assertion, to seek for any evidence, to correct any errors. ... We know that the only way to avoid error is to detect it and that the only way to detect it is to be free to inquire. And we know that as long as men are free to ask what they must, free to say what they think, free to think what they will, freedom can never be lost, and science can never regress." -J. Robert Oppenheimer
View user's profile View All Posts By User This user has MSN Messenger
chemrox
International Hazard
*****




Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline

Mood: LaGrangian

[*] posted on 26-2-2008 at 22:58


I have a large Coors for the lab .. mortar is over sized relative to the pestle for grinding ease. I have a 55 mm agate set for melting pint mixes, KBr pellets and making mulls. In my kitchen I have a medium size porcellain one since the Coors went to the lab and I have an extremely hard bamboo one as well. Came from Thailand.



"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
View user's profile View All Posts By User
Panache
International Hazard
*****




Posts: 1290
Registered: 18-10-2007
Member Is Offline

Mood: Instead of being my deliverance, she had a resemblance to a Kat named Frankenstein

[*] posted on 27-2-2008 at 15:43


Quote:
Originally posted by MagicJigPipe
Am I missing something? Is the joke on me or does that actually exist?


It was a very dry joke.

HA!! A PUN!!!!

However i think this thread should now include ridiculous suggestions for inconvenient materials to construct mortar and pestles out of. Points if you actually construct it and post a photograph.




View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 28-2-2008 at 03:26


Quote:
Originally posted by Panache
Quote:
Originally posted by MagicJigPipe
Am I missing something? Is the joke on me or does that actually exist?


It was a very dry joke.

HA!! A PUN!!!!

However i think this thread should now include ridiculous suggestions for inconvenient materials to construct mortar and pestles out of. Points if you actually construct it and post a photograph.


KClO3/P2S5 mortar :P




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
bfesser
Resident Wikipedian
*****




Posts: 2114
Registered: 29-1-2008
Member Is Offline

Mood: No Mood

[*] posted on 28-2-2008 at 05:53


Quote:
Originally posted by Fleaker
Anyone ever got to use one of those tiny little alumina mortar and pestles? They're pinkish in colour and fairly expensive, but they grind very well!


I've got a very tiny very hard and smooth mortar and pestle that <em>might</em> be made out of alumina. It seems too smooth to be made out of porcelain. It's not pinkish though, just sorta off-white. It's probably only an inch or so wide. I can post a picture if you like.

I also have a large marble, a medium sized brass, and a standard Coors ceramic. Used to have two others for cooking, but I gave them away. Mortars and pestles are as indispensable in the kitchen as in the lab.
View user's profile View All Posts By User
garage chemist
chemical wizard
*****




Posts: 1803
Registered: 16-8-2004
Location: Germany
Member Is Offline

Mood: No Mood

[*] posted on 28-2-2008 at 08:08


I have one porcelain mortar, and I don't really understand why one would need more than one mortar in the home lab.
I have never needed a different one, ever.
Iron is attacked by some substances, agate is not good for tough materials like chlorine tablets. Porcelain seems universally useable for everything.




www.versuchschemie.de
Das aktivste deutsche Chemieforum!
View user's profile View All Posts By User
bfesser
Resident Wikipedian
*****




Posts: 2114
Registered: 29-1-2008
Member Is Offline

Mood: No Mood

[*] posted on 28-2-2008 at 08:17


Porcelain cross contaminates samples because of it's porosity, which is why agate mortars come in handy--especially for IR prep. Having more than one mortar and pestle is like having more than one flask. You need to have the right size, shape, and material for the job. You wouldn't want to use an iron mortar and pestle to prepare an IR sample, just as you wouldn't want to use a plastic flask to boil a high-boiling organic.

That being said, porcelain is probably the best for all around grinding work--<em>if</em> you only have a choice of one material. It's got the porosity problem, but it's hard enough to grind hard materials without issue (also has a slightly rough surface, which makes fine grinding easier), it's cheap enough to be expendable under certain conditions (not like agate), it's not as fragile as glass, and not prone to attack from acids like metal mortars.

Personally, I'd really like to get my hands on an agate mortar and pestle, but they're out of my price range for now.

[edit]
I forgot to mention that you will have issues with loss of product when grinding very small quantities (perhaps a few mg) in a medium or large-sized porcelain mortar. <em>And,</em> porcelain makes working with sticky compounds more difficult.

[Edited on 2/28/08 by bfesser]
View user's profile View All Posts By User
Phosphor-ing
Hazard to Others
***




Posts: 245
Registered: 31-5-2006
Location: Deep South, USA
Member Is Offline

Mood: Inquisitive

[*] posted on 28-2-2008 at 08:26


I also only have a porcelain mortar and pestle. I do have 2 sizes medium and small. I agree with garage chemist there really is no reason, I can think of, to have anything but porcelain in a home lab setting. Maybe for aesthetics but that's it.
@bfesser not to many amateur chemist have IR available to them.




"The nine most terrifying words in the English language are: 'I'm from the government and I'm here to help.'" -Ronald Reagan
View user's profile View All Posts By User
bfesser
Resident Wikipedian
*****




Posts: 2114
Registered: 29-1-2008
Member Is Offline

Mood: No Mood

[*] posted on 28-2-2008 at 08:32


Quote:
Originally posted by Phosphor-ing
@bfesser not to many amateur chemist have IR available to them.


We can dream, can't we? :P

[Edited on 2/28/08 by bfesser]
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 28-2-2008 at 19:24


I needed to grind up a gold bearing quartz ore. For that I bought an iron mortar & pestle. I would have been afraid to attempt this grinding with my Coors porcelain set.

[Edited on 28-2-2008 by Magpie]
View user's profile View All Posts By User
domaani
Harmless
*




Posts: 10
Registered: 15-3-2008
Location: Finland
Member Is Offline

Mood: No Mood

[*] posted on 15-3-2008 at 17:33


Quote:
Alkuperäinen lähettäjä bfesser
Quote:
Originally posted by Phosphor-ing
@bfesser not to many amateur chemist have IR available to them.

We can dream, can't we? :P

Oh yes we can.

I got a Perkin Elmer 1600 FTIR unit for a Christmas present last year. I just had to get one after finding out the value of the similar unit I demolished for parts many years ago (found it from a local junkyard). What a tragedy, although I'm now almost getting over it. :)

I asked a friend to manufacture an agate M&P for IR sample preparation, he's a member of a local Stone Club. It'll cost me a bottle of liquor. Shopping for a new one was never an alternative, the prices seem to be quite awkward.
View user's profile View All Posts By User
microcosmicus
Hazard to Others
***




Posts: 287
Registered: 31-12-2007
Member Is Offline

Mood: spin up

[*] posted on 15-3-2008 at 18:51


For most purposes, I do just fine with a small porcelain mortar and pestle which I
picked up at the dollar store around the corner.

As for why anyone might legitimately want something other than
porcelain in a home laboratory, one answer is if they happen
to do chemistry at high temperatures and want to grind up things like
calcium aluminate or make glass frit form pieces of broken glass. Hard
materials like that (basically the same stuff the geologists encounter
in their mineral samples) can chew its way right through porcelain, so I
instead powder it using a hammer on a steel plate. One of these years,
I plan to make a mortar and pestle of tool steel or cast iron for tasks like this.

As for fantasies, mine would be a mortar and pestle made of diamond.

Another thought, not so fantastic, is to tie this discussion in with the
thermite thread --- make molten titanium using blogfast's reaction
and cast a mortar and pestle. Both the physical toughness and the
chemical resistance of titanium sound like they would suit
it to this task.
View user's profile Visit user's homepage View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 15-3-2008 at 19:04


Eh, titanium's strong, but steel has the edge (-holding capability).

What you want is manganese steel (about 5-15% alloy, IIRC), for abrasion resistance. They use that shit for *backhoe* buckets and teeth. Actually I'm not sure what the teeth are, I imagine they are something directly from the gates of hell! That's what you really want. :D

A similar proposition (i.e., a case of favorite alcoholic beverage) might get a tool and die maker to carve you one from a block around the shop.

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
 Pages:  1  

  Go To Top