[*] posted on 1-3-2008 at 14:37
Platinum Anode


Hello,

Searching, I was surprised not to find a 'Platinum Anode' thread or some such.
Anyhow, some bedtime reading:
http://www.geocities.com/lllwolly/further/PtPerkCell.zip

Dann2
View user's profile View All Posts By User
Fleaker
International Hazard
*****




Posts: 1254
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 1-3-2008 at 19:46


What of it? Should we discuss some platinum anodes?

I can post a picture of some commonly seen platinum anodes and/or how to make them from wire?




Neither flask nor beaker.


"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
View user's profile View All Posts By User
tentacles
Hazard to Others
***




Posts: 191
Registered: 11-11-2007
Member Is Offline

Mood: No Mood

[*] posted on 1-3-2008 at 19:52


The wear rates are both interesting, and alarming. The lowest wear rate was 5.3 g/ton of Na chlorate, and the highest (discounting the invalid data) 8.6g/t. At today's prices ($72/gram!) that's $381 per ton of perc, *if* we could replicate the lowest wear rate. I don't know if the chlorate to perc wear rates would be lower, but I would expect that as amateurs, we can expect higher wear rates with our less controlled cells.

At 8.6g/t the wear rate comes up to $619/ton, which is actually $.3096/lb of perc. Not terrible, really, but probably the biggest running cost besides the time.

Still, I'm interested in how 12AX7's cells are doing with his platinized Ti anodes. Chlorate is cheap to make, and a good working perc anode is worth a bit of cost.

Edit: Read to the end of the paper, and they were running the cell at 110C! I wonder what effect that had on the efficiency?

[Edited on 1-3-2008 by tentacles]
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 2-3-2008 at 04:29


Quote:
Originally posted by tentacles
Still, I'm interested in how 12AX7's cells are doing with his platinized Ti anodes. Chlorate is cheap to make, and a good working perc anode is worth a bit of cost.


They were going slowly until things went just too slowly, supply voltage rose and the platinum all but delaminated.

I'm still recovering wastes before I can replate anything.

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
garage chemist
chemical wizard
*****




Posts: 1803
Registered: 16-8-2004
Location: Germany
Member Is Offline

Mood: No Mood

[*] posted on 2-3-2008 at 05:46


Brauer has a recipe for a bath for electrolytical platinizing of titanium and tantalum.
It consists of:
H2[Pt(OH)6] 20g/L
KOH 15g/L

The anode is stainless steel.
This special alkaline bath is for titanium and tantalum only.

It is operated at 70- 80°C, 0,8A/dm2 current density and almost 100% current efficiency.
The substrate has to be pretreated, though it is not mentioned how.

This bath is found on page 1708, in the third volume, which is not included in the english version, but in the german one.

I have only found out about this method of Ti platinization recently, I was only aware of the molten salt elctrolysis before.

There is also a preparation of this H2[Pt(OH)6] compound (as the potassium salt, which of course would form in the KOH solution anyway) in this volume. I can translate this if needed.

[Edited on 2-3-2008 by garage chemist]




www.versuchschemie.de
Das aktivste deutsche Chemieforum!
View user's profile View All Posts By User
not_important
International Hazard
*****




Posts: 3873
Registered: 21-7-2006
Member Is Offline

Mood: No Mood

[*] posted on 2-3-2008 at 07:56


Titanium and tantalum only, and not other valve metals?
View user's profile View All Posts By User
dann2
International Hazard
*****




Posts: 1523
Registered: 31-1-2007
Member Is Offline

Mood: No Mood

[*] posted on 2-3-2008 at 08:00


Hello,

The temperature of the cell (110C) is crazy high. I though it was a misprint. One advantage of the very high temperatures is that the cell voltage goes down and you will get power savings. This is important when using megawatts of power. Price of Pt was much less then than now, wonder what price it will be in ten years????????????/

I would guess this type of cell/production setup never made it on an industrial scale, it was a study after all.

I think a way to make Ti plated anodes would be useful. The actual cost of the anode would not be too prohibitive, the problem is (IMHO), it will take a bit of cash to get to a point where an amateur process is usable and repeatable. With LD or Manganese Dioxide etc etc you can do a lot of experimentation with small finanical input.
Pt?..... :o
Did Tim's bath not cost $300, that's very bad news for a stingy gits pocket like myself (bad for the blood pressure too).

Would not mind seeing some plating solutions. Everyone seems to claim that not all the details are in the bath ingredients, as such. There always seems to be one detail/step/secret left out.

Perhaps wire is the best way to go..........

Cheers,

Dann2

[Edited on 2-3-2008 by dann2]
View user's profile View All Posts By User
Fleaker
International Hazard
*****




Posts: 1254
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 2-3-2008 at 08:38


Mind you it wasn't his 300 dollar a gallon plating bath, and that was back in December, about 600 dollars an ounce ago :p The good thing about it though, is that he can recover the platinum from failed attempts and reuse it.

I think the details are not in the bath ingredients but rather (as I keep repeating ad nauseum) in the preparation of your substrate!!! Proper pretreatment will give a suitable anode. This is true for almost anything in electrochemistry.

[Edited on 2-3-2008 by Fleaker]




Neither flask nor beaker.


"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 2-3-2008 at 10:50


Yeah, and I'd much rather have more like $1000 of Na2PtCl6, if not more, for the size of bath I started with. I suspect a higher concentration (giving higher current efficiency and less hydrogen) may produce a better deposit. It's just the price you have to pay. Only one-time, if you collect and process all your crud!

Brush plating may be more suitable, since it takes so much platinum in the bath. You still need to strike the titanium with something quickly though.

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
tentacles
Hazard to Others
***




Posts: 191
Registered: 11-11-2007
Member Is Offline

Mood: No Mood

[*] posted on 4-3-2008 at 10:02


12AX7: Have you tried plating platinum over ATO at all? A lot of these MMO patents mention using them as an interface layer with a noble metal or metal oxide active layer over top. Unfortunately I haven't seen it specified anywhere how they plate platinum over the interface. It was mentioned in the BTO patent as well.

[Edited on 4-3-2008 by tentacles]
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 4-3-2008 at 13:16


I don't have the pertinent nitrates or whatever on hand. Of course I have tin, but it's all alloyed with lead. Seems to me I was going to get lead-free solder from the hardware store at some point...

I do have a mixture of transition metals which I leached (with HCl) from carbide cutter grindings (should be roughly 80% WC, 20% Co). At the moment it has a yellow brown color similar to Fe(3+), but not nearly as orange as FeCl3. When reduced, it is green; when oxidized, it turns this color, and over time a precipitate (I think dark olive green, but I haven't washed it yet) has formed.

Incidentially, said grindings burn white hot with a chlorate. CO2 and tungstate formation perhaps?

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
Rosco Bodine
Banned





Posts: 6370
Registered: 29-9-2004
Member Is Offline

Mood: analytical

[*] posted on 4-3-2008 at 14:27


Yeah lead free solder simplifies things greatly . But it isn't absolutely essential .

You could separate your tin from the lead/tin alloy
using warm and medium strength HNO3 . On dilution the lead will remain in solution as lead nitrate while the tin will be dropped out as metastannic acid . You could use that metastannic acid for reaction with oxalic acid and H2O2 to make a stannic anhydride / peroxalic acid sol . Or you can peptize the metastannic acid to a sol using an organic amine . Or you can depolymerize the metastannic acid by fusion with NaOH , dissolve the product in H2O and neutralize with HCl to precipitate alpha stannic oxidehydroxide which you can use then to make stannic chloride , stannic nitrate , ammonium stannate , ect.

[Edited on 4-3-2008 by Rosco Bodine]
View user's profile View All Posts By User
R.P.Wang
Harmless
*




Posts: 7
Registered: 5-12-2007
Location: China
Member Is Offline

Mood: No Mood

[*] posted on 13-3-2008 at 04:43


Quote:
Originally posted by tentacles
12AX7: Have you tried plating platinum over ATO at all? A lot of these MMO patents mention using them as an interface layer with a noble metal or metal oxide active layer over top. Unfortunately I haven't seen it specified anywhere how they plate platinum over the interface. It was mentioned in the BTO patent as well.

[Edited on 4-3-2008 by tentacles]


I attached a article which is about adding Pt between titanium substrate and Sb-SnO2 layer, service life is increased!

Attachment: Preparation and Characterization of Antimony-Doped Tin Dioxide Electrodes. Part 1. Electrochemical Characterization.pdf (313kB)
This file has been downloaded 970 times

View user's profile View All Posts By User This user has MSN Messenger
dann2
International Hazard
*****




Posts: 1523
Registered: 31-1-2007
Member Is Offline

Mood: No Mood

[*] posted on 29-9-2008 at 15:38


Hurray, golly good show, yipee, etc ,etc,

Every cloud has a Silver lining (or should that be, every Silver lining has a great big piece of shit........... never mind).

A bit off topic. Pt is on the way down.
http://www.bloomberg.com/apps/news?pid=20601012&sid=a_4m...

Time to buy that brick sized lump.

pt1825nyb.gif - 8kB
View user's profile View All Posts By User
tentacles
Hazard to Others
***




Posts: 191
Registered: 11-11-2007
Member Is Offline

Mood: No Mood

[*] posted on 29-9-2008 at 17:26


I've been considering scoring some myself. An ounce might make a decent sized anode, but how do you work it - we need to find a jeweler's suppy or something. I thought I might speak with some jeweler's and see if they can't order me Pt in a sheet/foil. Isn't jewelry Pt usually a 90/10 Pt/Ir alloy that lasts longer as anode?
View user's profile View All Posts By User
garage chemist
chemical wizard
*****




Posts: 1803
Registered: 16-8-2004
Location: Germany
Member Is Offline

Mood: No Mood

[*] posted on 29-9-2008 at 17:44


Pure platinum is soft and malleable. You should be able to beat it out on an anvil.
Pt/Ir, on the other hand, is hard and elastic, and much harder to work with, though more resistant against corrosion in a perchlorate cell.




www.versuchschemie.de
Das aktivste deutsche Chemieforum!