Solvent ideas needed.
I have some large sheets of Polarised film, but there is a clear adhesive on the one side that I want to remove.
I expect that the material is some form of Cellulose (probably Acetate).
I`ve tried WD-40 and that does nothing (it Normally works).
I tried acetone and the adhesive turn to gel almost instantly BUT it ruins the film also.
I`ve tried Ligroin and that doesn`t touch it either.
ethanol works a Little bit, but leaves it Very messy.
any one have any ideas or have done this before?
edited to add: I just tried Toluene and that works exactly the same as the acetone and ruins the film too.
I`m hoping there may be an Inorganic method as I`m running out of known solvents that I have in stock.
[Edited on 1-3-2008 by YT2095]
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
|
chemrox
International Hazard
   
Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline
Mood: LaGrangian
|
|
MIBK has worked for me on similar substances
"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
|
|
|
YT2095
International Hazard
   
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
Hmmmm... I have non of that, not even a trace.
the closest I have as denaturing agent is MEK in a bottle off "pure" ethanol.
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
|
vulture
Forum Gatekeeper
   
Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline
Mood: No Mood
|
|
Isopropyl alcohol might be the best of both worlds. Or some higher alcohol. Diethyl ether?
[Edited on 1-3-2008 by vulture]
One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
|
|
|
YT2095
International Hazard
   
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
aha, Good ideas!
I have some Pre-Injection mediwipes that contain the IPA, and the Ether`s off site in the Machine shop (where I`m going tomorrow morning anyway).
I`ll let you know
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
|
lavenatti
Harmless
Posts: 17
Registered: 19-12-2006
Member Is Offline
Mood: No Mood
|
|
I hate to suggest something so simple, but how about soapy water and a good scrubbing? You'll probably end up with a bunch of little rolled up
adhesive balls but if the soap keeps the adhesive from resticking to the film it may work.
|
|
|
Tacho
National Hazard
  
Posts: 582
Registered: 5-12-2003
Member Is Offline
Mood: No Mood
|
|
I have succesfully removed adhesive coats from plastic surfaces using one of two techniques:
1- Soybean oil - sometimes it works, sometimes it doesn't.
2- I cut a piece of adhesive tape and do a repeated apply/remove on the surface. Somewhat as if you were depilating it. With some skill and luck, all
the adhesive end up on the tape, leaving the plastic surface clean and undamaged.
Good luck.
|
|
|
MagicJigPipe
International Hazard
   
Posts: 1555
Registered: 19-9-2007
Location: USA
Member Is Offline
Mood: Suspicious
|
|
"I have some Pre-Injection mediwipes that contain the IPA, and the Ether`s off site in the Machine shop (where I`m going tomorrow morning anyway)."
Any 24-hr gas station will have at least 70%
IPA and almost any grocery, Wal-Mart, pharmacy type store will carry the 91% and/or 100%. I suppose my question is, why even think about using
alcohol pads?
EDIT
I forgot you might live in Europe and I'm not sure what kind of stores are open when in your area but still, IPA IMO is one of the most common and
easy to get chemicals (as easy as 3% H2O2)
[Edited on 3-3-2008 by MagicJigPipe]
"There must be no barriers to freedom of inquiry ... There is no place for dogma in science. The scientist is free, and must be free to ask any
question, to doubt any assertion, to seek for any evidence, to correct any errors. ... We know that the only way to avoid error is to detect it and
that the only way to detect it is to be free to inquire. And we know that as long as men are free to ask what they must, free to say what they think,
free to think what they will, freedom can never be lost, and science can never regress." -J. Robert Oppenheimer
|
|
|
YT2095
International Hazard
   
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
I`ve never seen IPA here OTC other than in 25ml overpriced tape-head cleaner bottles.
and the soap or oils have no effect, also I didn`t manage to get to the machine shop yesterday to get the Ether, so I`m still hanging some hopes on
that.
as for scrubbing, it`s a No Go as it`s Optical film and even plastic on plastic will scratch it (as I found out).
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
|
bio2
Hazard to Others
 
Posts: 447
Registered: 15-1-2005
Member Is Offline
Mood: No Mood
|
|
.......I expect that the material is some form of Cellulose (probably Acetate)...........
Nitroalkanes are solvents for Cellulose Acetate.
|
|
|
YT2095
International Hazard
   
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
and so that`s Something I would wish to avoid (since dissolving the Film is NOT the intention), which is just as well because I don`t have any anyway
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
|
MagicJigPipe
International Hazard
   
Posts: 1555
Registered: 19-9-2007
Location: USA
Member Is Offline
Mood: Suspicious
|
|
I can buy OTC 91% IPA (or 99% or 100% w/ 1% oil) here in bulk and will gladly send it to you (or anyone else on this forum) at cost + shipping. It's
not about the money, just helping the cause. Does anyone know if it's hazmat since it's flammable? Maybe a lower concentration (70%?) wouldn't be.
Buying it from a supplier might be cheaper because of shipping but if it isn't, let me know.
91% is $1.50 (.99 Euros or .76 pounds)(probably a little less for bulk) for 16oz (473mL). You can judge the weight by the density + thin HDPE bottle.
"There must be no barriers to freedom of inquiry ... There is no place for dogma in science. The scientist is free, and must be free to ask any
question, to doubt any assertion, to seek for any evidence, to correct any errors. ... We know that the only way to avoid error is to detect it and
that the only way to detect it is to be free to inquire. And we know that as long as men are free to ask what they must, free to say what they think,
free to think what they will, freedom can never be lost, and science can never regress." -J. Robert Oppenheimer
|
|
|
vulture
Forum Gatekeeper
   
Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline
Mood: No Mood
|
|
Any pharmacist in europe should be able to get you IPA, as it's used for desinfection. If you're afraid they'll charge too much, take a copy of your
favourite chemical suppliers catalog along and have them order the cheapest IPA in there.
One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
|
|
|
MagicJigPipe
International Hazard
   
Posts: 1555
Registered: 19-9-2007
Location: USA
Member Is Offline
Mood: Suspicious
|
|
A pharmacist ordering chemicals from a catalog for a private individual? I'm almost positive that 99% of the time if that were tried in the US they
would respond with an impolite "No!". Even for something as mundane as isopropanol. First of all they would ask, "Why do you need something more
pure than the IPA on the shelves?" And you might as well forget trying to order anything else.
One time I tried to order benzoic acid USP and they told me it was a CONTROLLED SUBSTANCE (prescription only).
Even benzyl alcohol was a pain to get from a pharmacy (and insanely expensive).
If it wasn't for the stupid gun laws I would move to Europe.
EDIT
And the US used to be the place where people came to experience MORE personal freedoms. Now, sadly, it is the opposite.
[Edited on 3-3-2008 by MagicJigPipe]
"There must be no barriers to freedom of inquiry ... There is no place for dogma in science. The scientist is free, and must be free to ask any
question, to doubt any assertion, to seek for any evidence, to correct any errors. ... We know that the only way to avoid error is to detect it and
that the only way to detect it is to be free to inquire. And we know that as long as men are free to ask what they must, free to say what they think,
free to think what they will, freedom can never be lost, and science can never regress." -J. Robert Oppenheimer
|
|
|
woelen
Super Administrator
       
Posts: 8151
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
MagicJigPipe, it is not useful to compare your situation with our situation. In the EU (at least in NL, UK, BE and DE) I have not seen IPA in pure
form or only mixed with water as an OTC chemical. Of course we can buy it, but then we need to order it from a pharmacist or a better equipped
old-fashioned drug-store.
And yes, many of us can order chemicals from a chemical supplier. I have a local drugstore nearby, who orders chemicals from chemical suppliers, which
normally does not sell to private individuals. In this way I obtained NaN3, KF, and a few other nasties, which I otherwise could not get.
There really is a difference in what is OTC in one country and in another country. Pure diethylether is OTC over here, just like pure acetone and
ligroin, but IPA is not, nor is methanol (but in BE, methanol is OTC as well).
EU != USA
Even in different countries inside the EU there are differences, e.g. in NL I cannot buy more than 5% ammonia, in BE I can get 12% in a supermarket.
|
|
|
argyrium
Hazard to Others
 
Posts: 123
Registered: 3-2-2008
Location: Pacific
Member Is Offline
Mood: No Mood
|
|
YT2095,
You might try mineral spirits (aka "paint thinner") or kerosene - possibly "mixed" with a small amount of a polar solvent (2-propanol, EtOH). If the
adhesive absorbs enough and swells sufficiently, you may be able to "roll" it off. You might try letting the adhesive imbibe/swell to the point where
it becomes mobile, then transfer/submerge the sheet to a tray filled with water. Wet a soft cotton cloth with the non-polar solvents and rub the
adhesive off THROUGH the water. The water should help keep the gooey mess from transferring onto the clean side and all over everything. Likely need
to use many pieces of cloth (or paper towels) - and gloves. A few drops of detergent added to the water may help, too.
Hope this works.
PS - IF the above works, you will likely still have a real mess that would/will require further cleaning with more of the same solvents after removal
from the water bath. A final clean-up with a lighter hydrocarbon blend ("naptha", "lighter fluid") on paper towels should help.
[Edited on 4-3-2008 by argyrium]
|
|
|
JohnWW
International Hazard
   
Posts: 2849
Registered: 27-7-2004
Location: New Zealand
Member Is Offline
Mood: No Mood
|
|
The isopropyl alcohol sold in hardware or similar stores as "rubbing alcohol" is usually only the distilled stuff containing only about 70% of the
stuff, and 30% water, because of the isopropanol-water constant-boiling-point azeotrope. Purer isopropanol is more expensive, probably obtained by a
further distillation with benzene, like absolute ethanol. It is used widely as a substitute for 95% grain alcohol (without denaturing additives),
because of the heavy excise tax on the latter in most countries.
[Edited on 4-3-08 by JohnWW]
|
|
|
-jeffB
Hazard to Others
 
Posts: 185
Registered: 6-12-2007
Member Is Offline
Mood: No Mood
|
|
| Quote: | Originally posted by JohnWW
The isopropyl alcohol sold in hardware or similar stores as "rubbing alcohol" is usually only the distilled stuff containing only about 70% of the
stuff, and 30% water, because of the isopropanol-water constant-boiling-point azeotrope. Purer isopropanol is more expensive, probably obtained by a
further distillation with benzene, like absolute ethanol. |
In the US it's common to find "91%" (by volume) isopropanol. This is presumably the azeotrope, which is actually 87% IPA and 13% water:
http://www.shellchemicals.com/alcohols/1,1098,1089,00.html#2...
I seem to remember that diluting the mix to 70% IPA by volume makes it less flammable and less harsh on the skin, but 91% is still widely available.
I ran a fractionation of 70% IPA to try out my distillation setup. There were no surprises, the vapor temperature behaved as I expected, and the
product burned like "91%" IPA, but I didn't do any density or other measurements to verify my results.
Wikipedia says the industrial processes for anhydrous IPA use cyclohexane or diisopropyl ether as azeotroping agents.
|
|
|
YT2095
International Hazard
   
Posts: 1091
Registered: 31-5-2003
Location: Just left of Europe and down a bit.
Member Is Offline
Mood: within Nominal Parameters
|
|
the medi-swab IPA doesn`t work, nor does Paraffin ( a Kerosene analog).
maybe the IPA was too pure or something? as for the Paraffin, I didn`t really expect that would work anyway since WD-40 didn`t touch it either.
\"In a world full of wonders mankind has managed to invent boredom\" - Death
Twinkies don\'t have a shelf life. They have a half-life! -Caine (a friend of mine)
|
|
|
chemrox
International Hazard
   
Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline
Mood: LaGrangian
|
|
I find 99% in the pharmacy in 750 ml bottles as "isopropyl alcohol." We use it in the alcohol lamp. My wife goes through a bottle every two months
or so. This is in the US; home of controls.
"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
|
|
|
Saerynide
National Hazard
  
Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline
Mood: Ionic
|
|
Theres a petroleum based solvent product here in the US and Canada called "Goo Gone". It's yellowish and comes in a clear bottle and smells like
orange/citrus. Maybe they have it in the UK too?
It works wonders in removing sticky plastic glue from labels, tape, and what have you. So far, it hasn't hurt my plastic, but I always still test
with a small patch first.
"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to...
satisfy any applicable law, regulation or legal process"
|
|
|
pantone159
National Hazard
  
Posts: 594
Registered: 27-6-2006
Location: Austin, TX, USA
Member Is Offline
Mood: desperate for shade
|
|
| Quote: | Originally posted by Saerynide
It's yellowish and comes in a clear bottle and smells like orange/citrus. |
limonene??
|
|
|
Saerynide
National Hazard
  
Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline
Mood: Ionic
|
|
Hmmm.. I never thought of that. The label says its petroleum based, but I guess there could be probably a lot of limonene in there too.
"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to...
satisfy any applicable law, regulation or legal process"
|
|
|
MagicJigPipe
International Hazard
   
Posts: 1555
Registered: 19-9-2007
Location: USA
Member Is Offline
Mood: Suspicious
|
|
| Quote: |
Theres a petroleum based solvent product here in the US and Canada called "Goo Gone". It's yellowish and comes in a clear bottle and smells like
orange/citrus. Maybe they have it in the UK too?
|
I remember it being mostly xylenes. Of course there has to be something that makes it yellow and citrus-smelling.
"There must be no barriers to freedom of inquiry ... There is no place for dogma in science. The scientist is free, and must be free to ask any
question, to doubt any assertion, to seek for any evidence, to correct any errors. ... We know that the only way to avoid error is to detect it and
that the only way to detect it is to be free to inquire. And we know that as long as men are free to ask what they must, free to say what they think,
free to think what they will, freedom can never be lost, and science can never regress." -J. Robert Oppenheimer
|
|
|
unionised
International Hazard
   
Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
IPA OTC in UK
http://www.maplin.co.uk/Search.aspx?criteria=isopropyl&s...
|
|
|