chief
National Hazard
  
Posts: 630
Registered: 19-7-2007
Member Is Offline
Mood: No Mood
|
|
Here a link upon reaching 1300 [Cels] within a standard-microwave-oven,within 5 minutes, using "activated coal" as susceptor :
http://alp.dillingen.de/chemiekongress/doc/Workshopergebniss...
Maybe charcoal would work too ?
|
|
|
Nixie
Hazard to Others
 
Posts: 490
Registered: 12-12-2006
Member Is Offline
Mood: ?
|
|
Why does it need to be activated?
\"Good is a product of the ethical and spiritual artistry of individuals; it cannot be mass-produced.\" --Aldous Huxley
|
|
|
chief
National Hazard
  
Posts: 630
Registered: 19-7-2007
Member Is Offline
Mood: No Mood
|
|
I don't know if "activated" does better; I now tried a cup full of charcoal for 2 minutes: It heated up (but did not glow, neither catched fire) and
now is 2 half-cups; but it also had some solid NaCl-melt on the bottom, from a previous run, so maybe the cup was weak already ...
|
|
|
FrankRizzo
Hazard to Others
 
Posts: 207
Registered: 9-2-2004
Member Is Offline
Mood: No Mood
|
|
I *believe* that graphite will work. Maybe paint it on to the inner surface of the crucible with sodium silicate solution?
|
|
|
Nixie
Hazard to Others
 
Posts: 490
Registered: 12-12-2006
Member Is Offline
Mood: ?
|
|
I remember crushing up a silicon carbide grinding wheel and that worked best (bonded with clay). Second place was a ferrite yoke from an old TV.
Serious insulation is critical to get something really hot because the losses to the environment are huge when you get a decent temperature going (and
don't forget to block the fan grille on the inside of the oven cavity).
[Edited on 9-10-2008 by Nixie]
\"Good is a product of the ethical and spiritual artistry of individuals; it cannot be mass-produced.\" --Aldous Huxley
|
|
|
FrankRizzo
Hazard to Others
 
Posts: 207
Registered: 9-2-2004
Member Is Offline
Mood: No Mood
|
|
Silicon carbide can also be found in an already powdered form as well. Any online lapidary supply will have it in various particle sizes for use as a
grinding grit.
Carbon would seem to be the better material as it will withstand much higher temperatures.
|
|
|
Texium
|