Author: Subject: adapting a domestic MW
chief
National Hazard
****




Posts: 630
Registered: 19-7-2007
Member Is Offline

Mood: No Mood

[*] posted on 9-10-2008 at 07:55


Here a link upon reaching 1300 [Cels] within a standard-microwave-oven,within 5 minutes, using "activated coal" as susceptor :
http://alp.dillingen.de/chemiekongress/doc/Workshopergebniss...

Maybe charcoal would work too ?
View user's profile View All Posts By User
Nixie
Hazard to Others
***




Posts: 490
Registered: 12-12-2006
Member Is Offline

Mood: ?

[*] posted on 9-10-2008 at 10:38


Why does it need to be activated?



\"Good is a product of the ethical and spiritual artistry of individuals; it cannot be mass-produced.\" --Aldous Huxley
View user's profile View All Posts By User
chief
National Hazard
****




Posts: 630
Registered: 19-7-2007
Member Is Offline

Mood: No Mood

[*] posted on 9-10-2008 at 11:27


I don't know if "activated" does better; I now tried a cup full of charcoal for 2 minutes: It heated up (but did not glow, neither catched fire) and now is 2 half-cups; but it also had some solid NaCl-melt on the bottom, from a previous run, so maybe the cup was weak already ...
View user's profile View All Posts By User
FrankRizzo
Hazard to Others
***




Posts: 207
Registered: 9-2-2004
Member Is Offline

Mood: No Mood

[*] posted on 9-10-2008 at 13:41


I *believe* that graphite will work. Maybe paint it on to the inner surface of the crucible with sodium silicate solution?
View user's profile View All Posts By User
Nixie
Hazard to Others
***




Posts: 490
Registered: 12-12-2006
Member Is Offline

Mood: ?

[*] posted on 9-10-2008 at 15:01


I remember crushing up a silicon carbide grinding wheel and that worked best (bonded with clay). Second place was a ferrite yoke from an old TV. Serious insulation is critical to get something really hot because the losses to the environment are huge when you get a decent temperature going (and don't forget to block the fan grille on the inside of the oven cavity).

[Edited on 9-10-2008 by Nixie]




\"Good is a product of the ethical and spiritual artistry of individuals; it cannot be mass-produced.\" --Aldous Huxley
View user's profile View All Posts By User
FrankRizzo
Hazard to Others
***




Posts: 207
Registered: 9-2-2004
Member Is Offline

Mood: No Mood

[*] posted on 9-10-2008 at 16:13


Silicon carbide can also be found in an already powdered form as well. Any online lapidary supply will have it in various particle sizes for use as a grinding grit.

Carbon would seem to be the better material as it will withstand much higher temperatures.
View user's profile View All Posts By User