microcosmicus
Hazard to Others
 
Posts: 287
Registered: 31-12-2007
Member Is Offline
Mood: spin up
|
|
| Quote: |
Still toluene is the best solvent for contact adhesive,
I'm sure its used that way in the US as well.
|
Not anymore --- while hardware stores here carry plenty of
contact adhesives. the overwhelming majority no longer
carry toluene here. Rather, Americans are expected to make
do with other solvents or perhaps cleaning fluids which contain
toluene mixed with other ingredients.
[Edited on 2-4-2008 by microcosmicus]
|
|
|
MagicJigPipe
International Hazard
   
Posts: 1555
Registered: 19-9-2007
Location: USA
Member Is Offline
Mood: Suspicious
|
|
From what I've read the average benzene content in gasoline in the US 1% or less.
Microcosmicus is right. Toluene is only available in the US at a handful of places. Most of the non-specialist/big chain stores no longer carry it.
In my area it seems to be due to the meth scare hence my experience with attempting to obtain it.
The solvent supplier I go to gave me a brochure the last time I went. Next to toluene it says "Restricted". I need to ask them why when I get a
chance. Something tells me I already know.
"There must be no barriers to freedom of inquiry ... There is no place for dogma in science. The scientist is free, and must be free to ask any
question, to doubt any assertion, to seek for any evidence, to correct any errors. ... We know that the only way to avoid error is to detect it and
that the only way to detect it is to be free to inquire. And we know that as long as men are free to ask what they must, free to say what they think,
free to think what they will, freedom can never be lost, and science can never regress." -J. Robert Oppenheimer
|
|
|
jimwig
Hazard to Others
 
Posts: 215
Registered: 17-5-2003
Location: the sunny south
Member Is Offline
Mood: No Mood
|
|
tolurne is still out there you just have to find it.
craZy jiM wGGns
--packrat, professional bum. -- once just tired
now REtired.
|
|
|
MagicJigPipe
International Hazard
   
Posts: 1555
Registered: 19-9-2007
Location: USA
Member Is Offline
Mood: Suspicious
|
|
"tolurne is still out there you just have to find it."
Yes, I know. What I was saying is that it is getting harder and harder to find. I remember when I posted the thread "Chemicals to Stock Up On" I
mentioned something about my experiences trying to obtain toluene.
I really think we need to get that thread going again. Many called me paranoid then but it seems as if people are starting to see what I was talking
about.
"There must be no barriers to freedom of inquiry ... There is no place for dogma in science. The scientist is free, and must be free to ask any
question, to doubt any assertion, to seek for any evidence, to correct any errors. ... We know that the only way to avoid error is to detect it and
that the only way to detect it is to be free to inquire. And we know that as long as men are free to ask what they must, free to say what they think,
free to think what they will, freedom can never be lost, and science can never regress." -J. Robert Oppenheimer
|
|
|
Panache
International Hazard
   
Posts: 1290
Registered: 18-10-2007
Member Is Offline
Mood: Instead of being my deliverance, she had a resemblance to a Kat named Frankenstein
|
|
interesting read len1.
I had to read it several times to fully absorb it, i have some questions though and apologise in advance if they are silly.
You didn't quote a bp range for the distillation carried out on the mono/di/tri chlorides after the UV rxn step, is there a reason for this? It
appears that you spent considerable effort to remove the unreacted monochloride after the hydrolysis and i understand this was tricky given its
similar bp to that of benzaldehyde but i wonder why you wouldn't fractionate it out before the hydrolysis, i'm sure there is a sound reason.
Finally, given it took considerable effort, it would appear, to ensure that small amounts of benzaldehyde did not get carried out through the HCl vent
gases during the acid hydrolysis did you perhaps consider using this instead as your method to remove the chloride, by instead fractionally steam
distilling the benzaldehyde as it forms during the hydrolysis? You could collect the HCl gas/benzaldehyde water in a water trap. I'm sure there is
reason why this is not done also.
Further to this i am interested in discussing the mechanism's for the chlorination, as i understand the initial step is formation of the chlorine
radical by the UV photon, the chlorine radical then has to successfully collide with the toluene to begin the chain of transforms leading ultimately
to the HCl elimination. It would appear to me that the half-life of the chlorine radical, at temperature, in toluene is the rate determining factor.
Unless of course, the half-life is so small that it essentially requires the Cl2 molecule to be in the vicinity of, and have a favourable orientation
to, the benzylic carbon at the time it absorbs the UV photon.
As expected attempting to find any data on the chlorine radical under these conditions led to nothing, however i feel i am quite internet unsavvy so
it may be my ineptness in searching, not lack of data available.
This is the point where this discussion has too many unknowns for it to continue to be worthwhile. Any light you or anyone else could shed on this
would be of interest as it would help in establishing the optimal position for the uv light source.
Your time spent collating your practical efforts are appreciated and enjoyed, thank-you very much for the write up.
mark
[Edited on 21-5-2008 by Panache]
|
|
|
len1
National Hazard
  
Posts: 595
Registered: 1-3-2007
Member Is Offline
Mood: NZ 1 (goal) - Italy 1 (dive)
|
|
| Quote: | You didn't quote a bp range for the distillation carried out on the mono/di/tri chlorides after the UV rxn step, is there a reason for this? It
appears that you spent considerable effort to remove the unreacted monochloride after the hydrolysis and i understand this was tricky given its
similar bp to that of benzaldehyde but i wonder why you wouldn't fractionate it out before the hydrolysis, i'm sure there is a sound reason.
Finally, given it took considerable effort, it would appear, to ensure that small amounts of benzaldehyde did not get carried out through the HCl vent
gases during the acid hydrolysis did you perhaps consider using this instead as your method to remove the chloride, by instead fractionally steam
distilling the benzaldehyde as it forms during the hydrolysis? You could collect the HCl gas/benzaldehyde water in a water trap. I'm sure there is
reason why this is not done also. |
Interesting questions. First the distillation was done to separate the benzylCl2 from the condensation tars rather than from the benzylCl. The bps
are 205C/179C respectively and therein lies the answer why no fractional distillation was attempted. Its an interesting idea to let the BzO distill
with the HCl as its formed so shifting the equilibrium. I might try this keeping in mind success is not guaranteed given that the chlorotoluenes
might come along for the ride - their bps are similar to that of the benzaldehyde and it will have to be extra binding strength of BzO to water if
this is to work - the distilate will have to be analyzed, and assuming its 90% or more percent free of reactant this could be a goer.
If you look at the section on the photocatalysis I did some investigations as to rate determining step. I found increase in light flux does not
substantially increase chlorination rate, thus all Cl2 is essentially 'radicalised' and its the reaction of radical with toluene thats the rate
determining step in my setup.
|
|
|
Siddy
Hazard to Self

Posts: 81
Registered: 8-10-2007
Member Is Offline
Mood: No Mood
|
|
Your hydrolysis product is Benzaldehyde and Benzyl Chloride?
Did you consider adding hyroxide (as salt) to convert to benzyl alcohol?
eg NaOH (in EtOH) + BzCl > NaCl + BzOH.
Then you have Benzaldehyde and Benzyl alcohol, either fractionally distil or even add persulfate to oxidise the alcohol to aldehyde. Excess of
reagents will leave only very little Benzyl Chloride. Benzaldehyde should remain unchanged from stong base and persulfate.
|
|
|
len1
National Hazard
  
Posts: 595
Registered: 1-3-2007
Member Is Offline
Mood: NZ 1 (goal) - Italy 1 (dive)
|
|
If you read carefuly my article you would know thats not possible.
|
|
|
jimwig
Hazard to Others
 
Posts: 215
Registered: 17-5-2003
Location: the sunny south
Member Is Offline
Mood: No Mood
|
|
a big thanky goes out to mr lens for all his highly informative info.
thanks you, SIR
craZy jiM wGGns
--packrat, professional bum. -- once just tired
now REtired.
|
|
|
Panache
International Hazard
   
Posts: 1290
Registered: 18-10-2007
Member Is Offline
Mood: Instead of being my deliverance, she had a resemblance to a Kat named Frankenstein
|
|
| Quote: | Originally posted by len1
| Quote: | You didn't quote a bp range for the distillation carried out on the mono/di/tri chlorides after the UV rxn step, is there a reason for this? It
appears that you spent considerable effort to remove the unreacted monochloride after the hydrolysis and i understand this was tricky given its
similar bp to that of benzaldehyde but i wonder why you wouldn't fractionate it out before the hydrolysis, i'm sure there is a sound reason.
Finally, given it took considerable effort, it would appear, to ensure that small amounts of benzaldehyde did not get carried out through the HCl vent
gases during the acid hydrolysis did you perhaps consider using this instead as your method to remove the chloride, by instead fractionally steam
distilling the benzaldehyde as it forms during the hydrolysis? You could collect the HCl gas/benzaldehyde water in a water trap. I'm sure there is
reason why this is not done also. |
Interesting questions. First the distillation was done to separate the benzylCl2 from the condensation tars rather than from the benzylCl. The bps
are 205C/179C respectively and therein lies the answer why no fractional distillation was attempted. Its an interesting idea to let the BzO distill
with the HCl as its formed so shifting the equilibrium. I might try this keeping in mind success is not guaranteed given that the chlorotoluenes
might come along for the ride - their bps are similar to that of the benzaldehyde and it will have to be extra binding strength of BzO to water if
this is to work - the distilate will have to be analyzed, and assuming its 90% or more percent free of reactant this could be a goer.
If you look at the section on the photocatalysis I did some investigations as to rate determining step. I found increase in light flux does not
substantially increase chlorination rate, thus all Cl2 is essentially 'radicalised' and its the reaction of radical with toluene thats the rate
determining step in my setup. |
I have up until now had issue with this, however unable to frame my arguments coherently i have had to wait until i found someone else who could or
until i understood what my issues were.
My main issue is that the photo initation step, namely the formation of the chlorine radical, occurs only in the vapour phase. Re-reading your
response i see you now never said that rather you said that 'in my setup' it appears all chemistry occurs in the vapour phase. i believe Not important
also mentions earlier a large column packed with broken glass that the cl2/hcl fractionated upwards through and this is the point his light source is
positioned.
Well someone else described it for me, namely here
http://www.faizkaskar.8k.com/light1.html
For those unwilling to trawl through the various pages on photochlorination of toluene, the argument is quite basic, the Cl2 molecule has a bond
energy that correesponds to the energy of a photon of light of wavelength of 488nm or obviously lower (more energy again). The 488 nm slightly below
is blue light quickly descending into the UV range as the wavelength drops.
Once you have light of this wavelength or lower (and hence higher energy) the key parameter is the extinction coefficient of the wavelength of light
being used. It determines how far into the solution the light will travel before being, well extinct. For blue light a simple calculation will give a
penetration of roughly 11.5cm into toluene before 90% of the radiation is absorbed, whereas UV will only travel 0.3cm for 90% of radiation to be
absorbed. In the gas phase obviously both penetrate much further.
Hence the reason the reaction appears not to occur in the liquid phase is that no uV is effectively getting to the reagants. The author advocates
intense blue being used directly into the liquid phase.
The link explains it much better.
I might try this out this weekend, with a run using a blue light focused only on the solution and see if the reactions occurs more conveniently.
|
|
|
Sauron
International Hazard
   
Posts: 5351
Registered: 22-12-2006
Location: Barad-Dur, Mordor
Member Is Offline
Mood: metastable
|
|
Len1 has not posted for some time. I thinknthe prch light is on but nobody's home.
The radical chlorination of toluene in liquid phase with SO2Cl2 and benzoyl peroxide or AIBN initiation works quite well. In fact it will proceed to
banzaldichloride is 2 mols SO2Cl2 are used. This reaction of course has nothing to do with photochemistry and proceeds just fine in the dark and well
below the reflux temperature of toluene.
Sic gorgeamus a los subjectatus nunc.
|
|
|
len1
National Hazard
  
Posts: 595
Registered: 1-3-2007
Member Is Offline
Mood: NZ 1 (goal) - Italy 1 (dive)
|
|
I am still here, but have gotten a bit tired writing these articles since I dont see where this is leading to. To be honest a number of the
preparations I posted I had to do at work a while back and in what I posted here I adapted them for the amateur since I thought it a way to make these
known and I couldnt publish them in the literature as they do not represent the synthesis of anything 'new'. Now Im thinking of releasing them as a
compilation soon.
|
|
|
kclo4
National Hazard
  
Posts: 916
Registered: 11-12-2004
Location:
Member Is Offline
Mood: No Mood
|
|
| Quote: | Originally posted by len1
Now Im thinking of releasing them as a compilation soon. |
That would be very cool! I'd love to see that
|
|
|
starman
Hazard to Others
 
Posts: 318
Registered: 5-7-2008
Location: Western Australia
Member Is Offline
Mood: No Mood
|
|
| Quote: | Originally posted by len1
I am still here, but have gotten a bit tired writing these articles since I dont see where this is leading to. To be honest a number of the
preparations I posted I had to do at work a while back and in what I posted here I adapted them for the amateur since I thought it a way to make these
known and I couldnt publish them in the literature as they do not represent the synthesis of anything 'new'. Now Im thinking of releasing them as a
compilation soon. |
Len IMHO your "illustrated guides" pretty much set the standard on this board.I hope you can continue to find time and motivation to prepare
them.Whilst,perhaps,they represent nothing 'new' and hence perhaps somewhat tedious for you.For me and I'm sure many others find them clear,concise,
workable instructions that fill in the gaps of preparatory manuals like Vogels.
Perhaps it not professional publication,but it is certainly inspiring to non academic researchers such as myself.
Please keep up the good work!
|
|
|
Fleaker
International Hazard
   
Posts: 1254
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
Nice to see you back Len!
To be honest, I think if you collated all of your various syntheses together and did a few more, you could make quite the book(let) for the advanced
amateur chemist.
Your illustrated syntheses are always a pleasure to read.
Neither flask nor beaker.
"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
|
|
|
timtam
Harmless
Posts: 1
Registered: 31-1-2009
Member Is Offline
Mood: No Mood
|
|
its a very big help for my pre-laboratory discussions. thank you. I just wonder if you could supply me the NET EQUATION for the pathway of benzal
chloride to benzaldehyde. thanks
|
|
|
Sauron
International Hazard
   
Posts: 5351
Registered: 22-12-2006
Location: Barad-Dur, Mordor
Member Is Offline
Mood: metastable
|
|
I suggest you send a PM (private message) to len1
Use the U2U (User to User) buttom just below one of his posts.
Sic gorgeamus a los subjectatus nunc.
|
|
|
benzylchloride1
Hazard to Others
 
Posts: 299
Registered: 16-3-2007
Member Is Offline
Mood: Pushing the envelope of synthetic chemistry in one's basement
|
|
I am currently preparing benzaldehyde using Len's method, but running the reaction on a 1 mole scale. I currently have about 118g of benzal chloride
that I prepared last weekend. The reaction is very slow using a 60 W light bulb. The reaction took me about 12 hours. I ended up distilling the
product at 8 hours, but it still had a density of 1.18. I chlornated for another 4 hours and ended up with a product that has a density of 1.23. The
CRC Handbook of Organic Compound Identification states that benzal chloride has a density of 1.295.
Amateur NMR spectroscopist
|
|
|
chemrox
International Hazard
   
Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline
Mood: LaGrangian
|
|
Very nice writeup. I did NOT find it "too wordy." I would suggest being more 'academic' and listing at least the key refs. I missed one detail: I
don't see where you identified the light source you used. Light sources are much on my mind these days and I want all the information and suggestions
I can find on uv sources for free radical reax. Thanks for the post. CRX
"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
|
|
|
mowsala
Harmless
Posts: 9
Registered: 9-10-2010
Location: UK
Member Is Offline
Mood: No Mood
|
|
If anyone's still after benzyl alcohol to go backwards, I've got it cheap from here (UK, but I think they'll ship worldwide): www.thesoapkitchen.co.uk
£7.75 a litre. well I could barely get toluene for that price.
|
|
|
497
National Hazard
  
Posts: 778
Registered: 6-10-2007
Member Is Offline
Mood: HSbF6
|
|
I haven't seen any mention of this, so I thought I'd ask.
Wouldn't a "black light" be well suited for catalyzing radical chlorination? The main emission peak is around 400nm, which seems pretty ideal for this
purpose. Is this really the case?
|
|
|
Waffles SS
Fighter
   
Posts: 1019
Registered: 7-12-2009
Member Is Offline
|
|
Have you ever tried Blanc chloromethylation?
| Quote: |

The Blanc chloromethylation is the chemical reaction of aromatic rings with formaldehyde and hydrogen chloride catalyzed by zinc chloride to form
chloromethyl arenes. The reaction should be performed with care, as (like most chloromethylation reactions) it produces highly carcinogenic
bis(chloromethyl) ether as a by-product.
http://en.wikipedia.org/wiki/Blanc_chloromethylation
|
http://www.scielo.cl/scielo.php?pid=S0717-97072010000100023&...
http://universitypublishingonline.org/foundation/chapter.jsf...
|
|
|
Vargouille
Hazard to Others
 
Posts: 380
Registered: 16-4-2012
Member Is Offline
Mood: No Mood
|
|
No questions. Spam reported.
|
|
|