Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Thought you'd like to see this (eye taffy)
jgourlay
Hazard to Others
***




Posts: 249
Registered: 9-7-2008
Member Is Offline

Mood: No Mood

[*] posted on 1-6-2009 at 03:06
Thought you'd like to see this (eye taffy)


Gents, I'm posting this picture simply for the "gee whiz!" factor. This is the drain hole of a little furnace I use for melting this and that. Right now it's firing a pot and is just causing the cone 6 cone to bend over.

What you're looking at is a soft billowy flame coming out of the drain hole. The drain hole is there in case a crucible breaks. At this point, the drain hole is covered by a plinth so I'm guessing there is blow by. The clay is a Raku clay, and the source is propane.

The color you see is exactly right, and not a problem with the camera. Down below, you see a red glow. This is incandescence coming from the furnace through the drain hole, ie the plinth bottom.



View user's profile View All Posts By User
FrankRizzo
Hazard to Others
***




Posts: 209
Registered: 9-2-2004
Member Is Offline

Mood: No Mood

[*] posted on 1-6-2009 at 17:48


Neat! Must be some barium salts in the glaze of that Raku piece.
View user's profile View All Posts By User
Elawr
Hazard to Others
***




Posts: 174
Registered: 4-6-2006
Location: Alabama
Member Is Offline

Mood: vitriolic

[*] posted on 2-6-2009 at 21:46


Beautiful...

Please tell us more about your furnace! Is it of your own manufacture? It looks to made of some kind of castable refractory...can I ask what composition you used?




1
View user's profile View All Posts By User
jgourlay
Hazard to Others
***




Posts: 249
Registered: 9-7-2008
Member Is Offline

Mood: No Mood

[*] posted on 3-6-2009 at 02:57


Elawr: thanks! I'll answer your question this weekend when I have more time!

In the meantime: www.backyardmetalcasting.com --> 2 bucks furnace and Reil burner.
View user's profile View All Posts By User