Polystyrene Microspheres
Gday Gents,
Did a pretty simple experiment today and figured id share.
I wanted to make some polystyrene Microspheres to use to help characterise some imaging equipment.
So I de-solved some polystyrene in acetone. I was surprised to find that only a small amount of the polystyrene is soluble in acetone despite hours
of stirring the bulk of the 'disolved' styrene just sat at the bottom of the beaker as a floaty fluffy marshmellow type blob.
None the less I decanted the non marshmellow acetone off and added an equal amount of water producing a opaque milky suspension.
I then put a drop of this liquid onto a clean microscope slide evaporated it and had a look.
and this is what i saw.
![microsphears.jpg - 56kB](https://www.sciencemadness.org/whisper/files.php?pid=193068&aid=12064)
Im not sure if these are usefull for much but they seem look similar to some old comercal microsphears I found
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
It's consistent with a latex of polystyrene forming in the acetone/water liquid phase...
|
|