Can you extract MEKP from commercial liquid resin hardners?
This is a pretty interesting question in which i have been unable to find an answer for.
There are commercial catalysts used to harden resins that contain MEKP, but in dilute form. The average I am hearing is about 40% - 60%. Some of the
ingredients used to dilute MEKP according to the MSDS for one manufacturer of MEKP resin hardener are:
Methyl Ethyl Ketone Peroxide - 34%
Dimethyl Phthalate - 43%
2,2,4-Trimethyl-1,3-pentanediol diisobutyrate - 20
%
Hydrogen Peroxide - 01%
Methyl Ethyl Ketone - 02%
Water - 01%
Here is the msds link: http://www.eagerplastics.com/mekp.htm
Supplier link: http://www.tapplastics.com/shop/product.php?pid=40
Is there anyway to safely and easily extract the MEKP from these hardeners, or is it just easier to make it yourself. I ask because a 10oz bottle only
cost $8 dollars, and will yield 3.4oz of MEKP, if it could all be extracted. plus no hassle of dealing with temperature control, acids, and I would
assume a much better, and higher quality product in the end.
|
|
Saerynide
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline
Mood: Ionic
|
|
I dont think its worth it. My resin hardener contains much less than 34% MEKP and it cost $6 for a meager 1 fl oz. Better save it for making acrylic
casts
"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to...
satisfy any applicable law, regulation or legal process"
|
|
DougTheMapper
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 145
Registered: 20-7-2008
Location: Michigan, USA
Member Is Offline
Mood: Energetic
|
|
Even if you could extract it reasonably efficiently, that's 100mL for $8, putting your price at 8 cents per milliliter. I bought a gallon of MEK for
$21, a gallon of 31% HCl for $8, and I simmer down $1 quarts of 3% H2O2 for a total of around 3 cents per mL.
Everyone complains about this synth being difficult compared to TATP, but I really don't see why. I think it's worth it since this stuff is less
sensitive. It takes maybe 5 minutes to measure everything, then stick it in the fridge for an hour, 5 more to mix everything, forget it for 24 hours,
20 mins to neutralize and isolate... So 30 minutes? And if you have a Florence flask and a syringe, the isolated product is clean, clear, and free of
pesky water bubbles as long as you're careful.
|
|
crazywantabies
Harmless
Posts: 7
Registered: 12-3-2011
Member Is Offline
Mood: No Mood
|
|
I have the hardener, yet, A SAFE FORMALDEHYDE plastic rosin???? I will personally donate 20.00 to any brother or sister's favorite charity- IN THE
name of
part time stickered "slow" bumper stickers on vehicles, THE BOX and future consciousness "sin" detection unit P.E.A.R. project "baby- FOR A SAFER
FORMALDEHYDE PLASTIC RESIN idea. )
|
|
Bot0nist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1559
Registered: 15-2-2011
Location: Right behind you.
Member Is Offline
Mood: Streching my cotyledons.
|
|
I second DougTheMapper. Why the hell would you want to go through a cumbersome extraction for a compound that is:
A.) Not very useful.
B.) So trivial to synthesis that even the dullest of kewls could procure fine yields with minimal effort.
If it's a problem with being able to find the required chemicals to synthesize, then I assure you that the reagents needed for a clean extraction
would be much more of a daunting task to acquire.
[Edited on 20-3-2011 by Bot0nist]
|
|
Fossil
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 131
Registered: 4-4-2012
Location: Canada
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by DougTheMapper ![](images/xpblue/lastpost.gif) | Even if you could extract it reasonably efficiently, that's 100mL for $8, putting your price at 8 cents per milliliter. I bought a gallon of MEK for
$21, a gallon of 31% HCl for $8, and I simmer down $1 quarts of 3% H2O2 for a total of around 3 cents per mL.
Everyone complains about this synth being difficult compared to TATP, but I really don't see why. I think it's worth it since this stuff is less
sensitive. It takes maybe 5 minutes to measure everything, then stick it in the fridge for an hour, 5 more to mix everything, forget it for 24 hours,
20 mins to neutralize and isolate... So 30 minutes? And if you have a Florence flask and a syringe, the isolated product is clean, clear, and free of
pesky water bubbles as long as you're careful. |
Could you send me the procedure you use for this please. All of the methods of manufacture that I have found involve sulfuric acid, which I have
considerably less of than I do Hydrochloric acid.
What concentration Hydrochloric acid do you use and how far down do you concentrate the hydrogen peroxide, as in how much do you reduce it from its
original volume.
|
|
Bot0nist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1559
Registered: 15-2-2011
Location: Right behind you.
Member Is Offline
Mood: Streching my cotyledons.
|
|
Quote: Originally posted by Fossil ![](images/xpblue/lastpost.gif) | Quote: Originally posted by DougTheMapper ![](images/xpblue/lastpost.gif) | Even if you could extract it reasonably efficiently, that's 100mL for $8, putting your price at 8 cents per milliliter. I bought a gallon of MEK for
$21, a gallon of 31% HCl for $8, and I simmer down $1 quarts of 3% H2O2 for a total of around 3 cents per mL.
Everyone complains about this synth being difficult compared to TATP, but I really don't see why. I think it's worth it since this stuff is less
sensitive. It takes maybe 5 minutes to measure everything, then stick it in the fridge for an hour, 5 more to mix everything, forget it for 24 hours,
20 mins to neutralize and isolate... So 30 minutes? And if you have a Florence flask and a syringe, the isolated product is clean, clear, and free of
pesky water bubbles as long as you're careful. |
Could you send me the procedure you use for this please. All of the methods of manufacture that I have found involve sulfuric acid, which I have
considerably less of than I do Hydrochloric acid.
What concentration Hydrochloric acid do you use and how far down do you concentrate the hydrogen peroxide, as in how much do you reduce it from its
original volume. |
Don't blatantly ask for spoonfeeding on stupidly sensitive primaries, please.![:D](./images/smilies/biggrin.gif)
A search with the forum engine of Methyl Ethyl Ketone Peroxide would have yielded this thread, http://www.sciencemadness.org/talk/viewthread.php?tid=20 , in which madscientist replied to binary mz's question about varying the acid catalyst;
Quote: Originally posted by madscientist ![](images/xpblue/lastpost.gif) | If the temperature of the reaction is kept low, I suppose HCl could be used.
As for adding the H<sub>2</sub>SO<sub>4</sub>, I suggest diluting it prior to adding it to the solution prepared by mixing MEK
with hydrogen peroxide. |
Binary mz later posts that he has tried it, to success.
_________________________________________________
Quote: Originally posted by Fossil ![](images/xpblue/lastpost.gif) |
What concentration Hydrochloric acid do you use and how far down do you concentrate the hydrogen peroxide, as in how much do you reduce it from its
original volume. |
Concentrating H<sub>2</sub>O<sub>2</sub> and determining it's concentration.
http://www.sciencemadness.org/talk/viewthread.php?tid=18829&...
http://www.sciencemadness.org/talk/viewthread.php?tid=16726&...
http://www.sciencemadness.org/talk/viewthread.php?tid=15283&...
http://www.sciencemadness.org/talk/viewthread.php?tid=15283&...
http://www.sciencemadness.org/talk/viewthread.php?tid=1325&a...
Can 3% H<sub>2</sub>O<sub>2</sub> be used in the synthesis of energetic peroxides?
http://www.sciencemadness.org/talk/viewthread.php?tid=8420&a...
http://www.sciencemadness.org/talk/viewthread.php?tid=8425&a...
There are a lot more. Don't be lazy. READ.
UTFSE !!!! ![:P](./images/smilies/tongue.gif)
[Edited on 9-4-2012 by Bot0nist]
U.T.F.S.E. and learn the joys of autodidacticism!
Don't judge each day only by the harvest you reap, but also by the seeds you sow.
|
|
|