spirocycle
Hazard to Others
 
Posts: 197
Registered: 29-9-2010
Member Is Offline
Mood: No Mood
|
|
styrene
I'm trying to make acetophenone from styrene, but I am having issues sourcing styrene.
all my searches are clogged with plastic, of which no detailed composition is given.
Anyone have a place that sells pure styrene?
or maybe a method to get reasonably pure styrene from common sources?
I have read briefly about destructive polymerization, but i'd rather not go about melting plastic, because it seems like it'd make a big smelly mess.
|
|
|
Fleaker
International Hazard
   
Posts: 1254
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
You don't want to distill styrofoam of PS cups. A lot of really stinky things are produced.
Instead, go to a place that supplies fiberglass shops. It's fairly cheap, about $30/US gallon.
Neither flask nor beaker.
"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
|
|
|
Contrabasso
Hazard to Others
 
Posts: 277
Registered: 2-4-2008
Member Is Offline
Mood: No Mood
|
|
IIRC thinners 101 (or is it 1001?) is styrene as used in the GRP industry for thinning the polyester resin. Yes it is (was ) available in big cans,
BUT as a functional thinners for a work process it may (will) not be technical grade.
|
|
|
smuv
National Hazard
  
Posts: 842
Registered: 2-5-2007
Member Is Offline
Mood: Jingoistic
|
|
http://www.tapplastics.com/shop/product.php?pid=41&http:...
look for styrene monomer
|
|
|
Gualterio_Malatesta
Harmless
Posts: 39
Registered: 8-1-2010
Member Is Offline
Mood: No Mood
|
|
I don't really wanna question your authority here, if you tried that personally, 'cause I hadn't.
But I've read reports of people having successfully pyrolyzed CD boxes (PS) to yield styrene.
Just my two cents.
|
|
|
Hexagon
Harmless
Posts: 45
Registered: 11-5-2010
Member Is Offline
Mood: Fanf*ckingtastic
|
|
Styrene monomer is cheap and a readily available stuff, and it's true that you can pirolize CD cases, yougurth cups, what ever is made with PS, to
styrene monomer if you dont want to deal with supply houses or you want to go on the cheap as free schale. The monomer will not be as pure as the
comercial one though.
|
|
|
ScienceSquirrel
International Hazard
   
Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline
Mood: Dogs are pets but cats are little furry humans with four feet and self determination!
|
|
The pyrolysis of polystyrene will produce a reasonable sample of styrene of about 50 - 75% purity from the examples I have seen.
If you are going to make acetophenone out of it this is good enough as you can clean it up at the next stage.
|
|
|
Hexagon
Harmless
Posts: 45
Registered: 11-5-2010
Member Is Offline
Mood: Fanf*ckingtastic
|
|
Distilling out the monomer from the pyrolized mixture should yield pure styrene, the remaining high boilers upon another pyrolization should yield
more impure styrene, true?
|
|
|
ScienceSquirrel
International Hazard
   
Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline
Mood: Dogs are pets but cats are little furry humans with four feet and self determination!
|
|
It depends on the conditions but there are other things produced eg benzene, toluene, ethylbenzene, napthalene, etc.
There is a lab procedure here and their product seems reasonably pure.
http://chemeducator.org/sbibs/s0008005/spapers/850309rw.pdf
[Edited on 6-4-2011 by ScienceSquirrel]
|
|
|
Fleaker
International Hazard
   
Posts: 1254
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
I have destructively distilled polystyrene foam and extruded product before, and the pyrolysis does not go well. Something that is very lachrymatory
is made and it was an unhappy experience. Maybe I should have vacuum-distilled it.
Neither flask nor beaker.
"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
|
|
|
mowsala
Harmless
Posts: 9
Registered: 9-10-2010
Location: UK
Member Is Offline
Mood: No Mood
|
|
Styrene in the UK:
http://www.ecfibreglasssupplies.co.uk/p-1607-styrene.aspx
They also have MEKP (methyl ethyl ketone peroxide) as 35% solution in dimethyl phthalate if that is of interest to anyone.
And cheap acetone and isopropanol.
|
|
|