Hello, I would make a relatively inert anode with the greatest possible otc.

So this is the choise available to me:

lead dioxide-I have lead, carbon anode, 95% nitric acid and copper.
- problem I do not know the wish consentration of the solution or the type of the apparatus.

ATO anode - I think that applies more to my needs but I do not know in general, I have a welding rod 50/50 tin / antimony.
-the problem, I have no idea (aside from the topic about the ato anode , which recommended alkoloxy tin complex.

Magnetite: I have iron.
-I dont have acétylène torch so I need to put a layer of magnetite on a substrate.

So what of the following would you say to me, and a simple way to make them.

for those wondering, I read over 50 pages about anodes on sciencemadness.


[Edited on 18-1-2011 by plante1999]
View user's profile View All Posts By User
symboom
International Hazard
*****




Posts: 1145
Registered: 11-11-2010
Location: Wrongplanet
Member Is Offline

Mood: Doing science while it is still legal since 2010

[*] posted on 20-4-2011 at 13:59
oxy hydrogen torch


as for heating build an oxy hydrogen torch or if you have propane they have these small oxygen bottles that can be burned with propane for heating acetylene is to expensive or even use a Fresnel lens for heating you can get one from old crt monitors or tvs
there was a patent using hemitite that was prepared from clay sodium nitrate and iron

lead one would be easy easiest electroplate lead dioxide onto an cathode (iron copper) by running electricity through lead nitrate solution and graphite anode
View user's profile View All Posts By User
PolarSmokes
Harmless
*




Posts: 14
Registered: 26-10-2009
Member Is Offline

Mood: No Mood

[*] posted on 28-4-2011 at 15:42


Have you tried to deposit PbO2 on the "poor man's mmo" that you made?