Can Magnesium be extracted from epsom salt easily
Can Magnesium be extracted from Epsom salt easily either by plating it on a metal or chemically somehow.
|
|
|
Neil
National Hazard
  
Posts: 556
Registered: 19-3-2008
Member Is Offline
Mood: No Mood
|
|
Magnesium is prepared by electrolysis of it's molten chloride. So I guess your answer would be no.
|
|
|
cyanureeves
National Hazard
  
Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
i read here that it cannot because there is no magnesium metal in epsom salt rather a magnesium ion. i added ammonium hydroxide to epsom salt to
supposedly get magnesium hydroxide precipitate and ammonium sulphate solution. sure as heck i got a white precipitate and a solution that when dried
was also a white solid about 8 times more than the precipitate. they were both hard as heck to dry. maybe the magnesium hydroxide?
|
|
|
Neil
National Hazard
  
Posts: 556
Registered: 19-3-2008
Member Is Offline
Mood: No Mood
|
|
Yes... and if you calcine it you will have MgO or magnesium oxide. this can be chlorinated to make MgCl2 which can be electrolyzed to yield Mg metal.
It might be possible to super heat MgO with Lithium or Sodium to recover Mg gas, you can react MgO with carbon at around 2000C° but then you would
have 2000C° Mg gas, and good luck containing that.
but no, no Mg straight from MgSO4
|
|
|
symboom
International Hazard
   
Posts: 1145
Registered: 11-11-2010
Location: Wrongplanet
Member Is Offline
Mood: Doing science while it is still legal since 2010
|
|
electrolysis of magnesium oxide in molten calcium chloride then you don't have to worry about chlorine gas carbon dioxide when using a graphite
gouging rod is evolved instead
-melting point of calcium chloride 1,421.6F
-melting point of magnesium metal 1202 °F
might be able to get away without argon which you can get from a welding supply then again you dont want a white hot raging fire
2 ways to magnesium hydroxide to eventually form magnesium oxide by pyrolysis of magnesium hydroxide to oxide.
-first electrolysis of magnesium sulfate to form magnesium hydroxide and sulfuric acid using an ion exchange resin(or mgso4 salt bridge)
-another simpler way
ammonium hydroxide reacts with magnesium sulfate
forming magnesium hydroxide and ammonium sulfate
|
|
|
ScienceSquirrel
International Hazard
   
Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline
Mood: Dogs are pets but cats are little furry humans with four feet and self determination!
|
|
Magnesium is readily and cheaply available as ribbon, turnings and powder in most places.
It is also used in pencil sharpeners, hard disc cases, survival fire lighters, etc.
It is very hard to make in a laboratory and will cost you a lot more than buying it.
|
|
|
c-3h-8
Harmless
Posts: 2
Registered: 3-5-2011
Member Is Offline
Mood: No Mood
|
|
So if I get some Magnesium Chloride at a fish store I could extract Magnesium by electrolysis and does anyone know how to do this what anode and
cathode, temperature ,voltage, and would anything else be needed in the water MCl solution? Also was wondering can Magnesium be anodized?
|
|
|
blogfast25
International Hazard
   
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
@ c-3h-8:
This is your answer.
Quote: Originally posted by ScienceSquirrel  | Magnesium is readily and cheaply available as ribbon, turnings and powder in most places.
It is also used in pencil sharpeners, hard disc cases, survival fire lighters, etc.
It is very hard to make in a laboratory and will cost you a lot more than buying it. |
You're very obviously a beginner. Not one experimenter here, not even the most experienced, has ever tried the electrolysis of molten,
anhydrous MgCl2 to obtain the metal (it doesn't work in solution).
Look up the process on the Tinkerwebs and by all means study it for your knowledge base (there's nothing on the subject that we could teach you that
you can't find in basic web pages on it). But to try this at home lab level isn't just folly... it's also an UNNECESSARY folly!
[Edited on 4-5-2011 by blogfast25]
|
|
|
froot
Hazard to Others
 
Posts: 347
Registered: 23-10-2003
Location: South Africa
Member Is Offline
Mood: refluxed
|
|
You can obtain milk of magnesia at a local chemist.
Basically - (the principle, not the procedure)
Heat it above 400 deg C to dehydrate it leaving MgO.
Mix the MgO with carbon powder and heat it in a closed vented steel capsule to about 1000 Deg C.
MgO + C -> Mg + CO
Decant the molten Mg while it is above 700 deg C
If the molten Magnesium comes in contact with oxygen or water at any stage you may very well end up miamed for life. Think about that very carefully
when you design the capsule and the decanting procedure.
We salute the improvement of the human genome by honoring those who remove themselves from it.
Of necessity, this honor is generally bestowed posthumously. - www.darwinawards.com
|
|
|
Neil
National Hazard
  
Posts: 556
Registered: 19-3-2008
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by ScienceSquirrel  | Magnesium is readily and cheaply available as ribbon, turnings and powder in most places.
It is also used in pencil sharpeners, hard disc cases, survival fire lighters, etc.
It is very hard to make in a laboratory and will cost you a lot more than buying it. |
You can test to see if something is Mg or Al by preforming a spark test against a grinding wheel. Mg will spark, Al will not.
|
|
|
m1tanker78
National Hazard
  
Posts: 685
Registered: 5-1-2011
Member Is Offline
Mood: No Mood
|
|
From experience, magnesium formed by molten electrolysis is very short-lived. You'll see a bright blue-white flash of light and be glad you were
wearing protective gear (or possibly spend some time in your favorite hospital trying to rescue your eyesight if no protective gear). A fair bit of
molten electrolyte is ejected in the process. I'm sure there's a way to tame the hot Mg some but it's not worth the time or effort IMO. Trying to do
this in an inert environment puts it out of reach for most experimenters.
Mg fire starter: ~$2.49 (USD) for 25 grams or so. That's roughly 10 cents a gram. Even yours truly went out and bought a couple of Mg fire starter
blocks for a rainy day. 
Tank
|
|
|
blogfast25
International Hazard
   
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by froot  |
Mix the MgO with carbon powder and heat it in a closed vented steel capsule to about 1000 Deg C.
MgO + C -> Mg + CO
Decant the molten Mg while it is above 700 deg C
If the molten Magnesium comes in contact with oxygen or water at any stage you may very well end up miamed for life. Think about that very carefully
when you design the capsule and the decanting procedure.
|
Please don’t give advice to people about procedures you’ve never carried out yourself. The MgO-C method is possibly even more dangerous and
difficult to carry out in home lab circumstances, even more so by beginners.
This whole ‘let’s make some Mg at home’ lark is simply a nonsense.
The answer to 'Can Magnesium be extracted from epsom salt easily?' is a resounding 'NOOO'. It's pointless to encourage people to try and do the
impossible...
|
|
|
Mixell
Hazard to Others
 
Posts: 449
Registered: 27-12-2010
Member Is Offline
Mood: No Mood
|
|
I support blogfast, this procedure is quite dangerous and hard to achieve at laboratory conditions (not to mention in a home lab setup). One thing to
try to isolate very expensive and hard to get reagents/elements, but doing so for getting magnesium (which is cheap as crap in the USA and most of the
modern world) is pointless and even can be called stupid, risking your eyesight, your body and even your life for a thing that you can buy everywhere
is a something that should not be done.
|
|
|
Neil
National Hazard
  
Posts: 556
Registered: 19-3-2008
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by froot  |
Mix the MgO with carbon powder and heat it in a closed vented steel capsule to about 1000 Deg C.
|
Vented and closed?
The lit gives a temperature of 1800°C to 2000°C for this reduction at standard pressure. Or around 1200°C in a vacuum.
Magnesium can also be obtained free as sacrificial electrodes from water heaters, scrapped sacrificial anodes from ships/boats, transmission casings
from certain vehicles, if you live near a Pratt and Whitney plant or any other high tech manufacture they often produce large amounts of Mg Mg/Al and
Al scrap. Mg alloy tire rims are easily damaged and could be a possible source of large amounts of Mg.
|
|
|