Cl2 & carbon
does chlorine corrosive to carbon electrode ? if yes what is the corrosion products ?
|
|
plante1999
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1936
Registered: 27-12-2010
Member Is Offline
Mood: Mad as a hatter
|
|
not realy...
I never asked for this.
|
|
aeacfm
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 129
Registered: 24-7-2010
Member Is Offline
Mood: chem
|
|
what is the not really
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
aeactm:
Reactivity of any element towards any other is extremely dependent on conditions, mainly temperature, concentration and pressure. Put like you did
your question is more or less meaningless...
|
|
aeacfm
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 129
Registered: 24-7-2010
Member Is Offline
Mood: chem
|
|
ok , during electrolysis of brine (sodium chloride 3 %) using carbon electrodes i found in the anodic area particles like carbon ( great amount and c
electrode continued in producing these particles during electrolysis) i surprized as i know that c electrode is corrosion resistant ? so is this
corrosion or erosion or what?if so what is the corrosion products
|
|
plante1999
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1936
Registered: 27-12-2010
Member Is Offline
Mood: Mad as a hatter
|
|
ok now i could help you , no the carbon only get to fine powder , it doesn't react.
I never asked for this.
|
|
aeacfm
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 129
Registered: 24-7-2010
Member Is Offline
Mood: chem
|
|
C get to fine powder so this is erosion ! isnt it
|
|
ScienceSquirrel
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline
Mood: Dogs are pets but cats are little furry humans with four feet and self determination!
|
|
Sometimes undefined reactions can occur to form minor products with break up of the material.
Chemists like defined reactions with discrete reactants and products but things are not always like that.
|
|
LanthanumK
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 298
Registered: 20-5-2011
Location: New Jersey
Member Is Offline
Mood: No Mood
|
|
Every time I use carbon rods for electrolysis more than a few hours, they start eroding.
|
|
aeacfm
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 129
Registered: 24-7-2010
Member Is Offline
Mood: chem
|
|
in brine electrolysis it is only few minutes
|
|
IrC
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline
Mood: Discovering
|
|
I think consideration should be given to possible binders (if any) used to make a rod from the carbon. Clay is used as a binder to make a graphite rod
called a pencil as example. Depending upon your source of carbon rods I would think the possibility that the binder is being eroded should be
considered. I ran into this using rods scrapped from dead batteries once upon a time.
"Science is the belief in the ignorance of the experts" Richard Feynman
|
|
aeacfm
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 129
Registered: 24-7-2010
Member Is Offline
Mood: chem
|
|
i use the same source of carbon electrode , so not carbon it self it is only the binder which eroded
but for carbon electride with no binders will this erosion happen
|
|