Tungsten Compounds from W Electrodes
I have a couple of tungsten electrodes and have wondered about dissolving them to explore tungsten chemistry.
The search engine reveals little on the forum, and a (brief) search of my chemistry texts yields only that it is acid resistant and requires a fused
alkali with an oxidiser (KNO3?) to dissolve.
Is anyone aware of any interesting references, or other sources of practical information?
Potential hazards would also be useful information. I assume that being a heavy metal, it will be wise to be cautious about toxicity and disposal.
|
|
|
Intergalactic_Captain
Hazard to Others
 
Posts: 228
Registered: 4-9-2004
Location: somewhere where i don\'t know where i am
Member Is Offline
Mood: frabjous
|
|
If a search doesn't pull it up, I must not have posted it here - A while ago, I was interested in tungsten for tungstic acid for use in some odd
oxidation reaction. I've been going through my old stacks of journal articles recently, and I think I know where the refs are - If I find them I'll
post them for you... What I do remember is a reaction involving NaOH and H2O2 to form sodium tungstate, no specifics till I find the papers.
Are you interested in anything in particular? If you do a forum search for thorium compounds, you'll find quite a bit on working with tig rods.
Until my dad was layed off, I had almost unlimited access to used tig electrodes - only catch was I had no way to know which ones were thoriated and
which ones weren't...
If you see me running, try to keep up.
|
|
|
not_important
International Hazard
   
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
Not a lot of detail, but :
http://www.cleanroom.byu.edu/wet_etch.phtml (click on 'tungsten') sez 2 NH4OH : 1 H2O2
As I recall, 30% H2O2 at 40-55 C works, added alkali speeds it up a little and gets the W as more easily isolated tungstate
While proper disposal is always a good idea, tungsten and its compounds are not overly toxic. Toxicity in military applications has been related to
W-Ni_Co alloys, with dust being inhaled or bits being embedded into tissue; in these cases Ni has well established toxicity as does Co to a lesser
degree.
http://www.mod.uk/NR/rdonlyres/8062F2B1-6A9A-42F8-B819-17890...
|
|
|
bob800
Hazard to Others
 
Posts: 240
Registered: 28-7-2010
Member Is Offline
Mood: No Mood
|
|
There's a section in Experimenting with Chemistry, Experiments for the Home Lab by Burton Hawk on tungsten chemistry:http://books.google.com/ebooks/reader?id=RLUNAQAAIAAJ&pr... (page 55). It involves fusing the filaments with molten NaOH to produce sodium
tungstate (be extremely cautious if you attempt this, molten NaOH will eat through glass!). However, I think not_important's method would be safer.
|
|
|
ciscosdad
Hazard to Self

Posts: 76
Registered: 6-2-2007
Member Is Offline
Mood: Curious
|
|
Thanks for your responses.
The heads up on Thorium from W electrodes was instructive.
Any Journal References or other refernences would be appreciated as well.
My chemistry resources are limited. The simple electrolytic dissoltion may be all I can manage at least for the forseeable future. Maybe precipitate a
little thorium, just to say I've done it.
|
|
|
LanthanumK
Hazard to Others
 
Posts: 298
Registered: 20-5-2011
Location: New Jersey
Member Is Offline
Mood: No Mood
|
|
Just to obtain the oxide, place the filament in an enclosed space, such as a covered beaker. Attach mains voltage to each end. A brilliant flash
should be observed and there should be yellow smoke floating around. Wait for it to land on the walls of the beaker. This is anhydrous tungsten
trioxide. It is rather unreactive.
hibernating...
|
|
|
albqbrian
Hazard to Self

Posts: 73
Registered: 26-5-2011
Member Is Offline
Mood: Alternatingly paranoid or pi**ed
|
|
About the electrodes...
What are the basic dimensions of the W electrodes? Purity? Price?
Thanks???
|
|
|
LanthanumK
Hazard to Others
 
Posts: 298
Registered: 20-5-2011
Location: New Jersey
Member Is Offline
Mood: No Mood
|
|
Are they pure tungsten electrodes, thoriated tungsten, ceriated tungsten, or lanthanated tungsten?
hibernating...
|
|
|