What is this? (Pictures included)
A long time ago i got some pigment paint and separated the insoluble pigment from the actual paint, Now i look back at it and say to my self... what
is this? I remember looking over some wiki and somewhere i came across Barium Chromate or Strontium Chromate, both are yellow but im still unsure on
how to test it... i don't have overly that much and i dont want to waist it all doing tests when i want to make a youtube video about it if i know
what it is, is there some way to test what it actually is?

Im able to do very small scale if you have any idea's to what it is.
|
|
|
Teen Chemist
Harmless
Posts: 42
Registered: 27-4-2012
Member Is Offline
Mood: Effervescent
|
|
How about you try a flame test green for Barium red for Strontium.
|
|
|
Chemistry Alchemist
Hazard to Others
 
Posts: 403
Registered: 2-8-2011
Location: Australia
Member Is Offline
Mood: No Mood
|
|
Will that work with chromates?
|
|
|
Teen Chemist
Harmless
Posts: 42
Registered: 27-4-2012
Member Is Offline
Mood: Effervescent
|
|
Not sure but its worth a try seeing as it only needs a very small amount.
|
|
|
mineralman
Hazard to Self

Posts: 64
Registered: 15-6-2012
Location: WALES UK
Member Is Offline
Mood: complicated
|
|
Could also be zinc. I believe a flame test will work. I found this page and it shows what looks like a flame test in progress.
http://isearch.avg.com/images?s=sideNav&cid=%7b7F407966-...
http://isearch.avg.com/images?q=STRONTium+Chromate&sap=d...
http://www.indiamart.com/vapi-oxide-colour/anti-corrosive-pi... MM
|
|
|
TheChemINC
Hazard to Self

Posts: 61
Registered: 22-2-2012
Member Is Offline
Mood: fuming
|
|
in some paints they use cadmium salts for yellow color...
|
|
|
Yo-Yo
Harmless
Posts: 26
Registered: 27-5-2012
Member Is Offline
Mood: No Mood
|
|
I think it is iron ochre. Fe2O3. It is a common non-toxic yellow, red or black pigment.
I took a PhD in neuropharmacology and all I got was this bloody t-shirt.
|
|
|
woelen
Super Administrator
       
Posts: 8150
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
Add a pinch of it to hydrochloric acid and carefully sniff (!!). If it is CdS, then you will notice the smell of rotten eggs and the pigment dissolves
to a colorless solution.
Certain chromates also can be detected this way. E.g. zinc chromate or barium chromate give a yellow/orange solution in hydrochloric acid, but PbCrO4
does not (or only very slightly so), because of the immensely low solubility of PbCrO4.
|
|
|
Yo-Yo
Harmless
Posts: 26
Registered: 27-5-2012
Member Is Offline
Mood: No Mood
|
|
I think it is iron ochre. Fe2O3. It is a common non-toxic yellow, red or black pigment.
I took a PhD in neuropharmacology and all I got was this bloody t-shirt.
|
|
|
SM2
Hazard to Others
 
Posts: 359
Registered: 8-5-2012
Location: the Irish Springs
Member Is Offline
Mood: Affect
|
|
like woelen said, the basic tests are called for 1st. ESPECIALLY when, at the time this paint was made, it had to be inorganic, not withstanding. I
mean, it would probably be inorganic at any time it was made unless it was picric acid, or some horribly toxic hybrid. but that there does conger up
juicy stuff like picric or a nitro styrene.
Do what Yoyo suggests, and use some iron out or KMNO4 or some hydrosulphide - see if you get the sort of reduction you are looking for.
|
|
|