Powdered Graphite from pencils
I've recently come across a method of conductive paint through a mix of a glue / liquid tape and graphite powder. This interests me for a few DIY
applications, but I would first like a cheap source of graphite powder. Pencil lead is conductive, but mixed with clay. Could pencil lead be powdered,
put underwater to 'wash' the clay and others out of the mix, and leave behind only graphite?
Or is there a better method of conductive paint/glue?
Source: http://www.instructables.com/id/Conductive-Glue-And-Conducti...
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
watson.fawkes
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2793
Registered: 16-8-2008
Member Is Offline
Mood: No Mood
|
|
Hardware store, next to the other lubricants.
|
|
Diablo
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 113
Registered: 17-9-2011
Member Is Offline
Mood: Autodidactic
|
|
Also for a different conductive ink epoxy is mixed with copper powder that has been etched with an acid to remove non conductive oxides.
[Edited on 8-19-2012 by Diablo]
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
How does the copper-epoxy do, in terms of resistance?
Also, pencil lead would be a cheaper source of graphite than the lubricant section. I think.
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
barley81
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 481
Registered: 9-5-2011
Member Is Offline
Mood: No Mood
|
|
Graphite powder is not that expensive, if you need a lot of it:
http://www.ebay.com/itm/1-pound-Graphite-powder-fine-325-mes...
I don't think that clay can be easily separated from graphite in pencils. The wax binder can be removed with a suitable solvent, but the clay is a
problem.
Also, look here for something interesting:
firefox-fx.com/ChemC.htm
"Carbospheres - Conductive carbon - 22% -325 mesh - Stock #CCARB
Hollow microspheres, very light weight manufactured for a paint additive in radar absorbing coatings for the stealth aircraft. It is conductive and
can be used in conductive mixtures. Mixed with iron powders, it produces beautiful branching yellow sparks. Once this is gone, it's gone!! The
manufacturer is no longer in business."
$5.25/lb
|
|
Diablo
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 113
Registered: 17-9-2011
Member Is Offline
Mood: Autodidactic
|
|
I found the conductive epoxy via hackaday http://hackaday.com/2012/05/18/conductive-ink-circuit-experi... and the site it led to did not have much information, however i would think it
would be more conductive than a carbon based solution. Also for the graphit you could try the bricks of artists pencils which are conductive and
mostly carbon.
|
|
barbs09
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 113
Registered: 22-1-2009
Location: Australia
Member Is Offline
Mood: No Mood
|
|
How about this stuff. Liquid Chrome aerosol. Looks like it's loaded with metal and could conduct?
http://www.youtube.com/watch?v=qUc8QsLjS1s&feature=fvwre...
|
|
plante1999
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1936
Registered: 27-12-2010
Member Is Offline
Mood: Mad as a hatter
|
|
I already saw a conductive glue using epoxy and very fine copper powder. I don't know but you can make really fine copper powder by reduction of
copper sulphate with ascorbic acid to make copper I oxide. Then add diluted H2SO4 to make CuSO4 and Cu. It can also be made by reduction of CuSO4 sol.
with Zinc dust.
Cu2O + H2SO4 -) CuSO4 + H2O + Cu
I never asked for this.
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Nevermind, I learned how to make a circuitboard. Back to soldering!
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
barley81
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 481
Registered: 9-5-2011
Member Is Offline
Mood: No Mood
|
|
Nice! You probably knew this already, but a good cheap etchant can be made by mixing muriatic acid from the store with 3% hydrogen peroxide in a 1:3
ratio. I use this for my etching and it works quickly and doesn't stain like ferric chloride.
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Thanks for the info! How fast does this work, by the way?
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
Diablo
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 113
Registered: 17-9-2011
Member Is Offline
Mood: Autodidactic
|
|
Quite fast, and it's regeneratable.
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Would Sharpie work as a protector from the etchant?
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
Diablo
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 113
Registered: 17-9-2011
Member Is Offline
Mood: Autodidactic
|
|
I'm not sure but i believe it would, also an idea, if you have acetone, styrofoam, and a syringe youl could draw it on in polystyrene and clean the
board after etching.
[Edited on 8-27-2012 by Diablo]
|
|
watson.fawkes
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2793
Registered: 16-8-2008
Member Is Offline
Mood: No Mood
|
|
It can, but it's not very reliable. Enamel paint (for
model airplanes etc., also available in pens) or nail polish are both reliable.
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Got it, thanks.
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
morganism
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 105
Registered: 8-12-2012
Location: Az.
Member Is Offline
Mood: No Mood
|
|
conductive epoxy is used by aircraft mechanics, and has a limited shelf life. Can prob find it overdated cheap.
Latest conductive film is silver acetate on poly. Just saw it on PhysOrg 12/1/12
|
|
jock88
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 505
Registered: 13-12-2012
Member Is Offline
Mood: No Mood
|
|
Perhaps this:
http://www.ebay.co.uk/itm/REAR-WINDOW-DEMISTER-HEATER-REPAIR...
88
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
...
I literally can't tell what's going on here.
Attempted sockpuppeting? Joke?
Anyway, the problem I had was solved several weeks ago.
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
Texium
|
Thread Moved 20-11-2023 at 12:47 |