Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: titanium dioxide dielectric for HV capacitors
ElectroWin
Hazard to Others
***




Posts: 224
Registered: 5-3-2011
Member Is Offline

Mood: No Mood

[*] posted on 18-4-2013 at 14:26
titanium dioxide dielectric for HV capacitors


a friend asked me to help him build a Tesla coil; it seems i need a 25 kV, 2200 pF capacitor for this. i cannot afford the $200 price tag, so i got to thinking,....

could i make my own?

to be successful, i would have to sinter synthetic rutile powder, so i would need really high temperature. but what if i mixed like 80% TiO2 into some Al2O3 and/or SiO2 powders? would that reduce the sintering temperatures to manageable?
View user's profile View All Posts By User
Twospoons
International Hazard
*****




Posts: 1396
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline

Mood: A trace of hope...

[*] posted on 18-4-2013 at 20:05


The more usual dielectric would be polyethylene for home made capacitors. Its cheap, low dielectric loss, and readily available in sheet form. PET ('Mylar') sheet is often used too.




Helicopter: "helico" -> spiral, "pter" -> with wings
View user's profile View All Posts By User
Xenoid
National Hazard
****




Posts: 776
Registered: 14-6-2007
Location: Springs Junction, New Zealand
Member Is Offline

Mood: Comfortably Numb

[*] posted on 18-4-2013 at 20:10


Check out the various sellers on ebay - search for high voltage capacitors tesla doorknob. Suitable capacitors can be had for $5, $10, $20 or so, the normal procedure is to put several in parallel to increase capacitance or series for voltage, etc.

Do you really need 25KV, I would have thought 20KV at the most for NST based teslas.

I have a half-built tesla myself... must get around to finishing it!
View user's profile View All Posts By User
IrC
International Hazard
*****




Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline

Mood: Discovering

[*] posted on 19-4-2013 at 13:07


http://www.ebay.com/itm/0047uF-15KV-High-Voltage-Capacitor-H...

2 in series is very close at 2,350 pF and 30 KV in rating, all for a mere $13.80 shipped. $5.50 ea plus $2.50 + .30 for mailing. He has 7 of the .0047uF 15KV capacitors left.





"Science is the belief in the ignorance of the experts" Richard Feynman
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 19-4-2013 at 13:58


Film is easier than ceramic. Or glass, if you don't mind a lot of salt water around.



Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
AndersHoveland
Hazard to Other Members, due to repeated speculation and posting of untested highly dangerous procedures!
*****




Posts: 1986
Registered: 2-3-2011
Member Is Offline

Mood: No Mood

[*] posted on 19-4-2013 at 14:43


Capacitors are perhaps the easiest part of a Tesla coil to make yourself. You can use transparent projector film and sandwhich them with aluminum foil. Each layer can hold up to 15kV before breaking down.
http://en.wikipedia.org/wiki/Transparency_(projection)

I think they are usually made out of HD polyethylene, which has a dielectric constant of around 2

[Edited on 19-4-2013 by AndersHoveland]

[Edited on 19-4-2013 by AndersHoveland]
View user's profile Visit user's homepage View All Posts By User
franklyn
International Hazard
*****




Posts: 3026
Registered: 30-5-2006
Location: Da Big Apple
Member Is Offline

Mood: No Mood

[*] posted on 19-4-2013 at 21:19


www.youtube.com/watch?v=g1SN3rMTFok

www.youtube.com/watch?v=pdYJgnWe40s

www.youtube.com/watch?v=RUlAy-7AgC0

.
View user's profile View All Posts By User
ElectroWin
Hazard to Others
***




Posts: 224
Registered: 5-3-2011
Member Is Offline

Mood: No Mood

[*] posted on 20-4-2013 at 18:32


Quote: Originally posted by Twospoons  
The more usual dielectric would be polyethylene for home made capacitors. Its cheap, low dielectric loss, and readily available in sheet form. PET ('Mylar') sheet is often used too.


Polyethylene dielectric constant is 2.25, i need about 100.
View user's profile View All Posts By User
ElectroWin
Hazard to Others
***




Posts: 224
Registered: 5-3-2011
Member Is Offline

Mood: No Mood

[*] posted on 20-4-2013 at 19:24


Quote: Originally posted by franklyn  
www.youtube.com/watch?v=g1SN3rMTFok

www.youtube.com/watch?v=pdYJgnWe40s

www.youtube.com/watch?v=RUlAy-7AgC0

.


okay, the bucket cap may do just fine; in fact, we have the bucket and the bottles, a box of salt is $1, i'll strongly consider it.
View user's profile View All Posts By User
watson.fawkes
International Hazard
*****




Posts: 2793
Registered: 16-8-2008
Member Is Offline

Mood: No Mood

[*] posted on 20-4-2013 at 19:28


Quote: Originally posted by ElectroWin  
Polyethylene dielectric constant is 2.25, i need about 100.
Where does this "need" come from? You can just use larger plates as a substitute. Now "want" I can relate to, but unless you're going to get serious about technical ceramics, I don't see using barium titanate as a short path to finishing a coil project.
View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1752
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 20-4-2013 at 21:01


Teflon has some good qualities.
View user's profile View All Posts By User
ElectroWin
Hazard to Others
***




Posts: 224
Registered: 5-3-2011
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2013 at 09:21


Quote: Originally posted by watson.fawkes  
Quote: Originally posted by ElectroWin  
Polyethylene dielectric constant is 2.25, i need about 100.
Where does this "need" come from? You can just use larger plates as a substitute. [...]

ok, i just realized that if my chosen dielectric has much-greater dielectric strength than air, i can substitute high dielectric constant for thinner plates. (ie: i should be comparing the product of the dielectric strength and dielectric constant, when choosing the capacitors)

also, though i seriously do want to get to creating my own ceramic capacitors, those turn out to be deprecated for tesla coils by geek group, who says they tend to crack under mechanical stresses.

the bucket capacitor, described in the geek group video, looks like the cheapest.

thanks
View user's profile View All Posts By User
watson.fawkes
International Hazard
*****




Posts: 2793
Registered: 16-8-2008
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2013 at 11:20


Quote: Originally posted by ElectroWin  
also, though i seriously do want to get to creating my own ceramic capacitors, those turn out to be deprecated for tesla coils by geek group, who says they tend to crack under mechanical stresses.
Mechanical stress isn't trivial in oscillating high voltage. It the main reason that the DC rating for HV capacitors is five times or more higher than the AC rating on the same unit.

To be precise, it's not the mechanical stress that's actually the problem, it's the strain, which is to say it's not the force but the the motion. You can get rid of the motion by prestressing the capacitor stack by clamping it down. Commercial capacitors don't (as a rule) have such clamps but rather use alternate means to provide the pre-stress.
View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1752
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2013 at 12:01


I know this is primitive, but just a little salt water in an LDPE bottle held this nice little spark I made simply by rubbing a paper towel over a piece of PVC tubing. Salt water makes a decent capacitor. Under it is a piece of 1/8 inch thick PTFE. On top of the poly bottle is a stainless steel water bottle for the electrode. Probably not the design you are going for but I was really impressed by the simplicity.
Here's some tidbit I came across.
http://www.pupman.com/listarchives/1998/October/msg00790.htm...

33 Centimeters 13 Inches.JPG - 81kB
View user's profile View All Posts By User
Twospoons
International Hazard
*****




Posts: 1396
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline

Mood: A trace of hope...

[*] posted on 23-4-2013 at 14:47


have you been here : http://4hv.org/e107_plugins/forum/forum.php
Wealth of information, very helpful members.

Film (PE or PET) + Al foil, rolled and submerged in oil, is generally regarded as a good mix of low cost, simplicity and robustness.

[Edited on 23-4-2013 by Twospoons]




Helicopter: "helico" -> spiral, "pter" -> with wings
View user's profile View All Posts By User

  Go To Top