Author: Subject: Yellow stain on glassware
TheChemiKid
Hazard to Others
***




Posts: 493
Registered: 5-8-2013
Location: ̿̿ ̿̿ ̿'̿'̵͇̿̿з=༼ ▀̿̿Ĺ̯̿̿▀̿ ̿ ༽
Member Is Offline

Mood: No Mood

[*] posted on 29-12-2013 at 03:54
Yellow stain on glassware


I bought a second hand chemglass reflux condenser a while ago. When it arrived, it had a yellow stain on the inside of the cooling coil.
Even though this is on the inside of the coil and doesn't effect its usability at all (It works amazingly), I was wondering what this was caused by, whether it could be removed (I know cleaning things is already a thread, but since I don't know what this is, I don't know how to clean it), and whether it is a problem or not.

PS: Would it be possible for the cleaning method to not be caustic or toxic?

I will be posting pictures soon.




When the police come


\( * O * )/ ̿̿ ̿̿ ̿'̿'̵͇̿̿з=༼ ▀̿̿Ĺ̯̿̿▀̿ ̿ ༽
View user's profile View All Posts By User
papaya
National Hazard
****




Posts: 615
Registered: 4-4-2013
Member Is Offline

Mood: reactive

[*] posted on 29-12-2013 at 04:01


Obviously a rust.
View user's profile View All Posts By User
TheChemiKid
Hazard to Others
***




Posts: 493
Registered: 5-8-2013
Location: ̿̿ ̿̿ ̿'̿'̵͇̿̿з=༼ ▀̿̿Ĺ̯̿̿▀̿ ̿ ༽
Member Is Offline

Mood: No Mood

[*] posted on 29-12-2013 at 04:05


Why would that be?



When the police come


\( * O * )/ ̿̿ ̿̿ ̿'̿'̵͇̿̿з=༼ ▀̿̿Ĺ̯̿̿▀̿ ̿ ༽
View user's profile View All Posts By User
bahamuth
Hazard to Others
***




Posts: 384
Registered: 3-11-2009
Location: Norway
Member Is Offline

Mood: Under stimulated

[*] posted on 29-12-2013 at 04:43


It is simply minerals deposited from the water that has passed through it.

You might be able to remove it with dilute hydrochloric or nitric acid, but me I'd just whip up some aqua regia and let the whole thing soak in it for a day or two. I like my glass spotless, and as such a KOH/ethanol wash would follow the aqua regia soak...

Acetic acid or citric acid might remove the stain too, but I suspect a prolonged soak would be needed, even boiling perhaps..




Any sufficiently advanced technology is indistinguishable from magic.
View user's profile View All Posts By User
TheChemiKid
Hazard to Others
***




Posts: 493
Registered: 5-8-2013
Location: ̿̿ ̿̿ ̿'̿'̵͇̿̿з=༼ ▀̿̿Ĺ̯̿̿▀̿ ̿ ༽
Member Is Offline

Mood: No Mood

[*] posted on 29-12-2013 at 04:47


Thank you, I will try different methods and say how they perform.



When the police come


\( * O * )/ ̿̿ ̿̿ ̿'̿'̵͇̿̿з=༼ ▀̿̿Ĺ̯̿̿▀̿ ̿ ༽
View user's profile View All Posts By User
Random
International Hazard
*****




Posts: 1120
Registered: 7-5-2010
Location: In ur closet
Member Is Offline

Mood: Energetic

[*] posted on 29-12-2013 at 08:21


Iron stains are very hard to remove from glassware. If it doesn't get removed by HCl you might want to try aqua regia.
View user's profile View All Posts By User
Sublimatus
Hazard to Others
***




Posts: 108
Registered: 8-6-2011
Member Is Offline

Mood: No Mood

[*] posted on 29-12-2013 at 10:22


You might try a mix of dilute hydrochloric acid and hydrogen peroxide. That mixture removes many otherwise tenacious stains, in my experience, and is a lot safer than aqua regia.
View user's profile View All Posts By User
Zephyr
Hazard to Others
***




Posts: 341
Registered: 30-8-2013
Location: Seattle, WA
Member Is Offline


[*] posted on 29-12-2013 at 10:42


I usually clean rust off of my glassware buy soaking the dirty equipment in a hot solution of oxalic acid. This method has the perks of being efficient as well as non toxic.



Sciencemadness Patches for sale! U2U me if you are interested.
http://imgur.com/a/QmpHn http://www.sciencemadness.org/talk/viewthread.php?tid=62566&...
View user's profile View All Posts By User
Pyro
International Hazard
*****




Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline

Mood: No Mood

[*] posted on 29-12-2013 at 11:32


I acquired a lot of condensers that all had yellow stains in them, I found HCl to be of limited use. Chromic acid cleaned it right up though, and I prefer chromic acid as it doesn't fume like HCl and HNO3!



all above information is intellectual property of Pyro. :D
View user's profile View All Posts By User
Metacelsus
International Hazard
*****




Posts: 2554
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 29-12-2013 at 15:48


For really dirty glassware, I usually use saturated sodium chlorate solution and 31% hydrochloric acid. The chloric acid/chlorine oxides produced will oxidize away all the dirt. (It's like chromic acid, but no heavy metals.) Fumes, however, are a problem, so I do it outside.

Don't try using concentrated sulfuric acid instead of the hydrochloric acid. I did, and I'm lucky the resulting explosion didn't crack my glassware.

[Edited on 29-12-2013 by Cheddite Cheese]




As below, so above.

My blog: https://denovo.substack.com
View user's profile View All Posts By User
Pyro
International Hazard
*****




Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline

Mood: No Mood

[*] posted on 29-12-2013 at 18:52


thats true, but I hate HCl fumes!

have you tried that mix on orgo crap left over from distillation? those terrible tars that stick to everything.




all above information is intellectual property of Pyro. :D
View user's profile View All Posts By User
Metacelsus
International Hazard
*****




Posts: 2554
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 29-12-2013 at 19:14


Actually, I first tried it on tar (aldol condensation crap impurities) left over from distilling crude chloroacetone. After a soak overnight, it came right off.



As below, so above.

My blog: https://denovo.substack.com
View user's profile View All Posts By User
Pyro
International Hazard
*****




Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline

Mood: No Mood

[*] posted on 29-12-2013 at 19:30


it takes all night? well, I guess I'm just lazy (must be why my lab is so damn tidy :))




all above information is intellectual property of Pyro. :D
View user's profile View All Posts By User
macckone
Dispenser of practical lab wisdom
*****




Posts: 2211
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 29-12-2013 at 19:33


Quote: Originally posted by Pinkhippo11  
I usually clean rust off of my glassware buy soaking the dirty equipment in a hot solution of oxalic acid. This method has the perks of being efficient as well as non toxic.


Oxalic acid is actually toxic to humans.
More so than HCl.
However it is a very good cleaner for rust stains and
is sold for that purpose.
View user's profile View All Posts By User
Eddygp
National Hazard
****




Posts: 858
Registered: 31-3-2012
Location: University of York, UK
Member Is Offline

Mood: Organometallic

[*] posted on 30-12-2013 at 10:07


If it is iron, oxalic acid is usually your best bet. I remember watching a video in YouTube some months ago about cleaning rust... check it in case it's there.



there may be bugs in gfind

[ˌɛdidʒiˈpiː] IPA pronunciation for my Username
View user's profile View All Posts By User
Brain&Force
Hazard to Lanthanides
*****




Posts: 1302
Registered: 13-11-2013
Location: UW-Madison
Member Is Offline

Mood: Incommensurately modulated

[*] posted on 30-12-2013 at 11:03


I've never tried this, but if you can get ahold of EDTA, that may work to chelate the iron away. Acidic citrates also work, they're probably the least toxic solution.

There's also stuff called naval jelly, it's mostly phosphoric acid. It seems to work pretty well, as does ammonium dihydrogen phosphate.




At the end of the day, simulating atoms doesn't beat working with the real things...
View user's profile View All Posts By User
Zephyr
Hazard to Others
***




Posts: 341
Registered: 30-8-2013
Location: Seattle, WA
Member Is Offline


[*] posted on 30-12-2013 at 11:27


Quote: Originally posted by macckone  

Oxalic acid is actually toxic to humans.
More so than HCl.
However it is a very good cleaner for rust stains and
is sold for that purpose.


Yes you are right, isn't the oxalic acid in rhubarb leaves that make them poisonous?
I think this is the video you were thinking about Eddygp?




Sciencemadness Patches for sale! U2U me if you are interested.
http://imgur.com/a/QmpHn http://www.sciencemadness.org/talk/viewthread.php?tid=62566&...
View user's profile View All Posts By User
macckone
Dispenser of practical lab wisdom
*****




Posts: 2211
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 30-12-2013 at 14:44


Quote: Originally posted by Pinkhippo11  

Yes you are right, isn't the oxalic acid in rhubarb leaves that make them poisonous?


Yes and it is a cumulative toxin.
If forms kidney stones which in sufficient quantity cause
the kidneys to shut down.
Spinach also contains oxalic acid but it binds with
calcium also found in spinach to prevent it from being
absorbed. You have to eat pounds of rhubarb
to actually poison yourself. Antifreeze (ethylene glycol)
is converted to oxalic acid which makes it toxic.

http://helios.hampshire.edu/~nlNS/mompdfs/oxalicacid.pdf


View user's profile View All Posts By User
bahamuth
Hazard to Others
***




Posts: 384
Registered: 3-11-2009
Location: Norway
Member Is Offline

Mood: Under stimulated

[*] posted on 30-12-2013 at 18:20


While on the subject of oxalic acid toxicity.
My uncle almost died as a kid from rhubarb wine (which he stole from my grandfather) that had not been "calcified", in other words added a soluble calcium salt, most likely Ca(OH)2

I have no idea what they did to save him though...




Any sufficiently advanced technology is indistinguishable from magic.
View user's profile View All Posts By User
macckone
Dispenser of practical lab wisdom
*****




Posts: 2211
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 30-12-2013 at 23:56


Quote: Originally posted by bahamuth  
While on the subject of oxalic acid toxicity.
My uncle almost died as a kid from rhubarb wine (which he stole from my grandfather) that had not been "calcified", in other words added a soluble calcium salt, most likely Ca(OH)2

I have no idea what they did to save him though...


Probably pumped his stomach, balanced his blood ph and calcium levels with fluids

Most poisoning is not fatal but does lead to kidney stones.
View user's profile View All Posts By User
Fantasma4500
International Hazard
*****




Posts: 1682
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline

Mood: dangerously practical

[*] posted on 31-12-2013 at 04:45


i found it that Fe3O4 reacted very well with concentrated citric acid + H2O2
as i heated it it gave off a nearly explosive decomposition
the Fe3O4 was 'beach magnetite' and some of might be iron aswell

but ofcourse, the more dangerous the chemical is, the more reactive it is, so the more dangerous stuff you use for it, the bigger the chances are it will get rid of it (:




~25 drops = 1mL @dH2O viscocity - STP
Truth is ever growing - but without context theres barely any such.

https://en.wikipedia.org/wiki/Solubility_table
http://www.trimen.pl/witek/calculators/stezenia.html
View user's profile View All Posts By User
Arthur Dent
National Hazard
****




Posts: 553
Registered: 22-10-2010
Member Is Offline

Mood: entropic

[*] posted on 1-1-2014 at 13:41


THe idea of oxalic acid is interesting, although this chemical is pretty hard to find at reasonable prices in my neighborhood.

As for the HCl + bleach solution, it is indeed very efficient to remove most ferrous stains, but to my dismay, it also destroyed the company logo off of my expensive Ace Glass Soxhlet... The red logo turned dark brown, and while washing with soapy water and a brush, just disappeared! :mad: I thought that such a prestigious labware maker would make their logo a wee bit more resistant to mineral acids.

LOL

Robert





--- Art is making something out of nothing and selling it. - Frank Zappa ---
View user's profile View All Posts By User
macckone
Dispenser of practical lab wisdom
*****




Posts: 2211
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 1-1-2014 at 19:05


Bar Keepers friend contains Oxalic acid as well as other scrubbing agents. There are also sulfamic acid cleaners (ZEP CLR for one). And of course the good old cheap standby of vinegar and hydrogen peroxide. One of the sulfamic acid cleaners may be better as they
are specifically formulated to remove rust stains from ceramics.