Construction of a steel laboratory spatula.



Introduction.

Laboratory spatulas are useful instrument in any scientific setting. They are an excellent tool for transferring small quantities of reagents, scratching the sides of a flask to induce crystallisation and can be used as a platform for the deflagration of small amounts of pyrotechnic mixtures. Although cheap, finding high quality lab spatulas can, for some, be difficult and often through international sources, which entails shipping rates etc. This report will demonstrate the simplicity of designing and building one's own spatula for minimum costs at home.

Purpose

To built a laboratory spatula with minimum funds.

Materials

- 2 mm steel wire (free)
- butane torch (already had)
- hammer (already had)
- hard steel surface [anvil or bench vice] (already had)
- file(already had)
- sand paper, steel wool and or sanding sponge (already had)
- safety glasses and heavy duty gloves (already had)

Safety considerations

Because steel will be heated to high temperatures, caution must be used when handling the hot material. Keep a burn relief kit nearby and wear safety giggles and heavy duty gloves to protect from burns. Do this in a well ventillated area!

Procedure

1.Measure out about 18.5 cm of the steel wire.
Pic 1.jpg - 80kB

2. Begin heating with the torch until you obtain a cherry red, then begin hammering and flattening out the end of the wire (until roughly ~2 cm has been flattened)
pic 2.jpg - 71kB pic 3.jpg - 97kB
3.A technique known as "hot filing" maybe implemented to shape the spatula. Heat the end and start filling. Use caution. It is useful to thin out the spatula a little at this point.
pic 5.jpg - 96kB

4.Once the final shape has been achieved, heat the end of the spatula and quench it to harden the tip.
pic 4.jpg - 91kB

5.Repeat steps 1-4 for the other side with the desired shape.

6.Once hardened, the work up of the spatula may begin. use rough sand paper, then go to a finer grade and finish with a sanding block.
pic 7.jpg - 85kB

Discussion

The spatula came out with very satisfactory results. The main limitations of the spatula is that it is not stainless steel, hence it is mainly useful for only rough qualitative work and reactions that will not react with iron. It is also important to wash the spatula after every use and to dry it well to prevent corrosion.

Conclusion

The main goal of the procedure was achieved without major complication.



IMG_1782.jpg - 2.1MB IMG_1781.jpg - 2.3MB
View user's profile View All Posts By User
Chemosynthesis
International Hazard
*****




Posts: 1071
Registered: 26-9-2013
Member Is Offline

Mood: No Mood

[*] posted on 20-7-2014 at 03:46


Nicely done.
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 20-7-2014 at 10:09


I find that my 3 different shaped ss spatulas are among my most useful lab tools.

I have a 2mm diameter ss welding rod that has proved very handy at times also. I made a spiral in one end to remove packing from a narrow column, and a small loop in the other end for some use I can't now recall.

Maybe you could get a friend who does welding to give you a ss welding rod to make ss spatulas.




The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
HeYBrO
Hazard to Others
***




Posts: 290
Registered: 6-12-2013
Location: 'straya
Member Is Offline

Mood: :)

[*] posted on 20-7-2014 at 14:26


Quote: Originally posted by Magpie  
I find that my 3 different shaped ss spatulas are among my most useful lab tools.

I too have three, a micro wedge style, a round spatula with red handle and another one similar to what i made.

Quote: Originally posted by Magpie  
I have a 2mm diameter ss welding rod that has proved very handy at times also. I made a spiral in one end to remove packing from a narrow column, and a small loop in the other end for some use I can't now recall.

Maybe you could get a friend who does welding to give you a ss welding rod to make ss spatulas.
perhaps it was for hanging the tool up? That's a good idea, I'll see what I can do!

Quote: Originally posted by Chemosynthesis  
Nicely done.

Thanks!
View user's profile View All Posts By User
Pyro
International Hazard
*****




Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline

Mood: No Mood

[*] posted on 22-7-2014 at 05:53


niceley done!
one should try this with a nickel rod. nickel spatulas cost a furtune


[Edited on 22-7-2014 by Pyro]




all above information is intellectual property of Pyro. :D
View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1750
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 22-7-2014 at 09:33


Why is it realitively pure nickel coins from Canada are so cheap but a simple nickel rod on Amazon or ebay tremendously expensive?
http://www.vincentmetals.com/Daily_Nickel_Prices.html

[Edited on 22-7-2014 by Morgan]
View user's profile View All Posts By User
Pyro
International Hazard
*****




Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline

Mood: No Mood

[*] posted on 22-7-2014 at 09:52


id use this:
http://www.ebay.com/itm/10ft-Jewelry-Making-German-Nickel-Si...

might be a fun project to try to make one from a quarter

BTW:why rubber gloves when working with hot metal?

[Edited on 22-7-2014 by Pyro]




all above information is intellectual property of Pyro. :D
View user's profile View All Posts By User
Manifest
Script Kiddie Asshole
***




Posts: 229
Registered: 7-12-2012
Member Is Offline

Mood: No Mood

[*] posted on 22-7-2014 at 12:56


Nice post!
View user's profile Visit user's homepage View All Posts By User
HeYBrO
Hazard to Others
***




Posts: 290
Registered: 6-12-2013
Location: 'straya
Member Is Offline

Mood: :)

[*] posted on 22-7-2014 at 13:25


Quote: Originally posted by Pyro  

BTW:why rubber gloves when working with hot metal?

[Edited on 22-7-2014 by Pyro]


I was doing something else in the lab before and i forgot to take them off... I know, i know, look at me, the hypocrite :P
View user's profile View All Posts By User
chemrox
International Hazard
*****




Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline

Mood: LaGrangian

[*] posted on 22-7-2014 at 13:33


Why would you do this? I appreciate tinkering but those rulers are worth a lot more than micro spatulas that you can by all day on ebay.



"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
View user's profile View All Posts By User
HeYBrO
Hazard to Others
***




Posts: 290
Registered: 6-12-2013
Location: 'straya
Member Is Offline

Mood: :)

[*] posted on 22-7-2014 at 13:55


Quote: Originally posted by chemrox  
Why would you do this? I appreciate tinkering but those rulers are worth a lot more than micro spatulas that you can by all day on ebay.


thanks for the response.

Firstly, I'm a litte confused by your somewhat contradictory statement and question; if you appreciate it why do you choose to point out "flaws"?

Secondly, if you re-read my original post more carefully you would see the answer to your question:

Quote: Originally posted by HeYBrO  

Introduction.
Although cheap, finding high quality lab spatulas can, for some, be difficult and often through international sources, which entails shipping rates etc. This report will demonstrate the simplicity of designing and building one's own spatula for minimum costs at home.


Besides that, this is just a nice thread to spark ideas such building from different materials etc. This project was free and took less than two hours, I would have to wait two weeks if I bought it online. Why do you have to justify building something so useful and simple if the means for doing so are at your disposal? Surely that is the spirit of amateur chemistry?
View user's profile View All Posts By User
Manifest
Script Kiddie Asshole
***




Posts: 229
Registered: 7-12-2012
Member Is Offline

Mood: No Mood

[*] posted on 22-7-2014 at 14:32


I agree, you shouldn't be asking why, but why not.
This post fits the quality we should all be aiming to post and fits within the theme of amateur chemistry.
View user's profile Visit user's homepage View All Posts By User
MrHomeScientist
International Hazard
*****




Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline

Mood: No Mood

[*] posted on 24-7-2014 at 11:23


Quote: Originally posted by HeYBrO  

Keep a burn relief kit nearby and wear safety giggles and heavy duty gloves to protect from burns.

Sometimes I get the safety giggles too :)

Kidding aside this is a pretty neat idea. Looks like it turned out well! I'd be interested to see how long it lasts before corroding. With careful care and cleaning it should do pretty well.

It sounds like chemrox thought you hammered the ruler into a spatula? It was a metal wire that was used - the ruler was just there to measure, as they usually are.
View user's profile Visit user's homepage View All Posts By User
UnintentionalChaos
International Hazard
*****




Posts: 1454
Registered: 9-12-2006
Location: Mars
Member Is Offline

Mood: Nucleophilic

[*] posted on 24-7-2014 at 12:00


If you can get nickel wire/rod, you could make quite a few of these. Stainless won't work too well. The heating tends to ruin the corrosion-resistance.



Department of Redundancy Department - Now with paperwork!

'In organic synthesis, we call decomposition products "crap", however this is not a IUPAC approved nomenclature.' -Nicodem
View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1750
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 24-7-2014 at 12:28


If anyone knows a relatively low-cost source for pure nickel rod that would be nice. Nickel is starting to approach 9 dollars a pound but rods of it seem to cost quite a bit more.
View user's profile View All Posts By User
Metacelsus
International Hazard
*****




Posts: 2554
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 24-7-2014 at 12:34


I have 2 nickel rods (somewhere, I hope I can find them), and a heat source. I'm going to try making a nickel spatula right now!

Update: Well, I ran the induction heater at 48 volts, the nickel started glowing, I took it out and hammered on it, put it back in, and then one of my MOSFETs had a critical existence failure (aka magic smoke).

Now I have a slightly more pointy nickel rod!

[Edited on 24-7-2014 by Cheddite Cheese]




As below, so above.

My blog: https://denovo.substack.com
View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1750
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 25-7-2014 at 14:05


I suppose the train lines would frown on this but if you affixed a small piece of wire to the track with a spot of super glue or used a 1981 or older Canadian nickel which is 99.9 % nickel it would form the metal to some extent. Maybe one could join a flattened nickel to a nickel rod, making a large pure nickel spatula spoon.

1964–1981 4.54 g 21.21 mm, round 99.9% nickel
http://en.wikipedia.org/wiki/Nickel_(Canadian_coin)

Coins on the Track
https://www.youtube.com/watch?v=VitmL070-vQ
http://www.capecentralhigh.com/perry-county/coins-on-the-tra...

Here's a pretty shape.
http://www.instructables.com/id/Teardrop-Pendant/?ALLSTEPS
View user's profile View All Posts By User
aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 25-7-2014 at 14:54


Excellent !
Very well done, and nice photos.

There needs to be much more of this - actually making stuff, and using some imagination.

Ignore chemrox - clearly read very little of your post and just saw a word or two and a picture.

If you manage to get some Stainless rod, just try hitting it with a hammer a lot.

Allow it a little Time between sessions and you might find it works, albeit slowly.




View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1750
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 27-7-2014 at 10:53


This shine is fairly impressive for an ordinary nickel. I wonder how a Canadian 99.9% nickel would do? If it polished up as well, it would be possible to make a reflective spoon shape of some sort that could be attached to a rod for an artistic scoop-like spatula at one end.

How to polish, in real time
https://www.youtube.com/watch?v=n3Mc4NkCeo0

http://orgchem.colorado.edu/Technique/Equipment/Benchequip/S...
http://www.ajaxscientific.com/wp-content/uploads/2012/08/Lab...
http://strauchfiber.typepad.com/the-wool-goes-round/2010/02/...
View user's profile View All Posts By User

  Go To Top