| Pages:
1
2 |
golfpro
Banned
Posts: 179
Registered: 18-5-2013
Member Is Offline
Mood: Cap Sensitive
|
|
Detonator Casings
So I am trying to have caps that are as reliable, safe, and storage stable as possible. I have the materials to make an industry grade blast cap
(maybe not quiet), but I don't want the casing to just be drinking straw, and risk friction and other issues. Has anyone found a way to make a nice
uniform Al tube/case w/ thin walls for caps?
[Edited on 23-9-2013 by golfpro]
|
|
|
Bot0nist
International Hazard
   
Posts: 1559
Registered: 15-2-2011
Location: Right behind you.
Member Is Offline
Mood: Streching my cotyledons.
|
|
Aluminum arrow shafts are where its at. Brittle and consistent... Cut off sharpie marker backs too, or small HDPE test tubes if plastic is desired.
Drinking straws are a terrible idea, in my opinion. Much too flexible and elastic. Accident waiting to happen.
Play safe.
U.T.F.S.E. and learn the joys of autodidacticism!
Don't judge each day only by the harvest you reap, but also by the seeds you sow.
|
|
|
confused
Hazard to Others
 
Posts: 244
Registered: 17-3-2013
Location: Singapore
Member Is Offline
Mood: tired
|
|
being an archer myself, the thought of cutting my arrow shafts makes me cringe, anyway arrow shafts are expensive, why not use the cylinder of cheap
ballpoint pens?
|
|
|
Microtek
National Hazard
  
Posts: 982
Registered: 23-9-2002
Member Is Offline
Mood: No Mood
|
|
Buy a small lathe. Use it to bore an aluminum (or steel) rod to the desired dimensions. Then use it for producing rocket nozzles, or as a starting
point for a great new hobby that complements HEs nicely. Once you get some PTFE rod, you can make your own lab-ware without the glass-blowing.
|
|
|
Bot0nist
International Hazard
   
Posts: 1559
Registered: 15-2-2011
Location: Right behind you.
Member Is Offline
Mood: Streching my cotyledons.
|
|
Brittle metal is usually desired over plastics so that the cap doesnt "balloon" out at the moment of initiation and create a seperation from the
secondary. Metal arrows are not that cheap, but much much better than plastic pen cases. A single arrow would make many small caps I bet.
[Edited on 23-9-2013 by Bot0nist]
U.T.F.S.E. and learn the joys of autodidacticism!
Don't judge each day only by the harvest you reap, but also by the seeds you sow.
|
|
|
bfesser
Resident Wikipedian
   
Posts: 2114
Registered: 29-1-2008
Member Is Offline
Mood: No Mood
|
|
Can't you purchase short lengths/diameters of suitable aluminum, brass, steel, and stainless steel tubing from hobby supply shops (or hardware
stores)?
[edit] Admittedly, it can be expensive, but so is burning/exploding all of your chemicals.
[Edited on 23.9.13 by bfesser]
|
|
|
Fantasma4500
International Hazard
   
Posts: 1682
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline
Mood: dangerously practical
|
|
well i think bfesser of what ive seen the tubes are too thick, what would be desired would be like a permanent marker casing, in which ive heard being
used.. perhaps some stores or some online buy a tonne
of what ive seen theyre usually aluminium
otherwise guys
go buy yourself some aluminium foil tape, the thick kind..
you can then wrap this tightly around a straw and cut it however you want to, it should be possible to put on more layers to furthermore harden the
external casing..
|
|
|
golfpro
Banned
Posts: 179
Registered: 18-5-2013
Member Is Offline
Mood: Cap Sensitive
|
|
I'll look in the hobby store tomorrow for something like that, but right now I have good sized cases, but they are plastic, I'd like to get an
industry identical, but IMO, straw makes for good reliable initiation, but doesn't protect the materials inside very well.
|
|
|
Mathias94
Harmless
Posts: 41
Registered: 3-11-2012
Member Is Offline
Mood: No Mood
|
|
I don't know what your primary of choice is, but remember that mercury fulminate and probably a lot of other primaries is uncompatible with aluminium.
|
|
|
Mathias94
Harmless
Posts: 41
Registered: 3-11-2012
Member Is Offline
Mood: No Mood
|
|
EDIT: Double post, a moderator may delete this 
[Edited on 24-9-2013 by Mathias94]
|
|
|
Ral123
National Hazard
  
Posts: 735
Registered: 31-12-2011
Member Is Offline
Mood: No Mood
|
|
Copper for fulminate, Al for azide or I messed this one up badly?
|
|
|
Pulverulescent
National Hazard
  
Posts: 793
Registered: 31-1-2008
Member Is Offline
Mood: Torn between two monikers ─ "hissingnoise" and the present incarnation!
|
|
Quote: Originally posted by Mathias94  | | I don't know what your primary of choice is, but remember that mercury fulminate and probably a lot of other primaries is uncompatible with aluminium.
|
HMTD, the most useful of the organic peroxides, should not be used with any metal other than aluminium . . .
"I know not with what weapons World War III will be fought, but World War IV will be fought with sticks and stones"
A Einstein
|
|
|
golfpro
Banned
Posts: 179
Registered: 18-5-2013
Member Is Offline
Mood: Cap Sensitive
|
|
SADS works well with aluminum casing.
|
|
|
Gargamel
Hazard to Others
 
Posts: 166
Registered: 9-3-2013
Member Is Offline
Mood: No Mood
|
|
I wonder how SADS reacts to static discharge in such an aluminium cap. I only work with visco fuse.
I wonder if the fuse, that contains (somehow conductive???) charcoal but is isolated on the outside, like a coaxcable, can create a breach in the
faraday cage?
Also it leads directly to the primary, so any incoming current would have to pass the primary...
These things seem so simple, but are so complicated in detail, I'm a bit worried if this can ever be handled by hobby guys like us. IMHO such a cap
must be safe to be handled once closed.
I would assume that an aluminium cap is mechanically save as long as you don't drop a big stone on it. The only thing that remains is static,
especially with SADS...
|
|
|
Endo
Hazard to Others
 
Posts: 124
Registered: 5-1-2006
Location: USA
Member Is Offline
Mood: Cold
|
|
Befriend someone who works at a bow-shop. The typical process with a new arrow shaft is to trim them to length for the archer using them. The scrap
typically goes into a drum for recycling.
|
|
|
CaliusOptimus
Hazard to Self

Posts: 96
Registered: 10-6-2011
Member Is Offline
Mood: Subjectively Objective
|
|
0.253" ID x 9/32" OD aluminum 3003 tubing is imo a perfect choice for caps. It is soft enough to form, but strong enough to handle around 5000psi
during pressing. Lots of hobby shops and hardware stores have it in 1' lengths and mcmaster has it in 1' or 6'. It's cheap to boot.
|
|
|
dangerous amateur
Hazard to Others
 
Posts: 148
Registered: 8-7-2011
Member Is Offline
Mood: No Mood
|
|
Blasting cap from paper
Hi guys,
i just thought about using paper tubes for blasting caps.
I have some pyro related spolette tubes, they are 7mm on the inside and little more than 9,4mm on the outside. Wall thickness is about 1,2mm.
I figured that these will give at least some protection for a primary while handling the cap, and no dangerous shrapnel. On the other hand, there is a
zone of rather low density (compared to Al) paper between the caps booster and the secondary.
I'm not sure if paper is good or bad concerning ESD. But I read suggestions about how to package semiconductors, and I remember somehow that "paper is
not too bad, also it always accumulates some moisture"
How do you feel about using paper, looking at perfomance and safety?
|
|
|
greenlight
National Hazard
  
Posts: 790
Registered: 3-11-2014
Member Is Offline
Mood: Energetic
|
|
Al tubing for model plane construction from hobby shops is perfect for dets.
I successfully used soft drink can aluminum when i have run out of tube though as it is quite thin.
Cut the top and bottom off an empty soft drink can and cut a small rectangle from whats left. Roll it tight round a small pen or dowel and tape.
Once forcefully rolled a couple times you can get a very small tube from it.
Then push a small paper tissue plug through with the dowel to act as an end cap and fill with primary, place a fuse with some more tissue around it
and tape the top. Insert into explosive when ready.
|
|
|
Hawkguy
Hazard to Others
 
Posts: 326
Registered: 10-10-2014
Location: British Columbia (Canada eh!)
Member Is Offline
Mood: Body is Ready
|
|
Try using tent poles, bought for spares. Most are dreadfully thick, but some might work...
|
|
|
roXefeller
Hazard to Others
 
Posts: 463
Registered: 9-9-2013
Location: 13 Colonies
Member Is Offline
Mood: 220 221 whatever it takes
|
|
I just found a pile of discarded arrows at my gun club archery range. They were bent or fletchings were damaged and then discarded. You can also
find these things on ebay as auction lots of either functional arrows or whatnot. You can find them at a price of $1 per shaft. The trick is
choosing an elegant method of closing the bottom. As a way of keeping this post scientific (here's looking at you Bert )... +2 for brittle/high strength aluminum tubing. On the fracture toughness curve
materials like this will absorb less energy during a charpy test demonstrating that less deformation energy is taken from the shock front... the
material will deform elastically until the fracture point as opposed to a material that will transition past the elastic behavior into the plastic
deformation zone and absorb energy inelastically. Though this shouldn't matter much if the quantity of primary is sufficient. And one last note,
primaries don't really get characterized by critical diameter, but a composite cap with a boosting secondary should force you to compare this
secondary critical diameter with the tube ID.
|
|
|
TGT
Harmless
Posts: 46
Registered: 9-11-2014
Member Is Offline
Mood: No Mood
|
|
22 Magnum bullet casings I think would be perfect. You could heat them red hot and crash them in water or oil to make the metal more brittle, just a
suggestion.
TGT
|
|
|
UnintentionalChaos
International Hazard
   
Posts: 1454
Registered: 9-12-2006
Location: Mars
Member Is Offline
Mood: Nucleophilic
|
|
Quote: Originally posted by TGT  | 22 Magnum bullet casings I think would be perfect. You could heat them red hot and crash them in water or oil to make the metal more brittle, just a
suggestion.
TGT |
What, brass? Copper alloys readily anneal even with rapid quenching.
Department of Redundancy Department - Now with paperwork!
'In organic synthesis, we call decomposition products "crap", however this is not a IUPAC approved nomenclature.' -Nicodem
|
|
|
roXefeller
Hazard to Others
 
Posts: 463
Registered: 9-9-2013
Location: 13 Colonies
Member Is Offline
Mood: 220 221 whatever it takes
|
|
According to this copper alloy hardening article, you are more likely going to find non-quenchable brasses in brass cartridges. The typical path for hardening
material like that is cold working, where grains are shaped by continual material damage without heating, which would cause grain growth and softening. The earlier
article also mentions other methods, precipitation hardening being very common where bits of metals precipitate out of solid solution.
|
|
|
packetforger
Harmless
Posts: 48
Registered: 21-2-2014
Member Is Offline
Mood: Condensing
|
|
Avoid metal casings like the plague. Not only do they produce nasty metal shrapnel, but also, can react with certain primaries.
Back in the day when I used to experiment with such things, I often used paper casings dipped in the "liquid glass" sodium silicate solution to give
them more rigidity. A couple windings of paper around a dowel rod, fold in the end, dip the tube in the "liquid glass", and let harden up. You end up
with a nice cap with thin walls (which should transmit shock better), decent rigidity, and no scary metal parts.
The same liquid glass stuff can be used for all kinds of things, like reinforcing casings of salutes and such for a louder pop.
|
|
|
Microtek
National Hazard
  
Posts: 982
Registered: 23-9-2002
Member Is Offline
Mood: No Mood
|
|
Also, you get a detonator that is more prone to transportation mishaps because of the lower structural strength...
|
|
|
| Pages: