HOW TO MAKE longtitudinal porouse Alumina?


Hello everyone , does anyone have any Idea for making longtitudinal porouse Alumina ?

it would be something like the picture below but It would be made out of Alumina



[Edited on 24-12-2014 by wish i had a kraken!!!]

8-1.jpg - 147kB


the picture u are observing is a cross sectional view of longtitudinal porous copper



[Edited on 24-12-2014 by wish i had a kraken!!!]
View user's profile View All Posts By User
wish i had a kraken!!!
Hazard to Others
***




Posts: 157
Registered: 22-3-2012
Member Is Offline

Mood: No Mood

[*] posted on 25-12-2014 at 10:11


The picture U see above is a cross sectional view of a lotus type porous copper , I made them this way:
1.I had wires of Al coated with copper
2.I packed the coated wires in a copper tube
3.I extruded the billet
4.I put the produced sample in NAOH solution ,for a night and The next day the Al was gone!



[Edited on 25-12-2014 by wish i had a kraken!!!]

final.png - 918kB
View user's profile View All Posts By User
Bert
Super Administrator
*********




Posts: 2821
Registered: 12-3-2004
Member Is Offline

Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".

[*] posted on 25-12-2014 at 17:07


Nice work- How long/what Dia. segments of finished honeycomb have you achieved?

There are other techniques for producing alumina honeycomb substrates for catalytic reactions- see here:

http://www.sciencemadness.org/talk/viewthread.php?tid=2329&a...




Rapopart’s Rules for critical commentary:

1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.

Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).

View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1670
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 25-12-2014 at 18:18


Tidbit
"Catalytic converters are commonly made from ceramics containing a large proportion of synthetic cordierite. The manufacturing process deliberately aligns the cordierite crystals to make use of the very low thermal expansion seen for one axis. This prevents thermal shock cracking from taking place when the catalytic converter is used."
http://en.wikipedia.org/wiki/Cordierite
View user's profile View All Posts By User
wish i had a kraken!!!
Hazard to Others
***




Posts: 157
Registered: 22-3-2012
Member Is Offline

Mood: No Mood

[*] posted on 26-12-2014 at 07:49


Quote: Originally posted by Bert  
Nice work- How long/what Dia. segments of finished honeycomb have you achieved?

There are other techniques for producing alumina honeycomb substrates for catalytic reactions- see here:

http://www.sciencemadness.org/talk/viewthread.php?tid=2329&a...


Dear Bert , the samples I made had 4.6 mm and up to 20 mm height .
View user's profile View All Posts By User
AJKOER
Radically Dubious
*****




Posts: 3026
Registered: 7-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 30-12-2014 at 06:15


Alternately, one could focus on just creating highly reactive nano alumina. To quote a preparation from one source https://www.google.com/url?sa=t&source=web&rct=j&... :

"Catalyst Synthesis
Aluminum nitrate {Al(NO3)3-9H2O, 99.5%}(Merck), Ammonia {NH4OH, 32%} (Merck) and deionized water were used as starting chemicals. A transparent gel-like precursor containing Al cations is precipitated at pH ~7.5–8.5 when ammonia (%3.2) and Al nitrate salt solutions (0.26 M) are mixed together in 400 ml deionized water. The solution was mixing under ultrasonic vibration and maintained at a temperature 70 ºC for 2 h. The following chemical reactions occurred during preparation:
Al(NO)3 + 3NH4OH = Al(OH)3 (s) + 3 NH4NO3 (2)
Al(OH)3 = AlOOH (s) + H2O (3)
2 AlOOH = Al2O3 + H2O (4)
The precipitate obtained by reaction (2) was aged at a temperature ~70 ºC helped to homogenize the gel due. The ageing step is essential to convert Al (OH)3 to crystalline boehmite precursor by reaction (3). The precipitate is further processed by washing in deionized water. Then was added 300 ml ethanol to the filtered Al(OH)3 under ultrasonic vibration for 1 h then dried in oven at ~70 ºC for 18 h. "

Unfortunately, there is a downside to working with nano alumina, per a paper citing that nanoparticles kill and maim blood vessel cells found in the human brain, Oct 21, 2008 by Chen, L, RA Yokel, B Hennig and M Toborek, "Manufactured aluminum oxide nanoparticles decrease expression of tight junction proteins in brain vasculature" in Journal of Neuroimmune Pharmacology doi:10.1007/s11481-008-9131-5y.

Read the synopsis by Stacey L. Harper at https://www.google.com/url?sa=t&source=web&rct=j&...

Apparently a study using cells and rats indicated that nanoparticles of aluminum oxide can kill and adversely change the special cells that line the blood vessels in the human brain.

[Edited on 30-12-2014 by AJKOER]
View user's profile View All Posts By User
wish i had a kraken!!!
Hazard to Others
***




Posts: 157
Registered: 22-3-2012
Member Is Offline

Mood: No Mood

[*] posted on 30-12-2014 at 10:39


AJOKER , thanks for your reply , but Alumina coated with Pt are used in some special fixed bed Cracking reactors , I think if we could make a thing like the picture may be we could enhance the yield of cracking reactions., So , I think maybe Nano particles are not good for this purpose.
View user's profile View All Posts By User