| Pages:
1
2
3 |
Vpatent357
Harmless
Posts: 28
Registered: 10-7-2014
Member Is Offline
Mood: No Mood
|
|
Hi Laboratory of Liptakov,
First, thank you for your research on new kit-explosives easy to do and your innovations.
Cyklonan 1 seems to be the easiest but is it powerful ? (good booster for example?)
And 300 mg of silver acetylide/nitrate primary are sufficient for the complete detonation of one cube? i don't have ETN,PETN,MHN...
For NC, ping-pong balls lacquer can be used?
Small blasting caps, fingers safe !
|
|
|
Laboratory of Liptakov
International Hazard
   
Posts: 1457
Registered: 2-9-2014
Location: Tel Aviv University
Member Is Offline
Mood: old jew
|
|
Hi Patent :-)
Ping pong balls? Sure, of course. In 90 g of acetone dissolved 10 g balls. Ag binary salt primer? Unfortunately, I do not know. Untested. But I
think, 300mg will be good kick. Or 0,2-0,3g HMTD, of course. Yes, Cyklonan (1 cube) is a good booster for AN /fuel/ Al mixture. Coming soon you see
Ammonium nitrate, special fuel without nitro esters composition on only primary 0,5g sensitive.
... ...LL
[Edited on 10-3-2015 by Laboratory of Liptakov]
|
|
|
Vpatent357
Harmless
Posts: 28
Registered: 10-7-2014
Member Is Offline
Mood: No Mood
|
|
It remains for me to synthesize TACN
From what I know, it is secondary explosive. Is it safe to handle and store dry powder? more sensitive than ETN / PETN? for example
You have already experimented cyklonan with NC ping pong balls? it is of low quality and contains camphor ..
It's perfect I looking for exactly this kind of boost for AN mixtures, thank
I follow your youtube channel very closely
[Edited on 10-3-2015 by Vpatent357]
Small blasting caps, fingers safe !
|
|
|
Laboratory of Liptakov
International Hazard
   
Posts: 1457
Registered: 2-9-2014
Location: Tel Aviv University
Member Is Offline
Mood: old jew
|
|
Cyklonan 1 is similar sensitivity, low sensitivity as PETN. I see that Cyklonan works. Thank you for using Cyklonan explosive.... ...LL
|
|
|
Trotsky
Hazard to Others
 
Posts: 166
Registered: 6-2-2013
Location: US
Member Is Offline
Mood: No Mood
|
|
Why would you use ping pong balls for a nitrocellulose source? I don't get how you've got silver acetylide, but have to resort to ping pong balls for
NC? Nitrocellulose is ridiculously easy to synthesize, everything you need to do it is readily available, just sulfuric acid, some nitrate salt, and
cotton balls, sodium carbonate or even bicarbonate to neutralize when you're finished. You don't have to watch the temp very close, if you make any
attempt at all to keep it cool you should have zero risk of runaway, especially with a small batch. And even if you have a runaway you're not at risk
of accidental explosion…
|
|
|
Vpatent357
Harmless
Posts: 28
Registered: 10-7-2014
Member Is Offline
Mood: No Mood
|
|
Because I'm in the same approach as Dr. Liptakov,that is to say, Created my explosives as simply as possible with materials easily accessible and
without nitration ..
Yes SA.DS is very easy to do and effective as a primary, TACN seems very easy to produce secondary, even though we know nothing about him
(sensibility, storage..)
I can only find ammonia 20% and not 25%, it can work for the synthesis TACN? And are there specific recommendations for synthesis?
Small blasting caps, fingers safe !
|
|
|
Laboratory of Liptakov
International Hazard
   
Posts: 1457
Registered: 2-9-2014
Location: Tel Aviv University
Member Is Offline
Mood: old jew
|
|
Of course, only 20% NH3OH no problem to use. Because during the reaction concentration is decreasing. Perhaps 15%, perhaps only 10% at end of
reaction. That is no problem. The entire reaction works in a wide range. 10-40 g Cu wire. 50-120 g NH4NO3 dissolved. 100 -150 g NH3OH 15-25%. The
temperature reaction range 10-50 Celsius. 30 degrees Celsius is optimum, the optimum of 30 g of Cu, 100 g NH4NO3 optimum, 140 g NH3OH in aqa optimum
concentration of 20-25%. After cooling on 5C, separe on fine sieve. Dry. and etc. by Liptakov Channel.. ...LL
|
|
|
PHILOU Zrealone
International Hazard
   
Posts: 2894
Registered: 20-5-2002
Location: Brussel
Member Is Offline
Mood: Bis-diazo-dinitro-hydroquinonic
|
|
Quote: Originally posted by Laboratory of Liptakov  | Of course, only 20% NH3OH no problem to use. Because during the reaction concentration is decreasing. Perhaps 15%, perhaps only 10% at end of
reaction. That is no problem. The entire reaction works in a wide range. 10-40 g Cu wire. 50-120 g NH4NO3 dissolved. 100 -150 g NH3OH 15-25%. The
temperature reaction range 10-50 Celsius. 30 degrees Celsius is optimum, the optimum of 30 g of Cu, 100 g NH4NO3 optimum, 140 g NH3OH in aqa optimum
concentration of 20-25%. After cooling on 5C, separe on fine sieve. Dry. and etc. by Liptakov Channel.. ...LL |
NH4OH not NH3OH!
PH Z (PHILOU Zrealone)
"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
|
|
|
Laboratory of Liptakov
International Hazard
   
Posts: 1457
Registered: 2-9-2014
Location: Tel Aviv University
Member Is Offline
Mood: old jew
|
|
Of course, NH4OH, thanks Philou, I'm sorry.... ... ...LL
|
|
|
PHILOU Zrealone
International Hazard
   
Posts: 2894
Registered: 20-5-2002
Location: Brussel
Member Is Offline
Mood: Bis-diazo-dinitro-hydroquinonic
|
|
No problemo 
NH2OH (hydroxylamine) would be nice to experiment with owing to the high VOD of HAN (hydroxylamine nitrate - NH2OH.HNO3 (HO-NH3NO3)) (arround 8000
m/s).
I wonder if it will complexate competitively against NH3 via the NH2, via the OH or like NH2-NH2 with both.
[Edited on 14-3-2015 by PHILOU Zrealone]
PH Z (PHILOU Zrealone)
"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
|
|
|
Marcello0922
Harmless
Posts: 5
Registered: 15-8-2024
Member Is Offline
|
|
Quote: Originally posted by Rosco Bodine  | @ LL I agree about the possibility of a mixed salt of TACN and TACP being the product. A synthesis of TACP which I described many years ago and
posted again recently uses Cu(NO3)2 as precursor for TACP, however the yield resulting is lower than what would be quantitative for the desired TACP.
|
If you are synthesizing TACP using Cu(NO3)2 then the final reaction produces about 90% TACP and 10% TACN - I have tested this several times using XRD.
Synthesis of TACP with NH4ClO4, CuO and NH3(aq) gives a pure product. XRD showed that [Cu(NH3)4](ClO4)2 is then formed as a deformed octahedron.
The most interesting thing is that with the above method and the addition of hexamine, the reaction proceeds even at room temperature (reaction
catalyst?), while the XRD products showed that:
[Cu(NH3)5][NH3](ClO4)3 - crystals in the form of a pyramid with a square base and a perfect trigonal bipyramid. The content of the latter compound was
about 86%, while [Cu(NH3)4](ClO4)2 was only 14%.
|
|
|
Etanol
Hazard to Others
 
Posts: 249
Registered: 27-2-2012
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Marcello0922  |
The most interesting thing is that with the above method and the addition of hexamine, the reaction proceeds even at room temperature (reaction
catalyst?), while the XRD products showed that:
[Cu(NH3)5][NH3](ClO4)3 - crystals in the form of a pyramid with a square base and a perfect trigonal bipyramid. The content of the latter compound was
about 86%, while [Cu(NH3)4](ClO4)2 was only 14%. |
[Cu(NH3)5][NH3](ClO4)3 ?
Copper(III) complex?
May be [Cu(NH3)5][NH4](ClO4)3 or [Cu(NH3)4][NH4](ClO4)3 ?
|
|
|
Marcello0922
Harmless
Posts: 5
Registered: 15-8-2024
Member Is Offline
|
|
The pattern I wrote was confirmed by 3 people - 1 who did the XRD study and 2 who do the spectra resolving. And this was on 5 samples after each
synthesis. I know this is strange.
But I have another question by the way: what products can be in the filtrate? In addition to the Schweizer reagent, of course. And unreacted hexamine
or ammonium perchlorate.
|
|
|
Laboratory of Liptakov
International Hazard
   
Posts: 1457
Registered: 2-9-2014
Location: Tel Aviv University
Member Is Offline
Mood: old jew
|
|
Interesting research of crystalography, Marcello.....With a lot pyamides.
In mother liquor will NH4ClO4, CuO, diluted TACP, diluted hexamine + ammmonium hydroxide. This liquor
is possible evaporate about cca 30 C and obtain next dry energetic material with different (usually slow burned) properties against TACP / CHP.
Mother liquor 10g + 100g dH2O is also possible boil at cca 100 C.
At the high temperature arise fine dry powder CuO, crystalls NH4ClO4+ crystalls hexamine. All gas NH3/4 get out from solution.
At boiling pure TACP mother liquor arise CuO powder + NH4ClO4. All gas NH3/4 get out from solution....
Development of primarily - secondary substances: CHP (2015) neutral CHP and Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024) Diper
60 (2025)
|
|
|
Vpatent357
Harmless
Posts: 28
Registered: 10-7-2014
Member Is Offline
Mood: No Mood
|
|
Cube composition (det. failure)
Hi, i test Cyklonan1 comp. it's 90% TACN cube(10g) + 88% TACP PBX booster(1.2g) + SADS mini-cap(0.3g)
But after cap set off, i find some PBX & cube residues all around,
I think it's because i don't have confined PBX booster in Al tube, no ?
What optimizations do you recommand for a successful detonation ?
Small blasting caps, fingers safe !
|
|
|
Etanol
Hazard to Others
 
Posts: 249
Registered: 27-2-2012
Member Is Offline
Mood: No Mood
|
|
Vpatent357, what is the density of your SADS in primary detonator?
PBX-mix has a high initiation pressure. SADS at low density has very low detonation pressure. This is not enough to initiate a your mix.
|
|
|
Vpatent357
Harmless
Posts: 28
Registered: 10-7-2014
Member Is Offline
Mood: No Mood
|
|
I press SADS base to 150mg strong with hands, 100mg medium and 50mg low.
I tested another PBX TACP this time confined sample and don't explose too.
(below)

My lonely success with 300mg cap SADS is with TACP powder pressed & confined like 3g charge.
Small blasting caps, fingers safe !
|
|
|
Etanol
Hazard to Others
 
Posts: 249
Registered: 27-2-2012
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Vpatent357  | I press SADS base to 150mg strong with hands, 100mg medium and 50mg low.
I tested another PBX TACP this time confined sample and don't explose too.
|
SADS has no problems with DDT. Therefore, I think you can use 250mg strong pressed and 50mg low.
If the wall thickness between PBX-TACP and SADS is less than 0.2 mm, then the next idea is to increase the mass of SADS 
Unfortunately, I do not know the critical diameter of PBX-TACP.
|
|
|
dangerous amateur
Hazard to Others
 
Posts: 151
Registered: 8-7-2011
Member Is Offline
Mood: No Mood
|
|
In my opinion your SADS cap is to blame. 300mg is ok when directly in contact with PETN. But not alone and especially not alone in a pt100 tube made
of steel.
Make a real cap with PETN or ETN Booster and see what happens
|
|
|
Vpatent357
Harmless
Posts: 28
Registered: 10-7-2014
Member Is Offline
Mood: No Mood
|
|
Ah, I'd love to have ETN, but I don't have sulfuric acid in my country :/
And to be precise, these are caps from aluminum pipe 4 x 0.45 mm that I make myself.
Critical diameter for TACP is low ~2mm & ~3-4mm for PBX.
[Edited on 24-3-2026 by Vpatent357]
Small blasting caps, fingers safe !
|
|
|
Etanol
Hazard to Others
 
Posts: 249
Registered: 27-2-2012
Member Is Offline
Mood: No Mood
|
|
ok
It seems, the detonation wave is not able to transmit through the side wall. What material do you use to seal the end of the tube between the SADS and
PBX-TACP?
The ideal solution is to use 1 layer of aluminum tape to seal the tube.
Also, it seems to me that your column height of pressed SADS to internal diameter ratio is too high. It should be 1.5...2. It is advisable to use a
larger diameter tube for such a mass.
[Edited on 24-3-2026 by Etanol]
|
|
|
dangerous amateur
Hazard to Others
 
Posts: 151
Registered: 8-7-2011
Member Is Offline
Mood: No Mood
|
|
Then you probably also don't have nitric acid?
What leads to the next question, how to you make proper SADS without it?
Also I don't see why you should use TACP with any binder for this job. As Etanol pointed out, the binder will make it harder to initiate. Why not
press it in some container or tube?
|
|
|
Vpatent357
Harmless
Posts: 28
Registered: 10-7-2014
Member Is Offline
Mood: No Mood
|
|
I have an old NA bottle 60% for my SADS, no SA to date and cant buy
and yes i will make simple booster like 95 TACP + 5 Al in tube pressed
Small blasting caps, fingers safe !
|
|
|