Silver Oxide. Black/brown or purple?


On wikipedia this stuff is said to be brown or black and it also has pictures showing it.

I also found some silver oxide on ebay recently and it has a purple color to it... or im colorblind and I just realized...

Here is a picture directly from the post
http://i.ebayimg.com/00/$(KGrHqQOKjYE4278U6LNBOV7Tuh4Lw~~60_12.JPG

Does this have anything to do with color change due to being exposed to light or ...?
View user's profile View All Posts By User
cyanureeves
National Hazard
****




Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline

Mood: No Mood

[*] posted on 14-3-2015 at 18:56


i know my silver chloride always turns purple on the outside but stays white on the inside when i crumble the clumped up mass.

View user's profile View All Posts By User
bolbol
Hazard to Others
***




Posts: 167
Registered: 3-1-2015
Member Is Offline

Mood: No Mood

[*] posted on 14-3-2015 at 19:05


When exposed to light, doesn't the AgCl decompose to Silver and Chlorine? If it does indeed decompose to silver then why is it purple at all? Is that the color of silver when the particle size is small? I know gold is brown color when in fine powder and I thought maybe the same happens with silver
View user's profile View All Posts By User
Oscilllator
National Hazard
****




Posts: 659
Registered: 8-10-2012
Location: The aqueous layer
Member Is Offline

Mood: No Mood

[*] posted on 15-3-2015 at 02:13


The ~15g of silver oxide I made (for safe transport) was completely black. Nothing purple about it.
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8150
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 15-3-2015 at 07:28


Silver(I) oxide is black or very dark grey. Maybe the picture looks somewhat purple, due to off-white lighting.



The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User